# US 2024/0199819 A1 · A binder composition free of phenol compound

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0199819 A1
- Document ID: US20240199819A1
- Status: Published application
- Kind: A1
- Application number: 18/286,583
- Filed: 2021-04-15
- Published: 2024-06-20
- Earliest claimed: 2021-04-15
- Applicants: Upm-Kymmene Corporation
- Inventors: Sanna VALKONEN
- Web page: https://patentgrep.com/patent/US20240199819A1

## CPC

- C08H 6/00: {Macromolecular compounds derived from lignin, e.g. tannins, humic acids}
- C08G 8/24: with mixtures of two or more phenols which are not covered by only one of the groups C08G8/10 - C08G8/20
- C08G 14/04: with phenols
- C08L 97/005: {Lignin}
- C09J 197/005: {Lignin}
- C08H: DERIVATIVES OF NATURAL MACROMOLECULAR COMPOUNDS (polysaccharides C08B; natural rubber C08C; natural resins or their derivatives C09F; bituminous materials C10)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)

## Abstract

The invention relates to a method for producing a binder composition, without using a compound selected from the class of phenols. The method comprises: (i) heating an aqueous composition comprising lignin in the presence of a catalyst; (ii) mixing a crosslinking agent with the aqueous composition from (i) and heating the same at a temperature of 60-95° C. for pre-polymerizing lignin and crosslinking agent; (iii) mixing tannin with the aqueous composition from (ii) for polymerizing tannin with the pre-polymerized lignin and crosslinking agent until a binder composition with a predetermined viscosity value is formed; wherein the molar ratio of crosslinking agent to lignin and tannin is 0.5-1.7.

## Claims

### Claim 1

A method for producing a binder composition without using a compound selected from the class of phenols, wherein the method comprises:
(i) heating an aqueous composition comprising lignin in the presence of a catalyst at a temperature of 50-95° C. for 0.25-5 hours;
(ii) mixing a crosslinking agent with the aqueous composition from (i) and heating the same at a temperature of 60-95° C. for pre-polymerizing lignin and crosslinking agent; and
(iii) mixing tannin with the aqueous composition from (ii) until a binder composition with a predetermined viscosity value is formed,
wherein the molar ratio of crosslinking agent to lignin and tannin is 0.5-1.7.

### Claim 2 (depends on 1)

The method of claim 1, wherein the total amount of crosslinking agent used for producing the binder composition is 3-7 weight-%, based on the total weight of the binder composition.

### Claim 3 (depends on 1)

The method of claim 1, wherein the molar ratio of crosslinking agent to lignin and tannin is 0.9-1.7.

### Claim 4 (depends on 1)

The method of claim 1, wherein the weight ratio of catalyst to lignin and tannin is 0.20-0.37.

### Claim 5 (depends on 1)

The method of claim 1, wherein the weight ratio of tannin to lignin is 0.05-1.0.

### Claim 6 (depends on 1)

The method of claim 1, wherein step (ii) comprises heating at a temperature of 75-90° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein heating in step (ii) is continued until the aqueous composition has a viscosity value of 100-1200 cp, as measured at a temperature of 25° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein, in step (ii), the molar ratio of cross-linking agent to lignin is 1.2-1.9.

### Claim 9 (depends on 1)

The method of claim 1, wherein tannin is mixed with the aqueous composition while keeping the temperature of the composition at 15-90° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein step (iii) comprises mixing tannin with the aqueous composition from (ii) for polymerizing tannin with the pre-polymerized lignin and crosslinking agent until a binder composition with a predetermined viscosity value is formed.

### Claim 11 (depends on 1)

The method of claim 1, wherein the lignin is softwood Kraft lignin.

### Claim 12 (depends on 1)

The method of claim 1, wherein the crosslinking agent is an aldehyde prepared from bio-methanol.

### Claim 13 (depends on 1)

The method of claim 1, wherein the method comprises dispersing tannin before mixing it with the aqueous composition.

### Claim 14 (depends on 1)

The method of claim 1, wherein mixing in step (iii) is continued until a binder composition with a viscosity value of 150-800 cP is formed.

### Claim 15

A binder composition obtainable by a method comprising:
(i) heating an aqueous composition comprising lignin in the presence of a catalyst at a temperature of 50-95° C. for 0.25-5 hours;
(ii) mixing a crosslinking agent with the aqueous composition from (i) and heating the same at a temperature of 60-95° C. for pre-polymerizing lignin and crosslinking agent; and
(iii) mixing tannin with the aqueous composition from (ii) until a binder composition with a predetermined viscosity value is formed,
wherein the molar ratio of crosslinking agent to lignin and tannin is 0.5-1.7.

### Claim 16 (depends on 15)

An adhesive composition comprising the binder composition of claim 15.

### Claim 17 (depends on 15)

The binder composition of claim 15, wherein the binder composition is configured to be used in an impregnation application, for gluing a wood product or layered wood product or wood panel, for producing a laminate, shuttering film, mineral wool, nonwoven fiber product, molded fiber product, or extruded fiber product.

### Claim 18

A product comprising:
a binder composition obtained by the method comprising (i) heating an aqueous composition comprising lignin in the presence of a catalyst at a temperature of 50-95° C. for 0.25-5 hours, (ii) mixing a crosslinking agent with the aqueous composition from (i) and heating the same at a temperature of 60-95° C. for pre-polymerizing lignin and crosslinking agent, and (iii) mixing tannin with the aqueous composition from (ii) until a binder composition with a predetermined viscosity value is formed, wherein the molar ratio of crosslinking agent to lignin and tannin is 0.5-1.7;
wherein the product has one or more of the following properties:
the amount of formaldehyde emissions being 0.01-0.5 mg/l when measured by desiccator EN ISO 12460-4;
the amount of formaldehyde emissions being 0.01-0.40 mg/m2*h, when measured by gas analysis method EN ISO 12460-3; and
fulfilling the minimum bonding class 1-4, when measured by bonding quality test method EN 314-1 & EN 314-2.