# US 2024/0199820 A1 · Method for Preparing Cellulose and Lignin Oil by Depolymerizing Lignocellulose Without Exogenous Hydrogen

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0199820 A1
- Document ID: US20240199820A1
- Status: Published application
- Kind: A1
- Application number: 18/193,851
- Filed: 2023-03-31
- Published: 2024-06-20
- Earliest claimed: 2022-12-13
- Assignees: East China University of Science and Technology
- Applicants: East China University of Science and Technology
- Inventors: Yanqin WANG; Hao ZHOU; Yong GUO; Xiaohui LIU
- Web page: https://patentgrep.com/patent/US20240199820A1

## CPC

- C08H 8/00: Macromolecular compounds derived from lignocellulosic materials {(pretreatment thereof B27N)}
- B01J 23/42: Platinum
- B01J 23/44: Palladium
- B01J 23/462: {Ruthenium}
- B01J 23/56: Platinum group metals
- B01J 23/892: {Nickel and noble metals}
- C07G 1/00: Low-molecular-weight derivatives of lignin (high-molecular-weight derivatives of lignin {C08H6/00})
- D21C 5/00: Other processes for obtaining cellulose, e.g. cooking cotton linters (obtaining fibres for spinning D01C); {Processes characterised by the choice of cellulose-containing starting materials}
- C08H: DERIVATIVES OF NATURAL MACROMOLECULAR COMPOUNDS (polysaccharides C08B; natural rubber C08C; natural resins or their derivatives C09F; bituminous materials C10)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07G: COMPOUNDS OF UNKNOWN CONSTITUTION (sulfonated fats, oils or waxes of undetermined constitution C07C309/62)
- D21C: PRODUCTION OF CELLULOSE BY REMOVING NON-CELLULOSE SUBSTANCES FROM CELLULOSE-CONTAINING MATERIALS; REGENERATION OF PULPING LIQUORS; APPARATUS THEREFOR

## Abstract

Disclosed is a method for preparing cellulose and lignin oil by depolymerizing lignocellulose without exogenous hydrogen, including: performing reaction on the lignocellulose dispersed into an aqueous medium at 120° C. to 180° C. under the action of a catalyst; and separating a reaction product to obtain the cellulose and the lignin oil. The catalyst includes a carrier and an active ingredient loaded on the carrier, where the active ingredient is selected from one of platinum, palladium, ruthenium and nickel; the carrier is selected from one of a metal oxide, a metal composite material, silicon dioxide, nitrogen-doped carbon, molybdenum carbide and molybdenum nitride; and the metal oxide is selected from one of niobium oxide, tantalum oxide, tungsten oxide, zirconium oxide, aluminum oxide, titanium dioxide and molybdenum oxide.

## Claims

### Claim 1

A method for preparing cellulose and lignin oil by depolymerizing lignocellulose without exogenous hydrogen, comprising:
reacting the lignocellulose dispersed into an aqueous medium at 120° C. to 180° C. under the action of a catalyst; and
separating a reaction product to obtain the cellulose and the lignin oil,
wherein the catalyst comprises a carrier and an active ingredient supported on the carrier, wherein the active ingredient comprises at least one of platinum, palladium, ruthenium, nickel, and alloy thereof; the carrier comprises at least one of a metal oxide, a metal composite material, silicon dioxide, nitrogen-doped carbon, molybdenum carbide and molybdenum nitride; the metal oxide comprises at least one of niobium oxide, tantalum oxide, tungsten oxide, zirconium oxide, aluminum oxide, titanium dioxide and molybdenum oxide; and the metal composite material comprises at least one of a lanthanum nickel composite material, a magnesium aluminum composite material, a cobalt aluminum composite material, a zinc aluminum composite material, an iron aluminum composite material and a nickel aluminum composite material.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the lignocellulose comprises at least one of a woody plant and a herbaceous plant; the woody plant comprises at least one of birch, beech, poplar, camphorwood, oak, Nanmu, Schima superba, walnut, Chinese oak, ironwood, maple, teak, pine, Chinese fir and cedarwood; and the herbaceous plant comprises at least one of switchgrass, bamboo, wheat straw, rice straw and corn straw.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the lignocellulose comprises at least one of birch, poplar, pine, switchgrass and corn straw.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the active ingredient in the catalyst is platinum;
and the carrier comprises at least one of a nickel aluminum composite material, a magnesium aluminum composite material, a zinc aluminum composite material, a cobalt aluminum composite material, an iron aluminum composite material, molybdenum nitride, aluminum oxide, molybdenum carbide, molybdenum oxide, zirconium oxide, nitrogen-doped carbon, niobium oxide, titanium dioxide and tungsten oxide.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the active ingredient in the catalyst is the platinum; and the carrier comprises at least one of the nickel aluminum composite material, the magnesium aluminum composite material, the cobalt aluminum composite material, the zinc aluminum composite material, the iron aluminum composite material, the aluminum oxide, the molybdenum nitride, the molybdenum carbide, the nitrogen-doped carbon and the zirconium oxide.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the active ingredient in the catalyst is the platinum; and the carrier comprises at least one of the nickel aluminum composite material, the magnesium aluminum composite material, the zinc aluminum composite material, the cobalt aluminum composite material, the iron aluminum composite material, the molybdenum nitride, the aluminum oxide and the molybdenum carbide.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the active ingredient in the catalyst is the platinum, and the carrier comprises at least one of the nickel aluminum composite material, the magnesium aluminum composite material, the zinc aluminum composite material, the cobalt aluminum composite material and the iron aluminum composite material.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the active ingredient in the catalyst is the platinum, and the carrier comprises at least one of the magnesium aluminum composite material, the zinc aluminum composite material, the cobalt aluminum composite material and the nickel aluminum composite material.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the active ingredient in the catalyst is the platinum, and the carrier is selected from the nickel aluminum composite material and the magnesium aluminum composite material.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the active ingredient in the catalyst comprises at least one of palladium, ruthenium, nickel, platinum ruthenium alloy, platinum palladium alloy, platinum nickel alloy and ruthenium nickel alloy; and the carrier comprises a nickel aluminum composite material.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the active ingredient in the catalyst is selected from at least one of the platinum ruthenium alloy, the platinum palladium alloy, the platinum nickel alloy and the ruthenium nickel alloy; and the carrier is selected from the nickel aluminum composite material.

### Claim 12 (depends on 8)

The method according to claim 8, wherein the active ingredient in the catalyst comprises at least one of the platinum ruthenium alloy and the platinum palladium alloy, and the carrier is the nickel aluminum composite material.

### Claim 13 (depends on 1)

The method according to claim 1, wherein in the catalyst, the mass fraction of the active ingredient in the total amount of the catalyst is 0.5% to 5%.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the aqueous medium comprises at least one of water, a mixture of water and cyclohexane, a mixture of water and dioxane, and a mixture of water and tetrahydrofuran.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the weight ratio of the lignocellulose to the catalyst is 1:(0.01-0.2); the reaction temperature is 130° C. to 150° C.; and the reaction retention time is 2 to 30 hours.