# US 2024/0199865 A1 · Polypropylene composition for cable insulation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0199865 A1
- Document ID: US20240199865A1
- Status: Published application
- Kind: A1
- Application number: 18/549,717
- Filed: 2022-03-23
- Published: 2024-06-20
- Earliest claimed: 2021-03-25
- Assignees: Borealis AG
- Applicants: Borealis AG
- Inventors: Thomas Gkourmpis; Katja Klimke; Per-Ola Hagstrand; Ulf Nilsson; Lars Efraimsson; Anette Johansson
- Web page: https://patentgrep.com/patent/US20240199865A1

## CPC

- C08L 23/142: {at least partially crystalline copolymers of propene with other olefins}
- C08K 5/1575: Six-membered rings
- H01B 3/441: {from alkenes}
- C08L 2203/202: use in electrical wires or wirecoating
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/24: Crystallisation aids
- C08L 2207/02: Heterophasic composition
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})

## Abstract

The present invention relates to a polypropylene composition comprising (A) a copolymer of propylene and comonomer units selected from ethylene and alpha-olefins having from 4 to 12 carbon atoms with a total amount of comonomer units of from 10.0 to 16.0 wt %, based on the total amount of monomer units in the polypropylene composition, and (B) an alpha-nucleating agent; wherein the polypropylene composition has a xylene cold soluble (XCS) fraction in a total amount of from 25.0 to 50.0 wt %, based on the total weight amount of the polypropylene composition, with an amount of comonomer units of at least 23.0 wt %, based on the total amount of monomer units in the xylene cold soluble (XCS) fraction, a melt flow rate MFR2 of from 0.5 to 5.0 g/10 min, and a flexural modulus of not more than 470 MPa, an article comprising said polypropylene composition, preferably a cable comprising an insulation layer comprising said polypropylene composition and the use of said polypropylene composition as cable insulation for medium and high voltage cables.

## Claims

### Claim 1

A polypropylene composition comprising:
(A) a copolymer of propylene and comonomer units selected from ethylene and alpha-olefins having from 4 to 12 carbon atoms with a total amount of comonomer units of from 10.0 to 16.0 wt %, based on the total amount of monomer units in the polypropylene composition, and
(B) an alpha-nucleating agent;
wherein the polypropylene composition has
a xylene cold soluble (XCS) fraction in a total amount of from 25.0 to 50.0 wt %, based on the total weight amount of the polypropylene composition, with an amount of comonomer units of at least 23.0 wt %, such as 23.0 to 35.0 wt %, based on the total amount of monomer units in the xylene cold soluble (XCS) fraction,
a melt flow rate MFR2 of from 0.5 to 5.0 g/10 min, and
a flexural modulus of not more than 470 MPa.

### Claim 2 (depends on 1)

The polypropylene composition according to claim 1, wherein the xylene cold solubles (XCS) fraction has an intrinsic viscosity of from 150 to 350 cm3/g, measured in decalin.

### Claim 3 (depends on 1)

The polypropylene composition according to claim 1, having a fraction insoluble in cold xylene (XCI) with an amount of comonomer units of from 3.0 to 9.0 wt %, based on the total amount of monomer units in the fraction insoluble in cold xylene (XCI).

### Claim 4 (depends on 1)

The polypropylene composition according to claim 1, wherein the copolymer of propylene and comonomer units selected from ethylene and alpha-olefins having from 4 to 12 carbon atoms is a heterophasic copolymer of propylene which comprises a matrix phase and an elastomeric phase dispersed in said matrix phase, which comprises two glass transition temperatures attributed to the matrix phase and the elastomeric phase, wherein the glass transition temperature attributed to the matrix phase Tg (matrix) is in the range of from −1.0 to −15.0° C., and/or the glass transition temperature attributed to the elastomeric phase Tg (EPR) is in the range of from −40.0 to −55.0° C.

### Claim 5 (depends on 1)

The polypropylene composition according to claim 1, having a melting temperature Tm of from 140 to 159° C.

### Claim 6 (depends on 1)

The polypropylene composition according to claim 1, having a crystallization temperature Tc of from 105 to 130° C.

### Claim 7 (depends on 1)

The polypropylene composition according to claim 1, having a Charpy notched impact strength at −20° C. of at least 3.5 KJ/m2.

### Claim 8 (depends on 1)

The polypropylene composition according to claim 1, having a Charpy notched impact strength at 23° C. of at least 70.0 KJ/m2.

### Claim 9 (depends on 1)

The polypropylene composition according to claim 1, having a melt flow rate MFR2 of from more than 0.5 to 2.5 g/10 min.

### Claim 10 (depends on 1)

The polypropylene composition according to claim 1, having a melt flow rate MFR2 of from more than 2.5 to 5.0 g/10 min.

### Claim 11

The polypropylene composition according to 10, being subjected to vis-breaking.

### Claim 12 (depends on 1)

The polypropylene composition according to claim 1, being free of a dielectric fluid.

### Claim 13 (depends on 1)

An article comprising the polypropylene composition according to claim 1, comprising an insulation layer comprising the polypropylene composition.

### Claim 14 (depends on 13)

The article according to claim 13, being a cable comprising an insulation layer comprising the polypropylene composition and having a Weibull alpha-value of at least 35 kV/mm and/or a Weibull beta-value of at least 7.5, measured on a 10 kV cable.

### Claim 15 (depends on 13)

The article according to claim 13, wherein the polypropylene composition is a cable insulation for medium and high voltage cables.