# US 2024/0199818 A1 · Low-refractivity optical clear resin

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0199818 A1
- Document ID: US20240199818A1
- Status: Published application
- Kind: A1
- Application number: 18/080,616
- Filed: 2022-12-13
- Published: 2024-06-20
- Earliest claimed: 2022-12-09
- Assignees: BenQ Materials Corporation
- Applicants: BenQ Materials Corporation
- Inventors: Tetsuya Okazaki; Wen-Hsin Yang
- Web page: https://patentgrep.com/patent/US20240199818A1

## CPC

- C08G 77/44: containing only polysiloxane sequences
- C09D 7/20: Diluents or solvents
- C09D 183/04: Polysiloxanes
- C08G 77/04: Polysiloxanes
- C08L 83/04: Polysiloxanes
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A low-refractivity optical clear resin is disclosed. The low-refractivity optical clear resin comprises a polysiloxane composition and an organic solvent composition, wherein the polysiloxane composition comprises a polysiloxane and a hydroxyalkylsilane monomer, and the organic solvent composition comprises a high boiling point solvent with a boiling point more than 180° C. and a low boiling point solvent with a boiling point less than 150° C.; wherein the used amount of the organic solvent composition is 50 to 120 parts by weight per 10 parts by weight of the polysiloxane composition. The present low-refractivity optical clear resin can be used on the micro light emitting diode (micro-LED) display devices to enhance the light extracting efficiency thereof, and provide excellent optical properties on an adequate coating thickness.

## Claims

### Claim 1

A low-refractivity optical clear resin, comprising:
a polysiloxane composition, comprising a polysiloxane and a hydroxyalkylsilane monomer; and
an organic solvent composition, comprising a high boiling point solvent with a boiling point more than 180° C. and a low boiling point solvent with a boiling point less than 150° C.;
wherein the used amount of the organic solvent composition is 50 to 120 parts by weight per 10 parts by weight of the polysiloxane composition.

### Claim 2 (depends on 1)

The low-refractivity optical clear resin as claimed in claim 1, wherein the organic solvent composition comprises 97 to 80 weight percent of the high boiling point solvent and 3 to 20 weight percent of the low boiling point solvent.

### Claim 3 (depends on 2)

The low-refractivity optical clear resin as claimed in claim 2, wherein the organic solvent composition comprises 95 to 85 weight percent of the high boiling point solvent and 5 to 15 weight percent of the low boiling point solvent.

### Claim 4 (depends on 1)

The low-refractivity optical clear resin as claimed in claim 1, wherein the curing temperature for curing the low-refractivity optical clear resin is ranging between 50° C. to 170° C.

### Claim 5 (depends on 1)

The low-refractivity optical clear resin as claimed in claim 1, wherein the yellow index of the low-refractivity optical clear resin after being cured is not more than 1.5.

### Claim 6 (depends on 1)

The low-refractivity optical clear resin as claimed in claim 1, wherein the refractive index of the low-refractivity optical clear resin after being cured is ranging between 1.1 and 1.35.

### Claim 7 (depends on 1)

The low-refractivity optical clear resin as claimed in claim 1, wherein the surface roughness Sa of the low-refractivity optical clear resin after being cured is ranging between 5 μm and 50 μm.

### Claim 8 (depends on 1)

The low-refractivity optical clear resin as claimed in claim 1, wherein the viscosity of the low-refractivity optical clear resin is ranging between 2 mPa·s and 20 mPa·s at 25° C., and the surface tension thereof is ranging between 20 dyne/cm and 40 dyne/cm.

### Claim 9 (depends on 1)

The low-refractivity optical clear resin as claimed in claim 1, wherein the surface tension of the high boiling point solvent is ranging between 30 dyne/cm and 38 dyne/cm, and the surface tension of the low boiling point solvent is ranging between 23 dyne/cm and 30 dyne/cm.

### Claim 10 (depends on 1)

The low-refractivity optical clear resin as claimed in claim 1, wherein the high boiling point solvent is γ-butyrolactone, diethylene glycol monoethyl ether, N-methylpyrrolidone or combinations thereof.

### Claim 11 (depends on 1)

The low-refractivity optical clear resin as claimed in claim 1, wherein the low boiling point solvent is 2-ethylbutanol, 2-methyl-2-butanol, ethylene glycol monoethyl ether, ethylene glycol dimethyl ether, propylene glycol monomethyl ether, or combinations thereof.

### Claim 12 (depends on 1)

The low-refractivity optical clear resin as claimed in claim 1, wherein the high boiling point solvent of the organic solvent composition partially comprising a middle boiling point solvent with a boiling point ranging between 150° C. and 180° C. and a surface tension ranging between 20 dyne/cm and 30 dyne/cm.

### Claim 13 (depends on 12)

The low-refractivity optical clear resin as claimed in claim 12, wherein the high boiling point solvent comprising 25 weight percent to 35 weight percent of the middle boiling point solvent.

### Claim 14 (depends on 1)

The low-refractivity optical clear resin as claimed in claim 1, wherein the content of the hydroxyalkylsilane monomer is 10 to 70 parts by weight per 10 parts by weight of the polysiloxane, and the boiling point of the hydroxyalkylsilane monomer is ranging between 80° C. and 180° C.

### Claim 15 (depends on 1)

The low-refractivity optical clear resin as claimed in claim 1, wherein the polysiloxane is synthesized by the hydrolysis and condensation or co-condensation of silane monomers selected from the group consisting of tetramethoxysilane, methyltrimethoxysilane, methyltriethoxysilane, dimethyldimethoxysilane, dimethyldiethoxysilane, trimethylmethoxysilane, vinyltrimethylsilane oxysilane, glycidoxypropyltrimethoxysilane, phenyltrimethoxysilane, methacryloyloxypropyltrimethoxysilane and combination thereof, and the weight average molecular weight (Mw) of the polysiloxane is ranging between 5,000 and 100,000 g/mol.

### Claim 16 (depends on 1)

The low-refractivity optical clear resin as claimed in claim 1, wherein the hydroxyalkylsilane monomer is represented by the following formula (I):
wherein R1, R2, R3, R4 and R5 are respectively C1-C10 alkyl groups or C5-C20 aryl groups optionally mono-substituted, double-substituted or triple-substituted with C1-C10 alkyl groups or C3-C10 alicyclic groups; R6 is a C6-C30 alkyl chain, optionally having 1 to 3 double or triple bonds, and comprising at least one hydroxyl group; and n is an integer from 0 to 10.