# US 2024/0199474 A1 · Transparent glass ceramic, especially as a cover pane

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0199474 A1
- Document ID: US20240199474A1
- Status: Published application
- Kind: A1
- Application number: 18/542,367
- Filed: 2023-12-15
- Published: 2024-06-20
- Earliest claimed: 2022-12-16
- Assignees: Schott AG
- Applicants: Schott AG
- Inventors: Meike Schneider; Bernd Rüdinger; Uwe Martens
- Web page: https://patentgrep.com/patent/US20240199474A1

## CPC

- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 10/0009: {containing silica as main constituent}
- C03B 32/02: Thermal crystallisation, e.g. for crystallising glass bodies into glass-ceramic articles {(C03B27/012 takes precedence)}
- C03C 1/004: {Refining agents (refining C03B5/225)}
- C03C 3/093: containing zinc or zirconium
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 10/0027: {containing SiO2, Al2O3, Li2O as main constituents}
- C03C 10/0054: {containing PbO, SnO2, B2O3}
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 2204/00: Glasses, glazes or enamels with special properties
- H05K 5/03: Covers
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

A transparent, chemically prestressable or chemically prestressed glass ceramic is provided. The glass ceramic has keatite as a main crystal phase, a transmittance greater than 80% at a thickness of 0.7 mm, a haze of less than or equal to 10, and a crystal phase content of at least 80% by weight of keatite solid solution based on all crystal phases in the glass ceramic.

## Claims

### Claim 1

A transparent, chemically prestressable or chemically prestressed glass ceramic, comprising:
keatite as a main crystal phase;
a transmittance greater than 80% at a thickness of 0.7 mm;
a haze of less than or equal to 10; and
a crystal phase content of at least 80% by weight of keatite solid solution based on all crystal phases in the glass ceramic.

### Claim 2 (depends on 1)

The glass ceramic of claim 1, wherein the crystal phase content is at least 95% by weight.

### Claim 3 (depends on 1)

The glass ceramic of claim 1, wherein the glass ceramic has a composition comprising SiO2, Al2O3, and Li2O as main components and SnO2 and ZrO2 as nucleating agents.

### Claim 4 (depends on 3)

The glass ceramic of claim 3, wherein the SiO2 is present in a content of between 58 and 72 in percent by weight.

### Claim 5 (depends on 3)

The glass ceramic of claim 3, wherein the Al2O3 is present in a content of between 18 to 23 in percent by weight.

### Claim 6 (depends on 3)

The glass ceramic of claim 3, wherein the Li2O is present in a content of between 2 to 5.5 in percent by weight.

### Claim 7 (depends on 1)

The glass ceramic of claim 1, wherein the glass ceramic has a composition comprising 1 to 2% by weight of SnO2 and/or 2 to 3% by weight of ZrO2.

### Claim 8 (depends on 1)

The glass ceramic of claim 1, wherein the glass ceramic has a composition comprising less than 0.1% by weight of TiO2.

### Claim 9 (depends on 3)

The glass ceramic of claim 3, comprising a ratio of Al2O3 to SiO2, both in percent by weight, of less than 0.33.

### Claim 10 (depends on 1)

The glass ceramic of claim 1, wherein the glass ceramic has a composition that is substantially free of colouring components selected from a group consisting of V2O5, Nd2O3, CoO, and combinations thereof.

### Claim 11 (depends on 1)

The glass ceramic of claim 1, wherein the glass ceramic has a composition comprising 0 to 2% by weight of B2O3.

### Claim 12 (depends on 1)

The glass ceramic of claim 1, wherein the glass ceramic has a composition comprising less than 2% by weight of P2O5.

### Claim 13 (depends on 1)

The glass ceramic of claim 1, wherein the glass ceramic has a composition comprising less than 1% by weight of Na2O+K2O.

### Claim 14 (depends on 1)

The glass ceramic of claim 1, wherein the glass ceramic has a composition comprising a condition wherein Li2O—ZnO—CaO is less than 3% by weight.

### Claim 15 (depends on 1)

The glass ceramic of claim 1, wherein the glass ceramic has a composition that is substantially free of MgO and/or BaO.

### Claim 16 (depends on 1)

The glass ceramic of claim 1, wherein the glass ceramic has a composition comprising less than 1.8% by weight of CaO+SrO, and/or 0 to 2% by weight of ZnO, and/or a sum of ZrO2+SnO2 that is greater than 3.6% by weight, and/or up to 2% of one or more fining agents selected from a group consisting of As2O3, Sb2O3, halides, and SO3.

### Claim 17 (depends on 1)

The glass ceramic of claim 1, wherein the glass ceramic is configured as a cover pane having a thickness of 0.4 mm to 1 mm.

### Claim 18 (depends on 17)

The glass ceramic of claim 17, wherein the cover pane is configured for a use selected from a group consisting of an electronic display device, a mobile electronic display device, a mobile touch panel, a mobile digital display device, a smartphone, and a smart watch.

### Claim 19

A method for producing a prestressed glass ceramic, comprising:
producing a silicate green glass by a melting process and a hot shaping process;
exposing the silicate green glass to a temperature treatment having at least one nucleation step carried out in a temperature range of 690° ° C. to 850° C. for a period of 5 min to 72 hour and at least one ceramization step carried out in a temperature range of 780° C. to 1100° C. for a period of 3 min to 150 hours; and
performing at least one ion exchange in an exchange bath having a composition of 100% by weight to 0% by weight KNO3, 0% by weight to 100% by weight NaNO3, 0% by weight to 5% by weight LiNO3 at a temperature of the exchange bath between 370° C. and 500° C. and for a period of between 2 hours and 50 hours such that the prestressed glass ceramic has keatite as a main crystal phase, a transmittance greater than 80% at a thickness of 0.7 mm, a haze of less than or equal to 10, and a crystal phase content of at least 80% by weight of keatite solid solution based on all crystal phases in the glass ceramic.

### Claim 20 (depends on 19)

The method of claim 19, wherein the hot shaping process is selected from a group consisting of a floating process, a rolling process, a drawing process, and an ingot casting process.