# US 2024/0199469 A1 · Alkali-free glass

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0199469 A1
- Document ID: US20240199469A1
- Status: Published application
- Kind: A1
- Application number: 18/594,084
- Filed: 2024-03-04
- Published: 2024-06-20
- Earliest claimed: 2021-09-07
- Assignees: AGC Inc.
- Applicants: AGC Inc.
- Inventors: Yuya HAMADA; Hirofumi TOKUNAGA
- Web page: https://patentgrep.com/patent/US20240199469A1

## CPC

- C03C 3/091: containing aluminium
- C03B 18/02: Forming sheets
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 3/11: containing halogen or nitrogen
- C03C 3/112: containing fluorine
- C03C 3/118: containing aluminium
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

The present invention relates to an alkali-free glass having a strain point of 700° C. or higher and 740° C. or lower, a density of 2.6 g/cm3 or lower, a Young's modulus of 90 GPa or higher and 100 GPa or lower, an average coefficient of thermal expansion at 50° C. to 350° C. of 30×10−7/K or higher and 39×10−7/K or lower, a temperature T2 at which a glass viscosity reaches 102 dPa·s of 1590° C. or higher and 1690° C. or lower, a temperature T4 at which the glass viscosity reaches 104 dPa·s of 1350° C. or lower, a glass surface devitrification temperature (Tc) of lower than (T4+80)° C., and a specific elastic modulus of 36 MN·m/kg or higher, and including a prescribed glass composition.

## Claims

### Claim 1

An alkali-free glass having a strain point of 700° C. or higher and 740° C. or lower, a density of 2.6 g/cm3 or lower, a Young's modulus of 90 GPa or higher and 100 GPa or lower, an average coefficient of thermal expansion at 50° C. to 350° C. of 30×10−7/K or higher and 39×10−7/K or lower, a temperature T2 at which a glass viscosity reaches 102 dPa·s of 1590° C. or higher and 1690° C. or lower, a temperature T4 at which the glass viscosity reaches 104 dPa·s of 1350° C. or lower, a glass surface devitrification temperature (Tc) of lower than (T4+80)° C., and a specific elastic modulus of 36 MN·m/kg or higher, the alkali-free glass comprising:
as represented by mol % based on oxides,
SiO2: 55% or higher and 80% or lower;
Al2O3: 12% or higher and 20% or lower;
B2O3: 0.3% or higher and 5% or lower;
MgO: 5% or higher and 18% or lower;
CaO: 0.1% or higher and 12% or lower;
SrO: 0.1% or higher and 8% or lower; and
BaO: 0% or higher and 6% or lower; wherein
MgO+CaO+SrO+BaO is 20% or lower,
MgO/CaO is 1 or higher,
MgO/(MgO+CaO+SrO+BaO) is 0.5 or higher,
MgO+Al2O3 is 24% or higher and 38% or lower, and
when Formula (I) is (−3.125×[SiO2]−2.394×[Al2O3]−3.511×[B2O3]−2.167×[MgO]−2.608×[CaO]−3.161×[SrO]−3.583×[BaO]+3.795×102), a value of Formula (T) is 90 or higher and 100 or lower.

### Claim 2 (depends on 1)

The alkali-free glass according to claim 1, wherein
when Formula (II) is (0.213×[SiO2]+1.006×[Al2O3]−0.493×[B2O3]+1.158×[MgO]+1.386×[CaO]+3.092×[SrO]+4.198×[BaO]+2.004×102), a value of Formula (I)/Formula (II)×100 is 36 or higher.

### Claim 3 (depends on 1)

The alkali-free glass according to claim 1, wherein
(MgO+CaO)/(SrO+BaO) is 8 or higher.

### Claim 4 (depends on 1)

The alkali-free glass according to claim 1, wherein
when an average coefficient of linear expansion at 50° C. to 350° C. is set as a, the Young's modulus is set as E, and a photoelastic constant is set as C, a product α·E·C is 9.2×10−7/K or lower.

### Claim 5 (depends on 1)

The alkali-free glass according to claim 1, having the photoelastic constant of 31 nm/MPa/cm or lower.

### Claim 6 (depends on 1)

The alkali-free glass according to claim 1, having a glass transition point of 730° C. or higher and 850° C. or lower.

### Claim 7 (depends on 1)

The alkali-free glass according to claim 1, having a glass surface devitrification viscosity of 103.4 dPa·s or higher.

### Claim 8 (depends on 1)

The alkali-free glass according to claim 1, comprising: 0% to 1% of ZrO2 as represented by mol % based on oxides.

### Claim 9 (depends on 1)

The alkali-free glass according to claim 1, wherein
a total amount of Li2O, Na2O, and K2O is 0.2% or lower as represented by mol % based on oxides.

### Claim 10 (depends on 1)

The alkali-free glass according to claim 1, comprising: 0% or higher and 0.5% or lower of SnO2 as represented by mol % based on oxides.

### Claim 11 (depends on 1)

The alkali-free glass according to claim 1, comprising: 0% or higher and 1% or lower of F as represented by mol %.

### Claim 12 (depends on 1)

The alkali-free glass according to claim 1, having a β-OH value of the glass of 0.05 mm−1 or higher and 0.6 mm−1 or lower.

### Claim 13 (depends on 1)

A glass sheet, wherein
the glass sheet comprises the alkali-free glass according to claim 1, and has at least one side of 2400 mm or longer and a thickness of 1 mm or less.

### Claim 14 (depends on 1)

A method for manufacturing the alkali-free glass according to claim 1, the method comprising: forming the alkali-free glass by a float process or a fusion process.