# US 2024/0200172 A1 · Aluminum Casting Alloy for Near Net Shaped Casting of Structural or Non-structural Components

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0200172 A1
- Document ID: US20240200172A1
- Status: Published application
- Kind: A1
- Application number: 18/288,467
- Filed: 2022-04-21
- Published: 2024-06-20
- Earliest claimed: 2021-04-30
- Assignees: Nemak, S.A.B. de C.V.; McMaster University
- Applicants: Nemak, S.A.B. de C.V.; McMaster University
- Inventors: Glenn Edwin Byczynski; Anthony Marco Lombardi; Sumanth Shankar; Xiaochun Zeng
- Web page: https://patentgrep.com/patent/US20240200172A1

## CPC

- C22C 21/10: with zinc as the next major constituent
- B22D 21/007: {with low melting point, e.g. Al 659 degrees C, Mg 650 degrees C}
- B22D 21/04: Casting aluminium or magnesium {(no material; see B22D21/007)}
- C21D 1/56: characterised by the quenching agents
- C21D 9/0068: {for particular articles not mentioned below}
- C22C 1/026: {Alloys based on aluminium}
- C22F 1/053: of alloys with zinc as the next major constituent
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

An aluminum casting alloy for near net shaped casting of structural or non-structural components containing, in % by mass, Zn: 4.5-7.5%, Mg: 0.7-2.0%, Fe: 0.8-2.0%, Si: <0.3%, Cu: <0.1%, V: ≤0.2%, Ti: ≤0.2%, B: ≤0.04%, balance Al and unavoidable impurities, the sum of the contents of the impurities being≤0.1%. Also, a method for the manufacture of a cast part which has a yield strength of 180 to 200 MPa, an ultimate tensile strength of 300 to 320 MPa and an elongation of 11 to 14% and a method for the manufacture of a cast part which has a yield strength of 210 to 400 MPa, an ultimate tensile strength of 340 to 450 MPa and an elongation of 2 to 11% utilizing the described alloy.

## Claims

### Claim 1

An aluminum casting alloy for near net shaped casting of structural or non-structural components, the aluminum casting alloy consisting of, in % by mass,
Zn:
4.5-7.5%;
Mg:
0.7-2.0%;
Fe:
0.8-2.0%;
Si:
<0.3%;
Cu:
<0.1%;
V:
≤0.2%;
Ti:
≤0.2%;
B:
≤0.04%;
balance Al and unavoidable impurities, a sum of the contents of the impurities being≤0.1%.

### Claim 2 (depends on 1)

The aluminum casting alloy according to claim 1, wherein the Zn content is not more than 5.5% by mass.

### Claim 3 (depends on 1)

The aluminum casting alloy according to claim 1, wherein the Zn content is at least 4.6% by mass.

### Claim 4 (depends on 1)

The aluminum casting alloy according to claim 1, wherein the Mg content is not more than 1.0% by mass.

### Claim 5 (depends on 1)

The aluminum casting alloy according to claim 1, wherein the Mg content is at least 0.8% by mass.

### Claim 6 (depends on 1)

The aluminum casting alloy according to claim 1, wherein the Fe content is not more than 1.5% by mass.

### Claim 7 (depends on 1)

The aluminum casting alloy according to claim 1, wherein the Fe content is at least 1.0% by mass.

### Claim 8 (depends on 1)

The aluminum casting alloy according to claim 1, wherein the Si content is less than 0.2% by mass.

### Claim 9 (depends on 1)

The aluminum casting alloy according to claim 1, wherein the alloy contains at least 0.05% by mass of Ti.

### Claim 10 (depends on 1)

The aluminum casting alloy according to claim 1, wherein the alloy contains at least 0.1% by mass of V.

### Claim 11 (depends on 1)

The aluminum casting alloy according to claim 1, wherein the alloy contains 4.6 to 5.0% by mass Zn and 0.8 to 1.0% by mass Mg and the alloy has in the as-cast state (“F-temper”) a yield strength of 140 to 160 MPa, an ultimate tensile strength in the range of 280 to 300 MPa and elongation ranging from 11 to 14%.

### Claim 12 (depends on 1)

The aluminum casting alloy according to claim 1, wherein the alloy contains 5.0 to 5.5% by mass Zn and 1.6 to 2.0% by mass Mg and the alloy has in the as-cast state (“F-temper”) a yield strength of 180 to 210 MPa, an ultimate tensile strength in the range of 300 to 340 MPa and an elongation ranging from 4 to 7%.

### Claim 13 (depends on 11)

A method for the manufacture of a cast part which has a yield strength of 180 to 200 MPa, an ultimate tensile strength of 300 to 320 MPa and an elongation of 11 to 14% comprising the following working steps:
a) providing an aluminum melt alloyed in accordance with claim 11;
b) casting a cast part from the aluminum melt;
c) subjecting the cast part to a T4 temper treatment which involves a solution heat treatment at temperatures of 460 to 480° C. for 1 to 8 h optionally followed by a forced air quench and natural aging for 14 to 75 days.

### Claim 14 (depends on 12)

A method for the manufacture of a cast part which has a yield strength of 210 to 400 MPa, an ultimate tensile strength of 340 to 450 MPa and an elongation of 2 to 11% comprising the following working steps:
a) providing an aluminum melt alloyed in accordance with claim 12;
b) casting a cast part from the aluminum melt;
c) subjecting the cast part to heat treatment, wherein
c.1) the heat treatment is a T4 temper treatment which involves a solution heat treatment at temperatures of 450 to 480° C. for 2 to 24 h optionally followed by a forced air or water quench and natural aging for 7 to 75 days
or
c.2) the heat treatment is a T7 temper treatment which involves a solution heat treatment at temperatures of 450 to 480° C. for 2 to 24 h followed by forced air or water quench and 1-2 days of natural aging and an artificial aging at temperatures between 120 to 200° C. for 1 to 24 h in single or dual-stage aging.