# US 2024/0200183 A1 · Devices and methods for sputtering at least two elements

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0200183 A1
- Document ID: US20240200183A1
- Status: Published application
- Kind: A1
- Application number: 18/541,027
- Filed: 2023-12-15
- Published: 2024-06-20
- Earliest claimed: 2022-12-16
- Assignees: Techifab GmbH
- Applicants: TechIFab GmbH
- Inventors: Heidemarie SCHMIDT; Danilo BUERGER
- Web page: https://patentgrep.com/patent/US20240200183A1

## CPC

- C23C 14/14: Metallic material, boron or silicon
- C23C 14/3492: {Variation of parameters during sputtering}
- C23C 14/0042: {Controlling partial pressure or flow rate of reactive or inert gases with feedback of measurements}
- C23C 14/34: Sputtering
- C23C 14/54: Controlling or regulating the coating process
- C23C 14/541: {Heating or cooling of the substrates}
- C23C 14/548: {Controlling the composition}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

According to various aspects, a method is provided including: depositing a material layer on a substrate, wherein the material layer includes at least a first element and a second element in a predefined atomic ratio, wherein the first element has a higher temperature-dependent re-evaporation rate from the substrate and/or the material layer than the second element; wherein depositing the material layer includes: generating a deposition material stream for deposition on the substrate, wherein the deposition material stream includes an atomic ratio of the first element to the second element higher than the predefined atomic ratio, and setting a temperature of the substrate to evaporate atoms of the first element from the substrate and/or the material layer such that the material layer has the predefined atomic ratio of the first element and the second element.

## Claims

### Claim 1

A method, comprising:
depositing a material layer on a substrate, wherein the material layer comprises at least a first element and a second element in a predefined atomic ratio, wherein the first element has a higher temperature-dependent re-evaporation rate from the substrate and/or the material layer than the second element;
wherein depositing the material layer comprises:
generating a deposition material stream for deposition on the substrate, wherein the deposition material stream comprises an atomic ratio of the first element to the second element higher than the predefined atomic ratio, and
setting a temperature of the substrate to evaporate atoms of the first element from the substrate and/or the material layer such that the material layer has the predefined atomic ratio of the first element and the second element.

### Claim 2 (depends on 1)

The method according to claim 1,
wherein setting the temperature of the substrate comprises setting the temperature of the substrate to a temperature value equal to or greater than a lower threshold value, wherein the lower threshold value represents a vapor pressure of the first element at a working pressure of an atmosphere the deposition material stream is generated in.

### Claim 3 (depends on 1)

The method according to claim 1,
wherein, in a temperature range from about 400° C. to about 800° C., the temperature-dependent re-evaporation rate of the first element from the substrate and/or the material layer is at least two times the temperature-dependent re-evaporation rate of the second element from the substrate and/or the material layer.

### Claim 4 (depends on 1)

The method according to claim 1,
wherein the first element is bismuth and the second element is iron.

### Claim 5 (depends on 4)

The method according to claim 4,
wherein the temperature of the substrate is set to have a temperature value in a range from about 600° C. to about 650° C.

### Claim 6

A method, comprising:
determining a temperature value representing a temperature of a substrate on which a material layer comprising at least a first element and a second element in a predefined atomic ratio is to be deposited;
determining, based on the temperature value, a nominal power ratio between a first power associated with sputtering the first element and a second power associated with sputtering the second element; and
setting a first power value of the first power and a second power value of the second power in accordance with the nominal power ratio.

### Claim 7 (depends on 6)

The method according to claim 6, further comprising:
depositing the material layer on the substrate, wherein the first power value and the second power value are set prior to depositing the material layer on the substrate.

### Claim 8 (depends on 6)

The method according to claim 6, further comprising:
during depositing the material layer on the substrate:
detecting plasma properties associated with sputtering the first element and/or the second element,
determining an adapted nominal power ratio between the first power and the second power based on the plasma properties, and
controlling the first power and the second power in accordance with the adapted nominal power ratio.

### Claim 9

A method, comprising:
sputtering at least a first element and a second element to deposit, on a substrate, a material layer comprising the first element and the second element;
during sputtering the first element and the second element:
detecting a temperature value representing a temperature of the substrate;
determining, based on the temperature value, one or more operation parameters of the sputtering; and
controlling the sputtering based on the one or more operation parameters.

### Claim 10 (depends on 9)

The method according to claim 9, further comprising:
heating the substrate to a set temperature value prior to sputtering the first element and the second element, wherein the set temperature value is less than a threshold value which represents a vapor pressure of the first element at a working pressure of an atmosphere in which the material layer is deposited.

### Claim 11

A method, comprising:
sputtering at least a first element and a second element to deposit, on a substrate, a material layer comprising the first element and the second element;
during sputtering the first element and the second element:
detecting plasma properties associated with sputtering the first element and/or the second element;
determining, based on the plasma properties, one or more operation parameters of the sputtering; and
controlling the sputtering based on the one or more operation parameters.

### Claim 12 (depends on 11)

The method according to claim 11, further comprising:
heating the substrate to a set temperature value prior to sputtering the first element and the second element, wherein the set temperature value is less than a threshold value which represents a vapor pressure of the first element at a working pressure of an atmosphere in which the material layer is deposited.

### Claim 13 (depends on 11)

The method according to claim 11,
wherein sputtering the first element and the second element comprises sputtering the first element and the second element in an atmosphere comprising oxygen;
wherein the one or more operation parameters comprise an oxygen partial pressure; and
wherein controlling the sputtering comprises controlling an oxygen supply based on the oxygen partial pressure.

### Claim 14 (depends on 13)

The method according to claim 13,
wherein determining the oxygen partial pressure based on the plasma properties comprises determining one or more parameters representing electrical properties of a first plasma associated with sputtering the first element and/or a second plasma associated with sputtering the second element, and determining the oxygen partial pressure based on the one or more parameters; and/or
wherein detecting plasma properties comprises detecting a plasma emission of a first plasma associated with sputtering the first element and/or a second plasma associated with sputtering the second element, determining, based on the plasma emission, an intensity of an oxygen characteristic, wherein determining the oxygen partial pressure comprises determining the oxygen partial pressure using the oxygen characteristic.

### Claim 15 (depends on 11)

The method according to claim 11,
wherein sputtering the first element and the second element comprises sputtering the first element in accordance with a first power and the second element in accordance with a second power; and
wherein the one or more operation parameters comprise a power ratio between the first power and the second power, and wherein controlling the sputtering comprises controlling the first power and the second power in accordance with the power ratio.

### Claim 16 (depends on 11)

The method according to claim 11,
wherein sputtering the first element comprises radio frequency sputtering the first element in accordance with a first power and a first power frequency;
wherein sputtering the second element comprises direct-current sputtering the second element in accordance with a second power; and
wherein:
the one or more operation parameters comprise a power ratio between the first power and the second power and wherein controlling the sputtering comprises controlling the first power and the second power in accordance with the power ratio, and/or
the one or more operation parameters comprise a frequency value of the first power frequency and wherein controlling the sputtering comprises controlling the sputtering of the first element in accordance with the frequency value.

### Claim 17 (depends on 11)

The method according to claim 11,
wherein sputtering the first element comprises radio frequency sputtering the first element in accordance with a first power and a first power frequency;
wherein sputtering the second element comprises radio frequency sputtering the second element in accordance with a second power and a second power frequency; and
wherein the one or more operation parameters comprise a frequency ratio between the first power frequency and the second power frequency and wherein controlling the sputtering comprises controlling the sputtering of the first element and the second element in accordance with the frequency ratio.

### Claim 18 (depends on 11)

The method according to claim 11,
wherein sputtering the first element comprises magnetron sputtering the first element from a first target and wherein sputtering the second element comprises magnetron sputtering the second element from a second target; and
wherein the one or more operation parameters comprise a distance ratio between a first distance and a second distance, wherein the first distance is a distance between the first target and one or more first magnets associated with magnetron sputtering the first element and wherein the second distance is a distance between the second target and one or more second magnets associated with magnetron sputtering the second element.

### Claim 19 (depends on 11)

The method according to claim 11,
wherein sputtering the first element and the second element comprises sputtering the first element and the second element in an atmosphere; and
wherein the one or more operation parameters comprise a pressure value representing a pressure of the atmosphere, and wherein controlling the sputtering comprises controlling the pressure of the atmosphere in accordance with the pressure value.

### Claim 20 (depends on 11)

The method according to claim 11,
wherein the first element is bismuth and the second element is iron.