# US 2024/0200173 A1 · Magnesium alloys for thixomolding applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0200173 A1
- Document ID: US20240200173A1
- Status: Published application
- Kind: A1
- Application number: 18/375,301
- Filed: 2023-09-29
- Published: 2024-06-20
- Earliest claimed: 2022-12-16
- Assignees: UT-Battelle, LLC; Leggera Technologies LLC; Fca US LLC
- Applicants: UT-Battelle, LLC; Leggera Technologies LLC; Fca US LLC
- Inventors: Govindarajan Muralidharan; Bryan Macek; Nathan Sanko
- Web page: https://patentgrep.com/patent/US20240200173A1

## CPC

- C22C 23/02: with aluminium as the next major constituent
- B22D 17/007: {Semi-solid pressure die casting}
- B22D 21/007: {with low melting point, e.g. Al 659 degrees C, Mg 650 degrees C}
- C22C 23/00: Alloys based on magnesium
- C22C 23/04: with zinc or cadmium as the next major constituent
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)

## Abstract

A magnesium alloy includes, in weight percent Al: 4.5-6.5; Zn: 0.05-3.0; Ca: 0-1.5; Sn: 0-4.0; Mn: 0.1-0.5; Si: 0-0.5; B+Sr: 0-0.5; less than 0.1 Fe; less than 0.1 Cu; less than 0.01 Ni; and Mg: Balance. A process for thixomolding, and a large dimension magnesium alloy article are also disclosed.

## Claims

### Claim 1

A magnesium alloy comprising, in weight percent:
Al: 4.5-6.5;
Zn: 0.1-3.0;
Ca: 0-1.5;
Sn: 0-4.0;
Mn: 0.1-0.5;
Si: 0-0.5;
B+Sr: 0-0.5
less than 0.1 Fe
less than 0.1 Cu
less than 0.01 Ni; and,
Mg: balance.

### Claim 2 (depends on 1)

The magnesium alloy of claim 1, wherein the alloy consists essentially of, in weight percent, Al: 4.5-6.5; Zn: 0.05-3.0; Ca: 0-1.5; Sn: 0-4.0; Mn: 0.1-0.5; Si: 0-0.5; B+Sr: 0-0.5; less than 0.1 Fe; less than 0.1 Cu; less than 0.01 Ni; and Mg: balance.

### Claim 3 (depends on 1)

The magnesium alloy of claim 1, wherein the alloy consists of, in weight percent, Al: 4.5-6.5; Zn: 0.05-3.0; Ca: 0-1.5; Sn: 0-4.0; Mn: 0.1-0.5; Si: 0-0.5; B+Sr: 0-0.5; less than 0.1 Fe; less than 0.1 Cu; less than 0.01 Ni; and Mg: balance.

### Claim 4 (depends on 1)

The magnesium alloy of claim 1, wherein the alloy has a processability index P of 20 to 150.

### Claim 5 (depends on 1)

The magnesium alloy of claim 1, wherein the alloy has a Ge content of from 0-0.5 wt. % Ge.

### Claim 6 (depends on 1)

The magnesium alloy of claim 1, wherein the alloy has a Li content of from 0-0.5 wt. % Li.

### Claim 7 (depends on 1)

The magnesium alloy of claim 1, wherein the alloy has a yield strength of at least 90 MPa.

### Claim 8 (depends on 1)

The magnesium alloy of claim 1, wherein the alloy has a yield strength of at least 100 MPa.

### Claim 9 (depends on 1)

The magnesium alloy of claim 1, wherein the alloy has a yield strength of at least 120 MPa.

### Claim 10 (depends on 1)

The magnesium alloy of claim 1, wherein the elongation to failure is at least 16%.

### Claim 11 (depends on 1)

The magnesium alloy of claim 1, wherein the elongation to failure is at least 20%.

### Claim 12 (depends on 1)

The magnesium alloy of claim 1, wherein the alloy has a melting range of at least 200° ° C.

### Claim 13 (depends on 1)

The magnesium alloy of claim 1, wherein the alloy has a melting range of at least 175° C.

### Claim 14 (depends on 1)

The magnesium alloy of claim 1, wherein the alloy has a melting range of at least 150° C.

### Claim 15 (depends on 1)

The magnesium alloy of claim 1, wherein the alloy has a melting range of at least 135° C.

### Claim 16

A method of preparing a thixomolded article, comprising the steps of:
providing a magnesium alloy comprising, in weight percent Al: 4.5-6.5; Zn: 0.05-3.0; Ca: 0-1.5; Sn: 0-4.0; Mn: 0.1-0.5; Si: 0-0.5; B+Sr: 0-0.5; less than 0.1 Fe; less than 0.1 Cu; less than 0.01 Ni; and Mg: balance;
heating the magnesium alloy to a temperature of 500-600° C., producing a thixotropic alloy comprising 30-65 weight % solids;
introducing the thixotropic alloy into a mold under a pressure of 50-100 MPa; and,
allowing the thixotropic alloy to cool to produce a solid thixomolded article.

### Claim 17

A method of preparing a thixomolded article, comprising the steps of:
providing a magnesium alloy comprising, in weight percent Al: 4.5-6.5; Zn: 0.05-3.0; Ca: 0-1.5; Sn: 0-4.0; Mn: 0.1-0.5; Si: 0-0.5; B+Sr: 0-0.5; less than 0.1 Fe; less than 0.1 Cu; less than 0.01 Ni; and Mg: balance;
heating the magnesium alloy to a temperature of 500-600° C., producing a thixotropic alloy comprising 30-65 weight % solids;
introducing the thixotropic alloy into an open mold under ambient pressure;
closing the mold to compress the thixotropic alloy and thus fill the mold; and,
allowing the thixotropic alloy to cool to produce a solid thixomolded article.

### Claim 18

A thixomolded article, comprising a magnesium alloy comprising, in weight percent Al: 4.5-6.5; Zn: 0.05-3.0; Ca: 0-1.5; Sn: 0-4.0; Mn: 0.1-0.5; Si: 0-0.5; B+Sr: 0-0.5; less than 0.1 Fe; less than 0.1 Cu; less than 0.01 Ni; and Mg: balance.

### Claim 19 (depends on 18)

The thixomolded article of claim 18, wherein the article has a weight of at least 3.6 kg and an average thickness of between 2.0 mm and 4.0 mm.

### Claim 20 (depends on 18)

The thixomolded article of claim 18, wherein the article has a largest dimension of between 50 cm and 200 cm.

### Claim 21 (depends on 18)

The thixomolded article of claim 18, wherein the article contains at least 1 molded-in connecting feature, the connecting feature provides a positive location function and structural strength of at least 70% of the base material strength, and the article is joined with other articles to produce an article with a mass of at least 7.2 kg.