# US 2024/0200231 A1 · In-situ hydrophobically modified aramid nano aerogel fiber and uses thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0200231 A1
- Document ID: US20240200231A1
- Status: Published application
- Kind: A1
- Application number: 18/378,677
- Filed: 2023-10-11
- Published: 2024-06-20
- Earliest claimed: 2021-08-02
- Assignees: Suzhou Institute of Nano-Tech and Nano-Bionics (Sinano) , Chinese Academy of Sciences
- Applicants: Suzhou Institute of Nano-Tech and Nano-Bionics (Sinano) , Chinese Academy of Sciences
- Inventors: Xuetong ZHANG; Yaqian BAO; Zengwei LIU
- Web page: https://patentgrep.com/patent/US20240200231A1

## CPC

- D01D 5/06: Wet spinning methods {(D01D5/0046 takes precedence)}
- B29C 64/118: using filamentary material being melted, e.g. fused deposition modelling [FDM]
- B29C 64/30: Auxiliary operations or equipment
- B33Y 10/00: Processes of additive manufacturing
- B33Y 40/20: Post-treatment, e.g. curing, coating or polishing
- B33Y 80/00: Products made by additive manufacturing
- D01F 6/605: {from aromatic polyamides}
- B29K 2077/10: {Aromatic polyamides [polyaramides] or derivatives thereof}
- B29K 2105/0061: {Gel or sol}
- B29K 2105/04: cellular or porous
- B29K 2995/0013: Conductive
- B29K 2995/0077: Yield strength; Tensile strength
- B29K 2995/0093: hydrophobic
- D10B 2331/021: aromatic polyamides, e.g. aramides
- D10B 2401/063: high strength
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES

## Abstract

An in-situ hydrophobically modified aramid nano aerogel fiber as well as a preparation method and uses thereof are provided. The preparation method includes: providing an aramid nano spinning solution; preparing a hydrophobically modified aramid nano aerogel fiber by using a spinning technology, wherein the coagulating bath adopted by the spinning technology includes a first organic solvent and a halogenated reagent including a monochloroalkane, a monochloroalkane, a dibromoalkane, a dichloroalkane and a trichloroalkane; and then drying to obtain the in-situ hydrophobically modified aramid nano aerogel fiber. The in-situ hydrophobically modified aramid nano aerogel fiber has a unique three-dimensional porous network structure, low heat conductivity, high porosity, high tensile strength and elongation at break, a certain spinnability and structure stability, and can be applied to the field of textiles. A fabric knitted with the hydrophobic fibers has a self-cleaning ability.

## Claims

### Claim 1

An in-situ hydrophobically modified aramid nano aerogel, wherein the in-situ hydrophobically modified aramid nano aerogel fiber has a connected three-dimensional porous network structure formed by overlapping grafting modified aramid nano structures having a size of 8 nm-300 nm; the connected three-dimensional porous network structure is composed of micropores having a size of less than 2 nm, mesopores having a size of 2-50 nm and macropores having a size of 50 nm-500 μm; the connected three-dimensional porous network structure has a porosity of 60%-99% and a specific surface area of 100-1000 m2/g; the in-situ hydrophobically modified aramid nano aerogel fiber has a diameter of 10 μm-2 mm and a draw ratio of more than 10; the in-situ hydrophobically modified aramid nano aerogel fiber has a heat conductivity of 50 mW/(m·K), a tensile strength of 3-35 Mpa, and an elongation at break of 10-50%;
the in-situ hydrophobically modified aramid nano aerogel fiber is prepared by a preparation method comprising:
providing an aramid nano spinning solution;
preparing a hydrophobically modified aramid nano gel fiber by using a spinning technology, wherein a coagulating bath adopted by the spinning technology comprises a first organic solvent and a halogenated reagent comprising a combination of any one or more than two of monochloroalkane, monochloroalkane, dibromoalkane, dichloroalkane, and trichloroalkane; and
drying the hydrophobically modified aramid nano gel fiber to obtain the in-situ hydrophobically modified aramid nano aerogel fiber.

### Claim 2 (depends on 8)

The in-situ hydrophobically modified aramid nano aerogel fiber according to claim 8, wherein a contact angle between a surface of the in-situ hydrophobically modified aramid nano aerogel fiber and water is from 90° to 150°, and a grafting substitution degree of the in-situ hydrophobically modified aramid nano aerogel fiber is 0.01-20%.

### Claim 3 (depends on 1)

A method of using the in-situ hydrophobically modified aramid nano aerogel fiber according to claim 1, comprising using the in-situ hydrophobically modified aramid nano aerogel fiber in fields of oil-water separation, waterproof self-cleaning fabrics, composite materials, hydrophobic fiber flocs, filtration materials, or thermal insulation materials.

### Claim 4 (depends on 1)

The in-situ hydrophobically modified aramid nano aerogel fiber according to claim 1, wherein in a preparation process, a volume ratio of the halogenated reagent to the first organic solvent is 20:1-1:20; and/or, the first organic solvent comprises a combination of any one or more than two of DMSO, methanol, ethanol, propanol, butanol, formic acid, and acetic acid; and/or, the halogenated reagent comprises a combination of one or more than two of monobromobutane, monobromoethane, monochloroethane, dibromobutane, dichlorobutane, and trichloromethane.

### Claim 5 (depends on 1)

The in-situ hydrophobically modified aramid nano aerogel fiber according to claim 1, wherein in a preparation process, the aramid nano spinning solution comprises a second organic solvent and a poly(p-phthaloyl p-phenylenediamine) polymer; the second organic solvent comprises a combination of any one or more than two of DMF, DMSO, NMP, and methanol; the poly(p-phthaloyl p-phenylenediamine) polymer comprises a combination of any one or more than two of aramid 1313, aramid 1414, and a poly(p-phthaloyl-p-phenylenediamine) modified polymer; a concentration of the poly(p-phthaloyl p-phenylenediamine) polymer in the aramid nano spinning solution is 1-30 wt %;
the aramid nano spinning solution also comprises an alkaline substance; the alkaline substrate comprises a combination of any one or more than two of KOH, NaOH, and potassium tert-butoxide.

### Claim 6 (depends on 1)

The in-situ hydrophobically modified aramid nano aerogel fiber according to claim 1, wherein in a preparation process, the spinning technology comprises a combination of any one or more than two of a wet spinning technology and a 3D printing technology.

### Claim 7 (depends on 6)

The in-situ hydrophobically modified aramid nano aerogel fiber according to claim 6, wherein in the preparation process, the wet spinning technology comprises: providing the aramid nano spinning solution with a selected concentration, and controlling compositions of the coagulating bath, so that poly(p-phthaloyl p-phenylenediamine) polymer in the aramid nano spinning solution is cross-linked to form the hydrophobically modified aramid nano gel fiber;
process conditions adopted by the wet spinning technology comprise: the concentration of the aramid nano spinning solution is 1-30wt %, the aramid nano spinning solution is extruded into the coagulating bath through an injection pump, and a diameter of an extrusion needle is 10 μm-2 mm.

### Claim 8 (depends on 6)

The in-situ hydrophobically modified aramid nano aerogel fiber according to claim 6, wherein in the preparation process, the 3D printing technology comprises: carrying out a physical crosslinking or a chemical crosslinking on a fiber printed by using the aramid nano spinning solution as a printing ink in an environment where a mixed solution of a second organic solvent and the halogenated reagent is used as the coagulating bath to form the hydrophobically modified aramid nano gel fiber.

### Claim 9 (depends on 1)

The in-situ hydrophobically modified aramid nano aerogel fiber according to claim 1, wherein the preparation method comprises: a solvent not easy to dry in the hydrophobically modified aramid nano gel fiber is replaced with a solvent easy to dry, and then the hydrophobically modified aramid nano gel fiber subjected to replacement is dried, the solvent easy to dry comprises a combination of any one or more than two of water, methanol, ethanol, tertiary butanol, acetone, cyclohexane, and n-hexane;
and/or, the drying comprises a combination of any one or more than two of a supercritical fluid drying method, a vacuum freeze drying method, and an ambient drying method.

### Claim 10 (depends on 3)

The method according to claim 3, wherein a contact angle between a surface of the in-situ hydrophobically modified aramid nano aerogel fiber and water is from 90° to 150°, and a grafting substitution degree of the in-situ hydrophobically modified aramid nano aerogel fiber is 0.01-20%.

### Claim 11 (depends on 1)

The in-situ hydrophobically modified aramid nano aerogel fiber according to claim 1, wherein the porosity of the connected three-dimensional porous network structure is 70%-99%.

### Claim 12 (depends on 1)

The in-situ hydrophobically modified aramid nano aerogel fiber according to claim 1, wherein the diameter of the in-situ hydrophobically modified aramid nano aerogel fiber is 50 μm-1 mm.

### Claim 13 (depends on 1)

The in-situ hydrophobically modified aramid nano aerogel fiber according to claim 1, wherein the diameter of the in-situ hydrophobically modified aramid nano aerogel fiber is 50 μm-500 μm.

### Claim 14 (depends on 6)

The in-situ hydrophobically modified aramid nano aerogel fiber according to claim 6, wherein the spinning technology is the wet spinning technology.