# US 2024/0199494 A1 · Zirconia molded body, zirconia pre-sintered body, and zirconia sintered body, and methods of production thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0199494 A1
- Document ID: US20240199494A1
- Status: Published application
- Kind: A1
- Application number: 18/286,780
- Filed: 2022-04-15
- Published: 2024-06-20
- Earliest claimed: 2021-04-16
- Assignees: Kuraray Noritake Dental lnc.
- Applicants: Kuraray Noritake Dental lnc.
- Inventors: Yasutaka KUDO; Kirihiro NAKANO
- Web page: https://patentgrep.com/patent/US20240199494A1

## CPC

- C04B 35/488: Composites
- A61C 13/0022: {Blanks or green, unfinished dental restoration parts}
- C01G 25/02: Oxides
- C04B 35/486: Fine ceramics
- C04B 35/62675: {characterised by the treatment temperature}
- C04B 35/63424: {Polyacrylates; Polymethacrylates}
- C04B 35/63488: {Polyethers, e.g. alkylphenol polyglycolether, polyethylene glycol [PEG], polyethylene oxide [PEO]}
- C04B 35/6365: {Cellulose or derivatives thereof}
- C04B 35/638: Removal thereof
- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- A61C 13/0006: {Production methods}
- A61C 13/083: Porcelain or ceramic teeth {(A61C13/081 takes precedence; preparations A61K6/80)}
- A61C 2201/00: Material properties
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/3246: Stabilised zirconias, e.g. YSZ or cerium stabilised zirconia
- C04B 2235/444: Halide containing anions, e.g. bromide, iodate, chlorite
- C04B 2235/5454: nanometer sized, i.e. below 100 nm
- C04B 2235/549: the particle size being expressed by crystallite size or primary particle size
- C04B 2235/6023: Gel casting
- C04B 2235/6026: Computer aided shaping, e.g. rapid prototyping
- C04B 2235/6027: Slip casting
- C04B 2235/604: Pressing at temperatures other than sintering temperatures
- C04B 2235/656: characterised by specific heating conditions during heat treatment
- C04B 2235/6562: Heating rate
- C04B 2235/661: Multi-step sintering
- C04B 2235/668: Pressureless sintering
- C04B 2235/77: Density
- C04B 2235/781: Nanograined materials, i.e. having grain sizes below 100 nm
- C04B 2235/785: Submicron sized grains, i.e. from 0,1 to 1 micron
- C04B 2235/95: Products characterised by their size, e.g. microceramics
- C04B 2235/96: Properties of ceramic products, e.g. mechanical properties such as strength, toughness, wear resistance
- C04B 2235/9646: Optical properties
- C04B 2235/9653: Translucent or transparent ceramics other than alumina
- C04B 2235/9661: Colour
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- A61C: DENTISTRY; APPARATUS OR METHODS FOR ORAL OR DENTAL HYGIENE (non-driven toothbrushes A46B; {tongue scrapers A61B17/24;} preparations for dentistry A61K6/00; preparations for cleaning the teeth or mouth A61K8/00, A61Q11/00)
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)

## Abstract

The present invention provides a zirconia sintered body that excels in both mechanical strength and translucency, and a zirconia molded body and zirconia pre-sintered body capable of providing such a zirconia sintered body, and containing a binder in an amount that assumes a thickness of 10 mm or more. The invention also provides methods of production of these. The present invention relates to a zirconia molded body comprising: a zirconia particle containing 2.0 to 9.0 mol % of yttria relative to the total number of moles of zirconium oxide and yttria, and having an average primary particle diameter of 60 nm or less; a polyol; and a binder, the polyol and the binder satisfying the 10 relational formula X1<Y1<X2<Y2≤500° C. (The descriptions of the symbols in the formula are omitted.)

## Claims

### Claim 1

A zirconia molded body comprising:
a zirconia particle comprising 2.0 to 9.0 mol % of yttria relative to the total number of moles of zirconium oxide and yttria, and having an average primary particle diameter of 60 nm or less;
a polyol; and
a binder,
the polyol and the binder satisfying the relational formula X1<Y1<X2<Y2≤ 500° C., where X1 represents a combustion start temperature of the polyol, X2 represents a combustion end temperature of the polyol, Y1 represents a combustion start temperature of the binder, and Y2 represents a combustion end temperature of the binder, in which X1 and Y1 represent temperatures at which a 0.5% weight reduction is observed, and X2 and Y2 represent temperatures at which a 99.5% weight reduction is observed relative to the pre-heating weight of 100% measured by thermogravimetry.

### Claim 2 (depends on 1)

The zirconia molded body according to claim 1, which has a thickness of 10 mm or more.

### Claim 3 (depends on 1)

The zirconia molded body according to claim 1, wherein the polyol has a combustion start temperature (X1) of 50° C. or higher.

### Claim 4 (depends on 1)

The zirconia molded body according to claim 1, which has a ΔL*(W−B) of 5 or more at a thickness of 1.5 mm.

### Claim 5 (depends on 1)

The zirconia molded body according to claim 1, which has a crystal grain size of 180 nm or less after being sintered at 900 to 1,200° C. under ordinary pressure.

### Claim 6 (depends on 1)

The zirconia molded body according to claim 1, which has a three-point flexural strength of 500 MPa or more after being sintered at 900 to 1,200° C. under ordinary pressure.

### Claim 7 (depends on 1)

The zirconia molded body according to claim 1, which has a transmittance of 40% or more for light of 700 nm wavelength at a thickness of 0.5 mm after being sintered at 900 to 1,200° C. under ordinary pressure.

### Claim 8 (depends on 1)

The zirconia molded body according to claim 1, which has a linear light transmittance of 1% or more at a thickness of 1.0 mm after being sintered at 900 to 1,200° C. under ordinary pressure.

### Claim 9 (depends on 1)

The zirconia molded body according to claim 1, which has ten or fewer pores with a diameter of 50 nm or more per 28.5 μm2 cross sectional area after being sintered at 900 to 1,200° C. under ordinary pressure.

### Claim 10 (depends on 1)

The zirconia molded body according to claim 1, which has a ΔL*(W−B) of 5 or more at a thickness of 1.5 mm after being pre-sintered at 200 to 800° C.

### Claim 11

A zirconia pre-sintered body comprising 2.0 to 9.0 mol % of yttria relative to the total number of moles of zirconium oxide and yttria,
the zirconia pre-sintered body having a ΔL*(W−B) of 5 or more at a thickness of 1.5 mm, and having ten or fewer pores with a diameter of 50 nm or more per 28.5 μm2 cross sectional area, and a thickness of 10 mm or more after being sintered at 900 to 1,200° C.

### Claim 12 (depends on 1)

A method for producing a zirconia pre-sintered body, comprising pre-sintering a zirconia molded body according to claim 1 at 200 to 800° C.

### Claim 13

A zirconia sintered body comprising 2.0 to 9.0 mol % of yttria relative to the total number of moles of zirconium oxide and yttria,
the zirconia sintered body having ten or fewer pores with a diameter of 50 nm or more per 28.5 μm2 cross sectional area, and a thickness of 10 mm or more.

### Claim 14 (depends on 1)

A method for producing a zirconia sintered body, comprising sintering a zirconia molded body according to claim 1 at 900 to 1,200° C. under ordinary pressure.