# US 2024/0199796 A1 · High heat resistant and transparent polyethylene terephthalate (pet) copolyester and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0199796 A1
- Document ID: US20240199796A1
- Status: Published application
- Kind: A1
- Application number: 18/150,760
- Filed: 2023-01-05
- Published: 2024-06-20
- Earliest claimed: 2022-12-15
- Assignees: Nan Ya Plastics Corporation
- Applicants: Nan Ya Plastics Corporation
- Inventors: Te-Chao Liao; Han-Ching Hsu; Chen-Wei Chang
- Web page: https://patentgrep.com/patent/US20240199796A1

## CPC

- C08G 63/183: Terephthalic acids
- C08G 63/189: containing a naphthalene ring
- C08G 63/672: Dicarboxylic acids and dihydroxy compounds
- C08G 63/78: Preparation processes
- C08G 63/87: Non-metals or inter-compounds thereof (boron C08G63/84)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

A polyethylene terephthalate (PET) copolyester and a manufacturing method thereof are provided, including the following steps. A dispersion slurry including a talcum powder is formulated. Terephthalic acid and ethylene glycol are mixed, and the dispersion slurry and a side group ester compound are introduced to perform a transesterification reaction and form bis-2-hydroxylethyl terephthalate. Afterwards, a prepolymerization reaction and a polycondensation reaction are carried out to form a polyethylene terephthalate copolyester.

## Claims

### Claim 1

A manufacturing method of a polyethylene terephthalate copolyester, comprising:
preparing a dispersion slurry, wherein the dispersion slurry comprises a talcum powder;
mixing a terephthalic acid and an ethylene glycol, and introducing the dispersion slurry and a side group ester compound, so as to carry out a transesterification and therefore form a bis-2-hydroxylethyl terephthalate; and
carrying out a prepolymerization reaction and a polycondensation reaction, so that the bis-2-hydroxylethyl terephthalate forms a polyethylene terephthalate copolyester.

### Claim 2 (depends on 1)

The manufacturing method of claim 1, wherein the talcum powder has an average particle size of 1.0 μm to 5.0 μm, and an average specific surface area of 20 m2/g to 12 m2/g.

### Claim 3 (depends on 1)

The manufacturing method of claim 1, wherein the side group ester compound includes 2,6-naphthalene dicarboxylate.

### Claim 4 (depends on 1)

The manufacturing method of claim 1, wherein based on a total weight of the dispersion slurry, a content of the talcum powder ranges from 1 wt % to 8 wt %.

### Claim 5 (depends on 1)

The manufacturing method of claim 1, wherein the dispersion slurry further comprises a dispersant and an ethylene glycol, and based on a total weight of the dispersion slurry, a content of the dispersant ranges from 99 wt % to 1 wt %.

### Claim 6 (depends on 1)

The manufacturing method of claim 1, wherein based on a total weight of the bis-2-hydroxylethyl terephthalate, an added amount of the dispersion slurry ranges from 1 wt % to 6 wt %.

### Claim 7 (depends on 1)

The manufacturing method of claim 1, wherein during the transesterification reaction, an equivalent ratio of the terephthalic acid to the ethylene glycol ranges from 1/1.2 to 1/1.8, a reaction temperature ranges from 200° C. to 230° C., and a reaction time ranges from 2 hours to 4 hours.

### Claim 8 (depends on 1)

The manufacturing method of claim 1, wherein based on a total weight of the bis-2-hydroxylethyl terephthalate, an added amount of the side group ester compound is 1 wt % to 5 wt %.

### Claim 9 (depends on 1)

The manufacturing method of claim 1, wherein during the prepolymerization reaction, reactants comprise the bis-2-hydroxylethyl terephthalate and a polyethylene glycol, wherein based on a total weight of the bis-2-hydroxylethyl terephthalate, a content of the polyethylene glycol ranges from 0.5 wt % to 4 wt %, a reaction temperature ranges from 230° C. to 270° C., a vacuum degree is 760 mmHg to 10 mmHg, and a reaction time ranges from 1 hour to 2 hours.

### Claim 10 (depends on 1)

The manufacturing method of claim 1, wherein the polycondensation reaction is carried out after the prepolymerization reaction, and during the polycondensation reaction, a reaction temperature ranges from 260° C. to 280° C., a vacuum degree ranges from 1 mmHg to 3 mmHg, and a reaction time ranges from 2 hours to 4 hours.

### Claim 11 (depends on 1)

A polyethylene terephthalate copolyester, made by the manufacturing method of claim 1.