# US 2024/0200168 A1 · Copper alloy material and shunt resistor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0200168 A1
- Document ID: US20240200168A1
- Status: Published application
- Kind: A1
- Application number: 18/529,604
- Filed: 2023-12-05
- Published: 2024-06-20
- Earliest claimed: 2022-12-19
- Assignees: Koa Corporation
- Applicants: Koa Corporation
- Inventors: Yoshitaka KUMEDA; Tadahiko Yoshioka
- Web page: https://patentgrep.com/patent/US20240200168A1

## CPC

- C22C 9/05: with manganese as the next major constituent
- G01R 1/203: {Resistors used for electric measuring, e.g. decade resistors standards, resistors for comparators, series resistors, shunts (resistors in general H01C; microwave or radiowave terminations H01P1/26; coupling devices H01R)}
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- G01R: MEASURING ELECTRIC VARIABLES; MEASURING MAGNETIC VARIABLES (indicating correct tuning of resonant circuits H03J3/12)

## Abstract

A copper alloy material having a low volume resistivity, a low TCR and a small thermal electromotive force with respect to copper and a shunt resistor comprising a resistive body formed by the copper alloy material are provided. The copper-manganese-based copper alloy material includes 4.5-5.5 mass % of manganese, 0.1-0.3 mass % of iron, 0.1-0.5 mass % of tin, and a balance being copper. A volume resistivity is 15-25 μΩ·cm. An absolute value of TCR is 150×10−6/K or less. A thermal electromotive force with respect to copper is 1 μV/K or less. A resistance value change is −0.3% to 0% in a heat resistance test of 175° C. for 3000 hours.

## Claims

### Claim 1

A copper-manganese-based copper alloy material including 4.5-5.5 mass % of manganese, 0.1-0.3 mass % of iron, 0.1-0.5 mass % of tin, and a balance being copper.

### Claim 2 (depends on 1)

The copper alloy material according to claim 1, wherein a volume resistivity is 15-25 μΩ·cm.

### Claim 3 (depends on 1)

The copper alloy material according to claim 1, wherein an absolute value of TCR is 150×10−6/K or less.

### Claim 4 (depends on 1)

The copper alloy material according to claim 1, wherein a thermal electromotive force with respect to copper is 1 μV/K or less.

### Claim 5 (depends on 1)

The copper alloy material according to claim 1, wherein a resistance value change is −0.3% to 0% in a heat resistance test of 175° C. for 3000 hours.

### Claim 6

A shunt resistor for current detection comprising a resistive body and an electrode, wherein:
the resistive body is formed by a copper-manganese-based copper alloy material; and
the copper alloy material includes 4.5-5.5 mass % of manganese, 0.1-0.3 mass % of iron, 0.1-0.5 mass % of tin, and a balance being copper.