# US 2024/0199823 A1 · Method for manufacturing stretchable electrochromic device, and stretchable electrochromic device manufactured thereby

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0199823 A1
- Document ID: US20240199823A1
- Status: Published application
- Kind: A1
- Application number: 18/235,348
- Filed: 2023-08-18
- Published: 2024-06-20
- Earliest claimed: 2022-12-08
- Assignees: Korea University of Technology and Education Industry-University Cooperation
- Applicants: Korea University of Technology and Education Industry-University Cooperation
- Inventors: Jin Woo BAE; Seung Ju OH
- Web page: https://patentgrep.com/patent/US20240199823A1

## CPC

- C08J 3/11: from solid polymers
- C08J 3/215: at least one additive being also premixed with a liquid phase
- C08J 5/18: Manufacture of films or sheets
- C08J 7/04: Coating
- C09K 9/00: Tenebrescent materials, i.e. materials for which the range of wavelengths for energy absorption is changed as a result of excitation by some form of energy
- C09K 9/02: Organic tenebrescent materials
- G02F 1/0131: {based on photo-elastic effects, e.g. mechanically induced birefringence}
- G02F 1/15: based on an electrochromic effect
- G02F 1/15165: {Polymers}
- G02F 1/153: Constructional details
- C08J 2327/06: Homopolymers or copolymers of vinyl chloride
- G02F 2001/164: {the electrolyte is made of polymers}
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

The present invention relates to a method for manufacturing a stretchable electrochromic device and a stretchable electrochromic device manufactured thereby, and more specifically, the present invention is characterized in that a stretchable electrochromic device, which is manufactured by stretching color changeable polymer gel, and then coating one surface and/or the other surface thereof with a metal solution, has excellent water resistance and initial transmittance.

## Claims

### Claim 1

A method for manufacturing a stretchable electrochromic device, the method comprising:
stretching polymer gel;
coating a metal solution on one surface of the stretched polymer gel; and
restoring the stretched polymer gel to its original state.

### Claim 2 (depends on 1)

The method of claim 1, wherein
the polymer gel comprises a polymer resin, a plasticizer, an ionic liquid, a color changing material, and a reducing agent.

### Claim 3 (depends on 2)

The method of claim 2, wherein
the polymer resin comprises a polymer resin selected from the group consisting of polyvinyl chloride (PVC), polytetrafluoroethylene (PTFE), polyurethane (PU), polymethyl methacrylate (PMMA), polydimethylsiloxane (PDMS), polyvinyl alcohol (PVA), polyvinylpyrrolidone (PVP), polyethylene oxide (PEO), polyimide (PI), polyethylene terephthalate (PET), and combinations thereof.

### Claim 4 (depends on 2)

The method of claim 2, wherein
the ionic liquid comprises an ionic liquid selected from the group consisting of a neutral liquid, an anionic liquid, a cationic liquid, and combinations thereof.

### Claim 5 (depends on 4)

The method of claim 4, wherein
the neutral liquid comprises a neutral liquid selected from the group consisting of 1-ethyl-3-methylimidazolium bis(trifluoromethylsulfonyl)imide (Emim TFSI), 1-methyl-3-propylimidazolium iodide (MPII), 1-ethyl-3-methylimidazolium tetrafluoroborate (EMIBF4), 1-ethyl-3-methylimidazolium (EMIT), 1-ethyl-3- trifluoromethanesulfonate methylimidazolium hydrogensulfate (EMIHSO4), N-methyl-N-butylpyrrolidinium bis(trifluoromethanesulfonyl) imide (PYRTFSI), and combinations thereof.

### Claim 6 (depends on 4)

The method of claim 4, wherein
the anionic liquid comprises an anionic liquid selected from the group consisting of trifluoroacetate ([tfa]−), trifluoromethanesulfonate ([CF3SO3]−), bis(fluorosulfonyl)imide ([N(SO2F)2]−), bis(trifluoromethanesulfonyl)imide ([N(SO2CF3)2]−), dicyanamide ([N(CN)2]−), tetracyanoborate ([B(CN)4]−), dihydrogenphosphate ([H2PO4]−), hydrogen sulfate ([HSO4]−), and combinations thereof.

### Claim 7 (depends on 4)

The method of claim 4, wherein
the cationic liquid comprises a cationic liquid selected from the group consisting of imidazolium, pyrrolidinium, piperidinium alkylmethylimidazolium, and combinations thereof.

### Claim 8 (depends on 2)

The method of claim 2, wherein
based on 100 parts by weight of the polymer resin, the content of the ionic liquid is 40 parts by weight to 140 parts by weight,
the content of the plasticizer is 300 parts by weight to 1,500 parts by weight, and
the contents of the color changing material and the reducing agent are respectively 10 parts by weight to 140 parts by weight.

### Claim 9 (depends on 1)

The method of claim 1, wherein
the polymer gel is stretched by 20% to 80% with respect to the length of the polymer gel.

### Claim 10 (depends on 1)

The method of claim 1, wherein
the metal solution comprises a solution of a metal selected from a group consisting of silver (Ag), gold (Au), platinum (Pt), palladium (Pd), iridium (Ir), rhodium (Rh), ruthenium (Ru), osmium (Os) and combinations thereof.

### Claim 11 (depends on 1)

The method of claim 1, wherein
the concentration of the metal solution is 1 mg/mL to 20 mg/mL.

### Claim 12 (depends on 1)

The method of claim 1, wherein
the method for manufacturing a stretchable electrochromic device further comprises,
after the coating of the metal solution on one surface of the stretched polymer gel,
spraying water on one surface of the polymer gel coated with the metal solution and performing annealing.

### Claim 13 (depends on 12)

The method of claim 12, wherein
the annealing is performed for 10 seconds to 1 minute.

### Claim 14 (depends on 1)

The method of claim 1, wherein
the restoring of the polymer gel to its original state is performed at a rate of 0.01 mm/s to 5.0 mm/s.

### Claim 15 (depends on 1)

The method of claim 1, wherein
the method for manufacturing a stretchable electrochromic device further comprises,
after the restoring of the stretched polymer gel to its original state,
performing the same processes on the other surface of the polymer gel.

### Claim 16 (depends on 1)

A stretchable electrochromic device manufactured by the method for manufacturing a stretchable electrochromic device according to claim 1.

### Claim 17 (depends on 16)

A product comprising the stretchable electrochromic device according to claim 16.