# US 2024/0199824 A1 · Methods of manufacturing articles from casson compositions and articles formed therefrom

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0199824 A1
- Document ID: US20240199824A1
- Status: Published application
- Kind: A1
- Application number: 18/287,819
- Filed: 2022-04-20
- Published: 2024-06-20
- Earliest claimed: 2021-04-21
- Assignees: Sabic Global Technologies B.V.
- Applicants: Sabic Global Technologies B.V.
- Inventors: Tariq Syed; Zahir Bashir; Saleh Al-Karri; Fayez Abdullah Alfayez; Azzedine Kioul; Toseef Ahmed
- Web page: https://patentgrep.com/patent/US20240199824A1

## CPC

- C08J 3/201: {Pre-melted polymers}
- C08L 23/12: Polypropene
- C08L 67/03: the dicarboxylic acids and dihydroxy compounds having the carboxyl- and the hydroxy groups directly linked to aromatic rings
- C08J 2323/12: Polypropene
- C08J 2367/03: the dicarboxylic acids and dihydroxy compounds having the hydroxy and the carboxyl groups directly linked to aromatic rings
- C08J 2467/03: the dicarboxylic acids and dihydroxy compounds having the hydroxy and the carboxyl groups directly linked to aromatic rings
- C08L 2205/06: having improved processability or containing aids for moulding methods
- C08L 2205/08: containing additives to improve the compatibility between two polymers
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A method of manufacturing an article includes melt-mixing a first polymer with a second polymer and optionally an additive to form a thermoplastic composition, the first polymer having a first melting point or a first glass transition temperature T1, the second polymer having a second melting point or a second glass transition temperature T2 that is 30° C. to 150° C. higher than T1: and forming the article from the thermoplastic composition at a temperature between T1 and T2, such as via sheet extrusion, thermoforming, pipe extrusion, extrusion molding, injection molding, extrusion molding, blow molding, compression molding, or additive manufacturing. The first polymer and the second polymer can have a volume ratio of 75:25 to 35:65 with a co-continuous morphology in the thermoplastic composition, with the second polymer providing a network for containing a melt of the first polymer.

## Claims

### Claim 1

A method of manufacturing an article, the method comprising:
melt-mixing a first polymer with a second polymer and optionally an additive to form a thermoplastic composition,
the first polymer having a first melting point or a first glass transition temperature T1,
the second polymer having a second melting point or a second glass transition temperature T2 that is 30° C. to 150° C. higher than T1,
the first polymer and the second polymer having a co-continuous morphology in the thermoplastic composition, with the second polymer providing a network for containing a melt of the first polymer; and
forming the article from the thermoplastic composition at a temperature between T1 and T2.

### Claim 2 (depends on 1)

The method of claim 1, wherein forming the article is done via sheet extrusion, thermoforming, pipe extrusion, extrusion molding, injection molding, extrusion molding, blow molding, compression molding, or additive manufacturing,
wherein the first polymer and the second polymer have a volume ratio of 75:25 to 35:65; and
the article has a co-continuous morphology, with the second polymer providing a network for containing the first polymer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the thermoplastic composition has a first phase comprising the first polymer, and a second phase comprising the second polymer, and greater than 80% of the first phase and greater than 80% of the second phase are continuous as observed in an image of scanning electron microscopy or transmission electron microscopy.

### Claim 4 (depends on 1)

The method of claim 1, wherein the article has a first phase comprising the first polymer, and a second phase comprising the second polymer, and greater than 80% of the first phase and greater than 80% of the second phase are continuous as observed in an image of scanning electron microscopy or transmission electron microscopy.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first polymer and the second polymer have a volume ratio of 70:30 to 40:60.

### Claim 6 (depends on 1)

The method of claim 1, wherein T2 is 40° C. to 120° C. higher than T1.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first polymer and the second polymer are independently selected from a polyolefin, a polycarbonate, a polyester, a polyetherimide, a polyketone, a polyamide, a polyoxymethylene, and a polyacrylate.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first polymer comprises a polypropylene, the second polymer comprises a poly(ethylene terephthalate), and the polypropylene and the poly(ethylene terephthalate) have a volume ratio of 70:30 to 50:50.

### Claim 9 (depends on 1)

The method of claim 1, wherein the thermoplastic composition comprises 0.5 to 15 wt % of the additive based on the total weight of the thermoplastic composition, the additive comprising at least one of a compatibilizer, a filler, a dye, a pigment, an antioxidant, an ultra-violet absorber, an infrared absorber, a flame retardant, a mold release agent, or an impact modifier.

### Claim 10 (depends on 1)

The method of claim 1, wherein the thermoplastic composition comprises 0.5 to 15 wt % of the additive, the additive comprising a functionalized polyolefin.

### Claim 11 (depends on 1)

The method of claim 1, wherein the first polymer, the second polymer, and the optional additive are mixed at a temperature that is equal to or higher than T2 to form the thermoplastic composition.

### Claim 12 (depends on 1)

The method of claim 1, wherein forming the article comprises extruding or molding the thermoplastic composition at a temperature that is between T2−5° C. and T2−30° C. to form a preform.

### Claim 13 (depends on 12)

The method of claim 12, wherein the preform is processed at a temperature of T1+10° C. to T1+50° C. to form the article.

### Claim 14 (depends on 1)

An article manufactured by the method of claim 1.

### Claim 15 (depends on 13)

The article of claim 13, wherein the article is a Casson fluid, exhibiting no flow at low shear rates below a critical shear rate and a shear thinning behavior at high shear rates above the critical shear rate.

### Claim 16 (depends on 1)

The method of claim 1, wherein the article is a Casson fluid, exhibiting no flow at low shear rates below a critical shear rate and a shear thinning behavior at high shear rates above the critical shear rate.

### Claim 17

A method of manufacturing an article, the method comprising:
melt-mixing a first polymer with a second polymer and 5 to 15 wt % of an additive based on the total weight of the thermoplastic composition to form a thermoplastic composition,
the first polymer having a first melting point or a first glass transition temperature T1,
the second polymer having a second melting point or a second glass transition temperature T2 that is 30° C. to 150° C. higher than T1,
the first polymer and the second polymer having a co-continuous morphology in the thermoplastic composition, with the second polymer providing a network for containing a melt of the first polymer,
the additive comprising a functionalized polyolefin; and
forming the article from the thermoplastic composition at a temperature between T1 and T2, wherein the first polymer and the second polymer have a volume ratio of 70:30 to 40:60.

### Claim 18 (depends on 17)

The method of claim 17, wherein the article has a co-continuous morphology, with the second polymer providing a network for containing the first polymer.

### Claim 19

A method of manufacturing an article, the method comprising:
melt-mixing a first polymer with a second polymer and optionally an additive to form a thermoplastic composition,
the first polymer having a first melting point or a first glass transition temperature T1,
the second polymer having a second melting point or a second glass transition temperature T2 that is 30° C. to 150° C. higher than T1,
the first polymer and the second polymer having a co-continuous morphology in the thermoplastic composition, with the second polymer providing a network for containing a melt of the first polymer; and
extruding or molding the thermoplastic composition at a temperature that is between T2−5° C. and T2−30° C. to form a preform; and
processing the preform at a temperature of T1+10° C. to T1+50° C. to form the article;
wherein the first polymer comprises a polypropylene, the second polymer comprises a poly(ethylene terephthalate), and the polypropylene and the poly(ethylene terephthalate) have a volume ratio of 70:30 to 50:50.

### Claim 20 (depends on 19)

The method of claim 19, wherein the article has a co-continuous morphology, with the second polymer providing a network for containing the first polymer.