# US 2024/0199810 A1 · Method for producing polyimide resin powder

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0199810 A1
- Document ID: US20240199810A1
- Status: Published application
- Kind: A1
- Application number: 18/551,213
- Filed: 2022-03-01
- Published: 2024-06-20
- Earliest claimed: 2021-03-26
- Assignees: Mitsubishi Gas Chemical Company, Inc.
- Applicants: Mitsubishi Gas Chemical Company, Inc.
- Inventors: Yuuki SATO; Atsushi SAKAI
- Web page: https://patentgrep.com/patent/US20240199810A1

## CPC

- C08G 73/1028: {characterised by the process itself, e.g. steps, continuous}
- C08G 73/1082: {wholly aromatic in the tetracarboxylic moiety}
- C08G 73/10: Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors
- C08G 73/1032: {characterised by the solvent(s) used}
- C08G 73/1042: {Copolyimides derived from at least two different tetracarboxylic compounds or two different diamino compounds}
- C08J 5/18: Manufacture of films or sheets
- H05K 1/03: Use of materials for the substrate
- H05K 1/0346: {containing N}
- C08J 3/14: by precipitation from solutions {(C08J3/122 takes precedence)}
- C08J 2379/08: Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors
- H05K 1/0237: {High frequency adaptations (H05K1/0216 takes precedence)}
- H05K 2201/0154: Polyimide
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

A method for producing a polyimide resin powder, which involves reacting a tetracarboxylic acid component containing a tetracarboxylic dianhydride and a diamine component containing an aliphatic diamine in the presence of a solvent containing an alkylene glycol solvent of formula (1). In formula (1), Ra1 represents a hydrogen atom or an alkyl group having from 1 to 4 carbon atoms, Ra2 represents a linear alkylene group having from 2 to 6 carbon atoms, and n represents an integer of 1 to 3. The reacting produces a solution containing a polyimide resin precursor. This solution is then heated at an average heating rate of 0.5 to 8° C./min in a temperature range of 70 to 130° C. to imidize the polyimide resin precursor to produce the polyimide resin powder in the solution with a solid content concentration of 15 to 25% by mass.

## Claims

### Claim 1

A method for producing a polyimide resin powder, comprising:
a step of reacting a tetracarboxylic acid component (A) comprising a tetracarboxylic dianhydride and a diamine component (B) comprising an aliphatic diamine in the presence of a solvent (C) comprising an alkylene glycol solvent represented by the formula (1),
wherein the step comprises:
separately preparing a solution (a) comprising the tetracarboxylic acid component (A) in the solvent (C) and a solution (b) comprising the diamine component (B) in the solvent (C), and then adding the solution (b) to the solution (a) or adding the solution (a) to the solution (b) to prepare a solution (c) comprising a polyimide resin precursor comprising a polyamic acid; and
then imidizing the polyimide resin precursor comprising the polyamic acid by heating the solution (c) to deposit a polyimide resin powder in the solution,
wherein the solution (c) has a solid content concentration of 15 to 25% by mass, and an average heating rate in a temperature range of 70 to 130° C. during the heating of the solution (c) is 0.5 to 8° C./min:
wherein Ra1 represents a hydrogen atom or an alkyl group having from 1 to 4 carbon atoms, Ra2 represents a linear alkylene group having from 2 to 6 carbon atoms, and n represents an integer of 1 to 3.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the alkylene glycol solvent is at least one selected from the group consisting of 2-(2-methoxyethoxy)ethanol and 2-(2-ethoxyethoxy)ethanol.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the diamine component (B) comprises, as the aliphatic diamine, a diamine (B1) represented by the formula (B1-1) and a diamine (B2) represented by the formula (B2-1):
H2N—R1—NH2 (B1-1)
H2N—R2—NH2 (B2-1)
wherein R1 represents a divalent group having from 6 to 22 carbon atoms containing at least one alicyclic hydrocarbon structurell, and
wherein R2 represents a divalent chain aliphatic group having from 5 to 20 carbon atoms.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the tetracarboxylic dianhydride is represented by the formula (A-1):
wherein X represents a tetravalent group having from 6 to 22 carbon atoms and containing at least one aromatic ring.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the tetracarboxylic dianhydride is pyromellitic dianhydride.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the solvent (C) comprises 2-ethylhexanol.

### Claim 7 (depends on 1)

A polyimide resin powder produced by the method according to claim 1,
wherein the polyimide resin powder comprises a repeating structural unit represented by the following formula (I) and a repeating structural unit represented by the following formula (II),
wherein a content ratio of the repeating structural unit of the formula (1) with respect to the total of the repeating structural unit of the formula (1) and the repeating structural unit of the formula (II) is 20 to 70 mol %:
wherein; R1 represents a divalent group having from 6 to 22 carbon atoms containing at least one alicyclic hydrocarbon structure,
R2 represents a divalent chain aliphatic group having from 5 to 16 carbon atoms, and
X1 and X2 each independently represent a tetravalent group having from 6 to 22 carbon atoms containing at least one aromatic ring.

### Claim 8 (depends on 7)

The polyimide resin powder according to claim 7, wherein in the polyimide resin powder, the content ratio of the repeating structural unit of the formula (I) with respect to the total of the repeating structural unit of the formula (I) and the repeating structural unit of the formula (II) is 20 mol % or more and less than 40 mol %.

### Claim 9 (depends on 7)

The polyimide resin powder according to claim 7, wherein the polyimide resin powder has a volume average particle size D50 from 13 to 35 μm.

### Claim 10 (depends on 7)

A resin film obtained using a forming material comprising the polyimide resin powder according to claim 7.

### Claim 11 (depends on 10)

The resin film according to claim 10, wherein a ratio of a dielectric constant P40 at 40° C. and a dielectric constant P120 at 120° C., P120/P40 at 10 GHz is from 0.8 to 1.2.

### Claim 12 (depends on 10)

The resin film according to claim 10, wherein a ratio of a dielectric loss tangent Q40 at 40° C. and a dielectric loss tangent Q120 at 120° C., Q129/Q40, at 10 GHZ is from 1.0 to 1.5.

### Claim 13 (depends on 10)

The resin film according to claim 10, wherein a ratio of a dielectric constant P40 at 40° C. and a dielectric constant P120 at 120° C., P120/P40, at 20 GHz is from 0.8 to 1.2.

### Claim 14 (depends on 10)

The resin film according to claim 10, wherein a ratio of a dielectric loss tangent Q40 at 40° C. and a dielectric loss tangent Q120 at 120° C., Q129/Q40, at 20 GHZ is from 1.0 to 1.7.

### Claim 15 (depends on 10)

A high-frequency circuit board comprising the resin film of claim 10.

### Claim 16 (depends on 10)

A copper clad laminate comprising a layer comprising the resin film of claim 10.