# US 2024/0200227 A1 · SiC WAFER AND SiC EPITAXIAL WAFER

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0200227 A1
- Document ID: US20240200227A1
- Status: Published application
- Kind: A1
- Application number: 18/543,359
- Filed: 2023-12-18
- Published: 2024-06-20
- Earliest claimed: 2022-12-20
- Assignees: Resonac Corporation
- Applicants: Resonac Corporation
- Inventors: Shunsuke NOGUCHI
- Web page: https://patentgrep.com/patent/US20240200227A1

## CPC

- C30B 25/20: the substrate being of the same materials as the epitaxial layer
- C30B 29/36: Carbides
- B32B 3/02: characterised by features of form at particular places, e.g. in edge regions {(non-uniform thickness B32B3/263)}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

In a SiC wafer according to the present embodiment, a crystal surface has an offset angle of 0.5° or more and 10° or less in a first direction with respect to a surface of the SiC wafer, dislocations are confirmed when a first measurement point is confirmed through X-ray reflection topography using (3-3016) as a diffraction surface, the first measurement point is a point shifted by a length of ½ of a radius of the SiC wafer in the first direction from the center of a measurement region that is 5 mm or more inside from the outer circumferential end of the SiC wafer, the dislocations include first dislocations having an aspect ratio of 5 or more and second dislocations having an aspect ratio of less than 3, where the aspect ratio is obtained by dividing a long axis length of a rectangle that circumscribes the dislocation and has the smallest area by a short axis length, and at the first measurement point, the density of the first dislocations is higher than the density of the second dislocations.

## Claims

### Claim 1

A SiC wafer in which a crystal surface has an offset angle of 0.5° or more and 10° or less in a first direction with respect to a surface of the SiC wafer, and dislocations are confirmed when a first measurement point is measured using X-ray reflection topography with (3-3016) as a diffraction surface,
wherein the first measurement point is a point shifted by a length of ½ of a radius of the SiC wafer in the first direction from the center of a measurement region that is 5 mm or more inside from the outer circumferential end of the SiC wafer,
wherein the dislocations include first dislocations having an aspect ratio of 5 or more and second dislocations having an aspect ratio of less than 3, where the aspect ratio is obtained by dividing a long axis length of a rectangle that circumscribes the dislocation and has the smallest area by a short axis length, and
wherein, at the first measurement point, the density of the first dislocations is higher than the density of the second dislocations.

### Claim 2 (depends on 1)

The SiC wafer according to claim 1,
wherein dislocations are confirmed when a second measurement point is measured using X-ray reflection topography with (3-3016) as a diffraction surface,
wherein the second measurement point is a point shifted by a length of ½ of a radius of the SiC wafer in a direction opposite to the first direction from the center of the measurement region, and
wherein the density of the dislocations at the second measurement point is lower than the density of the dislocations at the first measurement point.

### Claim 3 (depends on 2)

The SiC wafer according to claim 2,
wherein the dislocations at the second measurement point include the first dislocations and the second dislocations, and
wherein, at the second measurement point, the density of the second dislocations is higher than the density of the first dislocations.

### Claim 4 (depends on 1)

The SiC wafer according to claim 1,
wherein the SiC wafer has a diameter of 140 mm or more.

### Claim 5 (depends on 1)

The SiC wafer according to claim 1,
wherein the SiC wafer has a diameter of 190 mm or more.

### Claim 6 (depends on 1)

The SiC wafer according to claim 1,
wherein, when supported on a support surface at a position overlapping a circumference with a radius of 17.5 mm from the center,
if a surface connecting first points overlapping the support surface when viewed in a thickness direction within the upper surface is set as a first reference surface, and the direction above the first reference surface is set as positive, a BOW is 40 μm or less.

### Claim 7 (depends on 1)

The SiC wafer according to claim 1,
wherein, when supported on a support surface at a position overlapping a circumference with a radius of 17.5 mm from the center,
if a surface connecting first points overlapping the support surface when viewed in a thickness direction within the upper surface is set as a first reference surface, a WARP is 100 μm or less.

### Claim 8

A SiC wafer in which, when a first measurement point, a second measurement point, a third measurement point and a fourth measurement point are measured using X-ray reflection topography with (3-3016) as a diffraction surface, dislocations are confirmed,
wherein the first measurement point is a point shifted by a length of ½ of a radius of the SiC wafer in a first direction from the center of a measurement region that is 5 mm or more inside from the outer circumferential end of the SiC wafer,
wherein the second measurement point is a point shifted by a length of ½ of a radius of the SiC wafer in a direction opposite to the first direction from the center of the measurement region,
wherein the third measurement point is a point shifted by a length of ½ of a radius of the SiC wafer in a second direction perpendicular to the first direction from the center of a measurement region that is 5 mm or more inside from the outer circumferential end of the SiC wafer,
wherein the fourth measurement point is a point shifted by a length of ½ of a radius of the SiC wafer in a direction opposite to the second direction from the center of the measurement region,
wherein the dislocations include first dislocations having an aspect ratio of 5 or more and second dislocations having an aspect ratio of less than 3, where the aspect ratio is obtained by dividing a long axis length of a rectangle that circumscribes the dislocation and has the smallest area by a short axis length, and
wherein, at each of the first measurement point, the second measurement point, the third measurement point and the fourth measurement point, the density of the first dislocations is higher than the density of the second dislocations.

### Claim 9 (depends on 1)

A SiC epitaxial wafer, comprising:
the SiC wafer according to claim 1; and
a SiC epitaxial layer formed on a surface of the SiC wafer.

### Claim 10 (depends on 8)

A SiC epitaxial wafer, comprising
the SiC wafer according to claim 8; and
a SiC epitaxial layer formed on a surface of the SiC wafer.