# US 2024/0199471 A1 · Fluorescent glass ceramic with high transparency and preparation method and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0199471 A1
- Document ID: US20240199471A1
- Status: Published application
- Kind: A1
- Application number: 17/910,462
- Filed: 2022-07-08
- Published: 2024-06-20
- Earliest claimed: 2021-10-28
- Assignees: Aidite (Qinhuangdao) Technology Co., Ltd.
- Applicants: Aidite (Qinhuangdao) Technology Co., Ltd.
- Inventors: Jiaxin ZHANG; Quanyi NIE; Lijia ZHAO; Yong YU; Zhenyu DU; Jingjing ZHENG
- Web page: https://patentgrep.com/patent/US20240199471A1

## CPC

- C03C 4/12: for luminescent glass; for fluorescent glass
- C03B 19/06: by sintering, {e.g. by cold isostatic pressing of powders and subsequent sintering, by hot pressing of powders, by sintering slurries or dispersions not undergoing a liquid phase reaction}
- C03B 25/02: in a discontinuous way
- C03B 32/02: Thermal crystallisation, e.g. for crystallising glass bodies into glass-ceramic articles {(C03B27/012 takes precedence)}
- C03C 1/04: Opacifiers, e.g. fluorides or phosphates; Pigments
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 10/00: Devitrified glass ceramics, i.e. glass ceramics having a crystalline phase dispersed in a glassy phase and constituting at least 50% by weight of the total composition
- C03C 10/0009: {containing silica as main constituent}
- C09K 11/7766: {containing two or more rare earth metals}
- C03B 19/1045: {by bringing hot glass in contact with a liquid, e.g. shattering}
- C03C 2204/00: Glasses, glazes or enamels with special properties
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

Provided are a fluorescent glass ceramic with high transparency and a preparation method and use thereof. The fluorescent glass ceramic includes the following raw materials by mass percentage: 63 wt % to 70 wt % of SiO2, 13 wt % to 16 wt % of Li2O, 1 wt % to 6 wt % of Al2O3, 1 wt % to 10 wt % of K2O, 2 wt % to 6 wt % of P2O5, 0.5 wt % to 3.5 wt % of CeO2, 0 wt % to 4 wt % of an additive, 1 wt % to 4 wt % of a lanthanide oxide with an atomic number of 59 to 71, and 0 wt % to 8 wt % of a colorant. The fluorescent glass ceramic has a lithium metasilicate crystal as a principal crystalline phase, and the lithium metasilicate crystal has a layered or plate-like structure and a grain size of 0.1 μm to 1.5 μm.

## Claims

### Claim 1

A fluorescent glass ceramic with high transparency, comprising the following raw materials by mass percentage: 63 wt % to 70 wt % of SiO2, 13 wt % to 16 wt % of Li2O, 1 wt % to 6 wt % of Al2O3, 1 wt % to 10 wt % of K2O, 2 wt % to 6 wt % of P2O5, 0.5 wt % to 3.5 wt % of CeO2, 0 wt % to 4 wt % of an additive, 1 wt % to 4 wt % of a lanthanide oxide with an atomic number of 59 to 71, and 0 wt % to 8 wt % of a colorant, wherein
the fluorescent glass ceramic has a lithium metasilicate crystal as a principal crystalline phase;
the lithium metasilicate crystal has a layered or plate-like structure; and
the lithium metasilicate crystal has a grain size of 0.1 μm to 1.5 μm.

### Claim 2 (depends on 1)

The fluorescent glass ceramic of claim 1, comprising the following raw materials by mass percentage: 64 wt % to 66 wt % of the SiO2, 14 wt % to 15 wt % of the Li2O, 2 wt % to 4 wt % of the Al2O3, 2 wt % to 5 wt % of the K2O, 3 wt % to 4 wt % of the P2O5, 1.5 wt % to 3.0 wt % of the CeO2, 1 wt % to 3 wt % of the additive, 1.5 wt % to 3.0 wt % of the lanthanide oxide with the atomic number of 59 to 71, and 1 wt % to 4 wt % of the colorant.

### Claim 3 (depends on 1)

The fluorescent glass ceramic of claim 1, wherein the additive comprises at least one selected from the group consisting of a monovalent metal oxide and a divalent metal oxide.

### Claim 4 (depends on 3)

The fluorescent glass ceramic of claim 3, wherein the monovalent metal oxide comprises at least one selected from the group consisting of Na2O, Rb2O, and Cs2O; and
the divalent metal oxide comprises at least one selected from the group consisting of MgO, SrO, ZnO, and CaO.

### Claim 5 (depends on 1)

The fluorescent glass ceramic of claim 1, wherein the lanthanide oxide with the atomic number of 59 to 71 comprises at least one selected from the group consisting of Nd2O3, Tb2O3, Pr6O11, Eu2O3, and Er2O3.

### Claim 6 (depends on 1)

The fluorescent glass ceramic of claim 1, wherein the colorant comprises at least one selected from the group consisting of TiO2, CuO, MnO, and SeO2.

### Claim 7 (depends on 1)

The fluorescent glass ceramic of claim 1, wherein a 1-mm-thick sample of the fluorescent glass ceramic has an optical transmittance of 40% to 90% at 550 nm.

### Claim 8 (depends on 1)

A method for preparing the fluorescent glass ceramic of claim 1, comprising:
(1) mixing the raw materials of the fluorescent glass ceramic according to a proportion to obtain a mixture, and subjecting the mixture to primary melting and water quenching in sequence to obtain a glass slag;
(2) subjecting the glass slag obtained in step (1) to secondary melting and a forming annealing treatment in sequence to obtain a first glass matrix; or
subjecting the glass slag obtained in step (1) to grinding, dry pressing, and vacuum sintering in sequence to obtain a second glass matrix; and
(3) subjecting the first glass matrix or the second glass matrix obtained in step (2) to a first heat treatment and a second heat treatment in sequence to obtain the fluorescent glass ceramic with high transparency.

### Claim 9 (depends on 8)

The method of claim 8, wherein in step (1), the primary melting is conducted at a temperature of 1,300° C. to 1,600° C.; and
in step (1), the primary melting is conducted for 1 h to 6 h.

### Claim 10 (depends on 8)

The method of claim 8, wherein in step (2), the secondary melting is conducted at a temperature of 1,300° C. to 1,600° C.; and
in step (2), the secondary melting is conducted for 1 h to 6 h.

### Claim 11 (depends on 8)

The method of claim 8, wherein in step (2), the forming annealing treatment comprises: pouring a base glass liquid obtained after the secondary melting into a first mold preheated to a temperature of 200° C. to 500° C. and subjecting the base glass liquid to annealing.

### Claim 12 (depends on 8)

The method of claim 8, wherein the forming annealing treatment is conducted for 0.5 h to 24 h; and
the method further comprises cooling the first glass matrix to ambient temperature after the forming annealing treatment.

### Claim 13 (depends on 8)

The method of claim 8, wherein in step (2), a glass powder with a particle size of 0.2 μm to 50 μm is obtained after the grinding.

### Claim 14 (depends on 8)

The method of claim 8, wherein in step (2), the dry pressing comprises: subjecting the glass powder obtained after the grinding to dry pressing at a pressure of 5 MPa to 50 MPa in a second mold to obtain the biscuit.

### Claim 15 (depends on 8)

The method of claim 8, wherein in step (2), the vacuum sintering is conducted at a vacuum degree of 100 Pa to 3,000 Pa;
in step (2), the vacuum sintering is conducted at a temperature of 900° C. to 1,200° C.; and
in step (2), the vacuum sintering is conducted for 100 min to 240 min.

### Claim 16 (depends on 8)

The method of claim 8, wherein in step (3), the first heat treatment is conducted at a temperature of 450° C. to 580° C.; and
in step (3), the first heat treatment is conducted for 1 h to 48 h.

### Claim 17 (depends on 8)

The method of claim 8, wherein in step (3), the second heat treatment is conducted at a temperature of 600° C. to 700° C.; and
in step (3), the second heat treatment is conducted for 10 min to 240 min.

### Claim 18 (depends on 1)

Use of the fluorescent glass ceramic with high transparency of claim 1 in a chair-side restoration system.

### Claim 19 (depends on 2)

The fluorescent glass ceramic of claim 2, wherein the additive comprises at least one selected from the group consisting of a monovalent metal oxide and a divalent metal oxide.

### Claim 20 (depends on 2)

The fluorescent glass ceramic of claim 2, wherein the lanthanide oxide with the atomic number of 59 to 71 comprises at least one selected from the group consisting of Nd2O3, Tb2O3, Pr6O11, Eu2O3, and Er2O3.