# US 2024/0198447 A1 · Arc welded joint and arc welding method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0198447 A1
- Document ID: US20240198447A1
- Status: Published application
- Kind: A1
- Application number: 18/287,348
- Filed: 2022-04-26
- Published: 2024-06-20
- Earliest claimed: 2021-04-28
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Kyohei KONISHI; Hiroshi MATSUDA; Koichi TANIGUCHI
- Web page: https://patentgrep.com/patent/US20240198447A1

## CPC

- B23K 9/23: taking account of the properties of the materials to be welded
- B23K 9/025: for rectilinear seams
- B23K 9/173: and of a consumable electrode
- B23K 35/0261: {Rods, electrodes or wires}
- B23K 35/38: Selection of media, e.g. special atmospheres for surrounding the working area
- B23K 35/383: {mainly containing noble gases or nitrogen}
- B23K 2101/18: Sheet panels
- B23K 2103/04: Steel {or steel} alloys
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

An arc welded joint and an arc welding method. The arc welded joint has a weld formed by arc welding of an overlap of at least two steel sheets. A slag-covered area ratio is 20% or less. A Vickers hardness of a weld metal and a Vickers hardness of softened portions of a weld heat affected zone in the weld satisfy a specified relationship.

## Claims

### Claim 1

An arc welded joint having a weld formed by arc welding of an overlap of at least two steel sheets,
wherein a slag-covered area ratio SRATIO (%) represented by formula (1) is 20% or less:
SRATIO=100×SSLAGSBEAD (1)
where SBEAD is a bead surface area (mm2) of a weld bead in the weld, and SSLAG is part of the bead surface area SBEAD and is a slag surface area (mm2) of a region covered with a slag, and
a Vickers hardness of a weld metal and a Vickers hardness of softened portions of a weld heat affected zone in the weld satisfy the following relationships;
Hmax≤550, and
Hmin≥1.07×HHAZ
where Hmax is a maximum value of the Vickers hardness of the weld metal, Hmin is a minimum value of the Vickers hardness of the weld metal, and HHAZ is an average value of the Vickers hardness of the softened portions of the weld heat affected zone.

### Claim 2 (depends on 1)

The arc welded joint according to claim 1, wherein the maximum value of the Vickers hardness of the weld metal and the minimum value of the Vickers hardness of the weld metal satisfy the relationship Hmax−Hmin≤100.

### Claim 3 (depends on 1)

An arc welding method for obtaining the arc welded joint according to claim 1, the method comprising:
forming the weld by arc welding of the overlap of the at least two steel sheets while using a shielding gas including Ar gas and an oxidizing gas, the oxidizing gas satisfying the relationship of formula (2):
2×[O2]+[CO2]≤5 (2)
where [O2] is a vol % of O2 in the shielding gas, and [CO2] is a vol % of CO2 in the shielding gas.

### Claim 4 (depends on 3)

The arc welding method according to claim 3, wherein the steel sheets and a welding wire are intermittently short-circuited during the arc welding, and
an average short-circuit frequency FAVE (Hz) during the short-circuit is in a range of 20 to 300 Hz and a maximum short-circuit cycle TCYC (s) during the short-circuit is 1.5 s or less.

### Claim 5 (depends on 3)

The arc welding method according to claim 3, wherein the arc welding uses a pulse current as a welding current, and
a value of X (A·s/m) represented by formula (3) satisfies:
50≤X≤250X=(IPEAKλtPEAK/L)+(IPEAK+IBASE×(tUP+tDOWN)/(2×L) (3)
where IPEAK is a peak current (A) of the pulse current, IBASE is a base current (A), tPEAK (is a peak time (ms), tUP is a rise time (ms), tDOWN is a fall time (ms), and L is a distance (mm) between the steel sheets and a contact tip.

### Claim 6 (depends on 3)

The arc welding method according to claim 3, wherein the arc welding uses a solid wire as a welding wire, and
the arc welding is performed in reverse polarity.

### Claim 7

(canceled)

### Claim 8 (depends on 2)

An arc welding method for obtaining the arc welded joint according to claim 2, the method comprising:
forming the weld by arc welding of the overlap of the at least two steel sheets while using a shielding gas including Ar gas and an oxidizing gas, the oxidizing gas satisfying the relationship of formula (2):
2×[O2]+[CO2]≤5 (2)
where [O2] is a vol % of O2 in the shielding gas, and [CO2] is a vol % of CO2 in the shielding gas.

### Claim 9 (depends on 8)

The arc welding method according to claim 8, wherein the steel sheets and a welding wire are intermittently short-circuited during the arc welding, and
an average short-circuit frequency FAVE (Hz) during the short-circuit is in a range of 20 to 300 Hz and a maximum short-circuit cycle TCYC (s) during the short-circuit is 1.5 s or less.

### Claim 10 (depends on 8)

The arc welding method according to claim 8, wherein the arc welding uses a pulse current as a welding current, and
a value of X (A·s/m) represented by formula (3) satisfies:
50≤X≤250X=(IPEAK×tPEAK/L)+(IPEAK+IBASE)×(tUP+tDOWN)/(2×L) (3)
where IPEAK is a peak current (A) of the pulse current, IBASE is a base current (A), tPEAK is a peak time (ms), tUP is a rise time (ms), tDOWN is a fall time (ms), and L is a distance (mm) between the steel sheets and a contact tip.

### Claim 11 (depends on 4)

The arc welding method according to claim 4, wherein the arc welding uses a pulse current as a welding current, and
a value of X (A·s/m) represented by formula (3) satisfies:
50≤X≤250X=(IPEAK×TPEAK/L)+(IPEAK(+IBASE)×(TUP+TDOWN)/(2×L) (3)
where IPEAK is a peak current (A) of the pulse current, IBASE is a base current (A), tPEAK is a peak time (ms), tUP is a rise time (ms), tDOWN is a fall time (ms), and L is a distance (mm) between the steel sheets and a contact tip.

### Claim 12 (depends on 9)

The arc welding method according to claim 9, wherein the arc welding uses a pulse current as a welding current, and
a value of X (A·s/m) represented by formula (3) satisfies:
50≤X≤250X=(IPEAK×tPEAK/L)+(IPEAK+IBASE)×(tUP+tDOWN)/(2×L) (3)
where IPEAK is a peak current (A) of the pulse current, IBASE is a base current (A), tPEAK is a peak time (ms), tUP is a rise time (ms), tDOWN is a fall time (ms), and L is a distance (mm) between the steel sheets and a contact tip.

### Claim 13 (depends on 8)

The arc welding method according to claim 8, wherein the arc welding uses a solid wire as a welding wire, and
the arc welding is performed in reverse polarity.

### Claim 14 (depends on 4)

The arc welding method according to claim 4, wherein the arc welding uses a solid wire as a welding wire, and
the arc welding is performed in reverse polarity.

### Claim 15 (depends on 9)

The arc welding method according to claim 9, wherein the arc welding uses a solid wire as a welding wire, and
the arc welding is performed in reverse polarity.

### Claim 16 (depends on 5)

The arc welding method according to claim 5, wherein the arc welding uses a solid wire as a welding wire, and
the arc welding is performed in reverse polarity.

### Claim 17 (depends on 10)

The arc welding method according to claim 10, wherein the arc welding uses a solid wire as a welding wire, and
the arc welding is performed in reverse polarity.

### Claim 18 (depends on 11)

The arc welding method according to claim 11, wherein the arc welding uses a solid wire as a welding wire, and
the arc welding is performed in reverse polarity.

### Claim 19 (depends on 12)

The arc welding method according to claim 12, wherein the arc welding uses a solid wire as a welding wire, and
the arc welding is performed in reverse polarity.