# US 2024/0199475 A1 · Transparent spinel glass ceramic and preparation method therefor and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0199475 A1
- Document ID: US20240199475A1
- Status: Published application
- Kind: A1
- Application number: 18/555,948
- Filed: 2022-12-15
- Published: 2024-06-20
- Earliest claimed: 2021-12-30
- Assignees: Chongqing Aureavia Hi-tech Glass Co., Ltd.
- Applicants: Chongqing Aureavia Hi-tech Glass Co., Ltd.
- Inventors: Yanqi ZHANG; Jingpeng ZHOU; Hao HUANG
- Web page: https://patentgrep.com/patent/US20240199475A1

## CPC

- C03C 10/0045: {containing SiO2, Al2O3 and MgO as main constituents}
- C03B 32/02: Thermal crystallisation, e.g. for crystallising glass bodies into glass-ceramic articles {(C03B27/012 takes precedence)}
- C03C 3/085: containing an oxide of a divalent metal
- C03C 4/0092: {for glass with improved high visible transmittance, e.g. extra-clear glass}
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 2214/20: Glass-ceramics matrix
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

Disclosed in the invention is transparent spinel glass ceramic, in mole percentage of oxides, the glass ceramic comprising: LizO: 3.50˜6.00 mol %, Na2O: 2.00˜4.00 mol %. A crystal phase of the glass ceramic has a spinel crystal and a zirconia crystal, and does not have a crystal containing Li. According to the invention, components of a spinel glass ceramic material are optimized by introducing into the spinel glass ceramic more Li ions and Na ions used for chemical strengthening via ion exchange to obtain the spinel glass ceramic without an impurity crystal phase, and the glass ceramic does not exhibit phenomena of atomization, devitrification and the like, ensuring that the glass ceramic material has an excellent transmittance. More Li ions and Na ions are introduced into the spinel glass ceramic components, so that the prepared spinel glass ceramic can be chemically strengthened to obtain transparent strengthened glass ceramic having high CS, DOL_0, CT_AV and CT_LD, and the strengthened glass ceramic shows excellent drop resistance performance.

## Claims

### Claim 1

A transparent spinel glass ceramic, wherein, in molar percentage of oxides, the glass ceramic comprises:
LizO: 3.50 to 6.00 mol %, and
NazO: 2.00 to 4.00 mol %; and
wherein a crystal phase of the glass ceramic comprises a spinel crystal and a zirconia crystal, and does not comprise a Li-containing crystal.

### Claim 2 (depends on 1)

The transparent spinel glass ceramic according to claim 1, wherein, the crystal phase of the glass ceramic does not comprise quartz and a solid solution of quartz.

### Claim 3 (depends on 1)

The transparent spinel glass ceramic according to claim 1, wherein, the glass ceramic has a crystallinity of at least 30.00 wt. %.

### Claim 4 (depends on 1)

The transparent spinel glass ceramic according to claim 1, wherein, the average crystal size in the glass ceramic is less than or equal to 15.00 nm.

### Claim 5 (depends on 1)

The transparent spinel glass ceramic according to claim 1, wherein, the spinel crystal comprises a zinc spinel and a magnesium spinel.

### Claim 6 (depends on 1)

The transparent spinel glass ceramic according to claim 1, wherein, the transmittance of the glass ceramic with a thickness of 0.70 mm is greater than 85.00% at a light having a wavelength of 550.00 nm.

### Claim 7 (depends on 1)

The transparent spinel glass ceramic according to claim 1, wherein, in molar percentage of oxides, the glass ceramic further comprises:
SiO2: 50.00 to 65.00 mol %,
Al2O3: 14.50 to 25.00 mol %,
MgO: 3.50 to 8.00 mol %,
ZnO: 8.00 to 16.00 mol %,
BaO: 0 to 2.00 mol %, and
TiO2+ZrO2: 3.00 to 5.50 mol %.

### Claim 8 (depends on 7)

The transparent spinel glass ceramic according to claim 7, wherein, in molar percentage of oxides, the glass ceramic satisfies:
0.40≤(Al2O3+ZnO+MgO+ZrO2+TiO2)/(Li2O+Na2O+SiO2+BaO)≤0.70.

### Claim 9 (depends on 8)

The transparent spinel glass ceramic according to claim 8, wherein, in molar percentage of oxides, the glass ceramic satisfies:
0.43≤(Al2O3+ZnO+MgO+ZrO2+TiO2)/(Li2O+Na2O+SiO2+BaO)≤0.68.

### Claim 10 (depends on 7)

The transparent spinel glass ceramic according to claim 7, wherein, in molar percentage of oxides, the glass ceramic satisfies:
Na2O/(Li2O+Na2O+SiO2+BaO)≥0.035; and/or
Li2O/(Li2O+Na2O+SiO2+BaO)≥0.054.

### Claim 11 (depends on 10)

The transparent spinel glass ceramic according to claim 10, wherein, in molar percentage of oxides, the glass ceramic satisfies:
0.035≤Na2O/(Li2O+Na2O+SiO2+BaO)≤0.070; and/or
0.054≤Li2O/(Li2O+Na2O+SiO2+BaO)≤0.090.

### Claim 12 (depends on 7)

The transparent spinel glass ceramic according to claim 7, wherein, in molar percentage of oxides, the glass ceramic comprises:
SiO2: 50.00 to 63.00 mol %; and/or
Al2O3: 14.50 to 20.00 mol %; and/or
MgO: 3.90 to 7.60 mol %; and/or
ZnO: 8.00 to 15.50 mol %; and/or
BaO: 0 to 1.50 mol %; and/or
LizO: 3.50 to 5.00 mol %; and/or
NazO: 2.30 to 3.60 mol %; and/or
TiO2: 0 to 2.00 mol %; and/or
ZrO2: 2.50 to 5.00 mol %.

### Claim 13 (depends on 1)

The transparent spinel glass ceramic according to claim 1, wherein, the transparent spinel glass ceramic is prepared by a preparation method comprising:
(1) batching and mixing raw materials to prepare a glass precursor; and
(2) subjecting the prepared glass precursor to nucleation and crystallization successively to prepare the transparent spinel glass ceramic.

### Claim 14 (depends on 13)

The transparent spinel glass ceramic according to claim 13, wherein, in step (2):
the nucleation is performed at a nucleation temperature of 700 to 800° C. for a nucleation time of 30 to 1440 min; and
the crystallization is performed at a crystallization temperature of 900 to 1000° C. for a crystallization time of 5 to 1440 min.

### Claim 15 (depends on 14)

The transparent spinel glass ceramic according to claim 14, wherein, in step (2), during the crystallization, the temperature is raised at a heating rate of greater than 20° C./min to reach the crystallization temperature; and/or
in step (2), during the nucleation, the temperature is raised at a heating rate of 5 to 20° C./min to reach the nucleation temperature.

### Claim 16 (depends on 15)

The preparation method according to claim 15, wherein, in step (2), during the crystallization, the temperature is raised at a heating rate of greater than or equal to 25° C./min to reach the crystallization temperature; and/or
in step (2), during the nucleation, the temperature is raised at a heating rate of 10° C./min to reach the nucleation temperature.

### Claim 17

(canceled)

### Claim 18

(canceled)

### Claim 19 (depends on 1)

The transparent spinel glass ceramic according to claim 1, wherein the transparent spinel glass ceramic can be prepared into a strengthened glass ceramic; through chemically strengthening via ion exchange; and the strengthened glass ceramic has a compressive stress zone extending from a surface of the strengthened glass ceramic to a compressive depth.

### Claim 20 (depends on 1)

The transparent spinel glass ceramic according to claim 1, wherein the transparent spinel glass ceramic is used in watches, transparent armors, guided missile windows, fairings, substrate materials, new lamps and lanterns, observation windows for equipment used in high-temperature, high-pressure and corrosive environments, automobiles, trains, aircrafts, marine vehicles, building materials, portable intelligent electronic devices.

### Claim 21 (depends on 7)

The transparent spinel glass ceramic according to claim 7, wherein, in molar percentage of oxides, the glass ceramic comprises:
SiO2: 50.00 to 57.00 mol %; and/or
Al2O3: 15.00 to 19.00 mol %; and/or
MgO: 4.00 to 7.50 mol %; and/or
ZnO: 9.00 to 15.20 mol %; and/or
BaO: 1.00 to 1.35 mol %; and/or
LizO: 4.00 to 5.00 mol %; and/or
Na2O: 3.00 to 3.60 mol %; and/or
TiO2: 0.30 to 1.30 mol %; and/or
ZrO2: 2.90 to 4.20 mol %.

### Claim 22 (depends on 1)

The transparent spinel glass ceramic according to claim 1, wherein, in molar percentage of oxides, the glass ceramic comprises:
LizO: 3.50 to 6.00 mol %,
Na2O: 2.00 to 4.00 mol %;
SiO2: 50.00 to 63.00 mol %,
Al2O3: 14.50 to 20.00 mol %,
MgO: 3.90 to 7.60 mol %,
ZnO: 8.00 to 15.50 mol %,
BaO: 0 to 1.50 mol %,
TiO2: 0 to 2.00 mol %, and
ZrO2: 2.50 to 5.00 mol %.