# US 2024/0199866 A1 · Resin composition, molded article, modifier for abs resin, method for manufacturing resin composition, and method for modifying abs resin

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0199866 A1
- Document ID: US20240199866A1
- Status: Published application
- Kind: A1
- Application number: 18/441,376
- Filed: 2024-02-14
- Published: 2024-06-20
- Earliest claimed: 2021-09-29
- Assignees: Mitsubishi Chemical Corporation
- Applicants: Mitsubishi Chemical Corporation
- Inventors: Yuuta KOBAYASHI
- Web page: https://patentgrep.com/patent/US20240199866A1

## CPC

- C08L 23/26: modified by chemical after-treatment (saponified copolymers C08L23/0861; unsaturated acid salts C08L23/0876)
- C08F 8/14: Esterification
- C08F 216/06: Polyvinyl alcohol {; Vinyl alcohol}
- C08G 63/08: Lactones or lactides
- C08L 23/0846: with unsaturated hydrocarbons containing atoms other than carbon or hydrogen
- C08L 55/02: ABS [Acrylonitrile-Butadiene-Styrene] polymers
- C08L 2203/16: used for films
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

A resin composition including: an ABS resin (A); and an ethylene-vinyl alcohol resin (B), wherein the ethylene-vinyl alcohol resin (B) includes a modified ethylene-vinyl alcohol resin (B1) having a structural unit represented by chemical formula (1), wherein X represents an organic chain having a heteroatom; and n represents a positive integer.

## Claims

### Claim 1

A modifier for an ABS resin, the modifier comprising a modified ethylene-vinyl alcohol resin (B1) having a structural unit represented by the following chemical formula (1),
wherein X represents an organic chain having a heteroatom; and n represents a positive integer.

### Claim 2 (depends on 1)

A resin composition comprising the modifier for an ABS resin according to claim 1 and an ABS resin (A).

### Claim 3

A resin composition, comprising:
an ABS resin (A); and
an ethylene-vinyl alcohol resin (B),
wherein the resin composition has a mass change rate in of not more than 0.45% in an immersion test conducted as follows:
a mass (W1) of a specimen of the resin composition that is 80 mm in length by 10 mm in width by 4 mm in thickness is measured; then, the specimen is immersed in a test oil at 23° C. for 168 hours; then, the test oil is wiped off; and a mass (W2) of the specimen is measured to determine the mass change rate (%) with the following formula:
Mass change rate (%)=(W2−W1)/W1×100.

### Claim 4 (depends on 2)

The resin composition according to claim 2, wherein the modified ethylene-vinyl alcohol resin (B1) is contained by 1 to 70 parts by mass relative to 100 parts by mass of a total of the ABS resin (A) and the modified ethylene-vinyl alcohol resin (B1).

### Claim 5 (depends on 2)

The resin composition according to claim 2, wherein the modified ethylene-vinyl alcohol resin (B1) is contained by 1 to 40 parts by mass relative to 100 parts by mass of a total of the ABS resin (A) and the modified ethylene-vinyl alcohol resin (B1).

### Claim 6 (depends on 1)

The modifier for an ABS resin according to claim 1, wherein the modified ethylene-vinyl alcohol resin (B1) having the structural unit represented by the chemical formula (1) has a modification rate of 0.1 to 30 mol %.

### Claim 7 (depends on 1)

The modifier for an ABS resin according to claim 1, wherein the modified ethylene-vinyl alcohol resin (B1) having the structural unit represented by the chemical formula (1) is a ring-opened polymer of a lactone ring having 3 to 10 carbon atoms constituting the ring.

### Claim 8 (depends on 2)

A molded article, formed with the resin composition according to claim 2.

### Claim 9 (depends on 8)

The molded article according to claim 8, wherein the molded article is a sheet or a film.

### Claim 10 (depends on 1)

A method for manufacturing a resin composition, the method comprising blending the modifier for an ABS resin according to claim 1 with an ABS resin (A).

### Claim 11 (depends on 1)

A method for modifying an ABS resin, the method comprising blending the modifier for an ABS resin according to claim 1 with an ABS resin (A).

### Claim 12

A molded article formed from a resin composition comprising: an ABS resin (A); and an ethylene-vinyl alcohol resin (B), wherein the molded article has a contact angle of less than 85°.

### Claim 13 (depends on 3)

The resin composition according to claim 3, wherein the ethylene-vinyl alcohol resin (B) is contained by 1 to 70 parts by mass relative to 100 parts by mass of a total of the ABS resin (A) and the ethylene-vinyl alcohol resin (B).

### Claim 14 (depends on 3)

The resin composition according to claim 3, wherein the ethylene-vinyl alcohol resin (B) is contained by 1 to 40 parts by mass relative to 100 parts by mass of a total of the ABS resin (A) and the ethylene-vinyl alcohol resin (B).

### Claim 15 (depends on 3)

A molded article, formed with the resin composition according to claim 3.

### Claim 16 (depends on 15)

The molded article according to claim 15, wherein the molded article is a sheet or a film.