# US 2024/0200169 A1 · Copper alloy sheet material and method for producing the copper alloy sheet material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0200169 A1
- Document ID: US20240200169A1
- Status: Published application
- Kind: A1
- Application number: 18/554,884
- Filed: 2022-06-21
- Published: 2024-06-20
- Earliest claimed: 2021-06-28
- Assignees: Dowa Metaltech Co., Ltd.
- Applicants: Dowa Metaltech Co., Ltd.
- Inventors: Ryosuke MIYAHARA; Tomohiro KAWAKAMI; Yuta SASAI; Tomotsugu AOYAMA; Hiroto NARIEDA
- Web page: https://patentgrep.com/patent/US20240200169A1

## CPC

- C22C 9/06: with nickel or cobalt as the next major constituent
- C22C 9/02: with tin as the next major constituent
- C22F 1/08: of copper or alloys based thereon
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

There is provided a copper alloy sheet material, containing: 0.0005% by mass or more and 0.1% by mass or less of Ni, 0.0005% by mass or more and 0.1% by mass or less of Sn, 100 ppm or less of C, 800 ppm or less of O, 10 ppm or less of H, and 50 ppm or less of Ag, with a balance being Cu and impurities, wherein a total content of Ni and Sn is 0.001% by mass or more and 0.11% by mass or less, and when a content of the impurities is expressed as A to B (ppm) in consideration of a quantitative lower limit of each element (here, A is a total impurity content when a content of elements less than the quantitative lower limit is deemed 0 ppm, and B is a total impurity content when a content of the element less than the quantitative lower limit is deemed the quantitative lower limit of each element), A is 100 or less and B is 250 or less.

## Claims

### Claim 1

A copper alloy sheet material, containing 0.0005% by mass or more and 0.1% by mass or less of Ni, 0.0005% by mass or more and 0.1% by mass or less of Sn, 100 ppm or less of C, 800 ppm or less of 0, 10 ppm or less of H, and 50 ppm or less of Ag, with a balance being Cu and impurities,
wherein a total content of the Ni and the Sn is 0.001% by mass or more and 0.11% by mass or less, and
when a content of the impurities are expressed as A to B (ppm) in consideration of a quantitative lower limit of each element (here, A is a total impurity content when a content of an element less than the quantitative lower limit is deemed 0 ppm, and B is a total impurity content when a content of the element less than the quantitative lower limit is deemed the quantitative lower limit of each element), A is 100 or less and B is 250 or less.

### Claim 2 (depends on 1)

The copper alloy sheet material according to claim 1, containing 1 to 50 ppm of S.

### Claim 3 (depends on 1)

The copper alloy sheet material according to claim 1, wherein conductivity of the copper alloy sheet material is 92 to 102% IACS.

### Claim 4 (depends on 1)

The copper alloy sheet material according to claim 1, wherein an average crystal grain size of the copper alloy sheet material is 1 to 30 μm.

### Claim 5 (depends on 1)

The copper alloy sheet material according to claim 1, wherein a ratio (HV1/HV0) of Vickers hardness HV1 after holding the copper alloy sheet material at 350° C. for 5 minutes in the atmosphere, with respect to Vickers hardness HV0 of the copper alloy sheet material before holding, is 0.80 or more.

### Claim 6 (depends on 1)

The copper alloy sheet material according to claim 1, wherein the copper alloy sheet material has an average crystal grain size of 100 μm or less after being held at 800° C. for 1 hour.

### Claim 7

A method for producing a copper alloy sheet material, comprising:
applying hot-rolling to a copper alloy; then,
applying cold-rolling to the copper alloy;
applying recrystallization-annealing to the cold-rolled copper alloy; then,
applying final cold-rolling to the copper alloy,
the copper alloy containing: 0.0005% by mass or more and 0.1% by mass or less of Ni, 0.0005% by mass or more and 0.1% by mass or less of Sn, 100 ppm or less of C, 800 ppm or less of O, 10 ppm or less of H, and 50 ppm or less of Ag, with a balance being Cu and impurities,
wherein a total content of the Ni and the Sn is 0.001% by mass or more and 0.11% by mass or less, and
when a content of the impurities is expressed as A to B (ppm) in consideration of a quantitative lower limit of each element (here, A is a total impurity content when a content of an element less than a quantitative lower limit is deemed 0 ppm, and B is a total impurity content when a content of the element less than the quantitative lower limit is deemed the quantitative lower limit of each element), A is 100 or less and B is 250 or less.

### Claim 8 (depends on 1)

A heat dissipating part in which the copper alloy sheet material of claim 1 is used.

### Claim 9 (depends on 1)

An electronic part in which the copper alloy sheet material according to claim 1 is bonded to an insulating substrate.