# US 2024/0198418 A1 · Copper paste for printing capillary structure and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0198418 A1
- Document ID: US20240198418A1
- Status: Published application
- Kind: A1
- Application number: 18/338,378
- Filed: 2023-06-21
- Published: 2024-06-20
- Earliest claimed: 2022-12-20
- Assignees: AAC Technologies (Nanjing) Co., Ltd.
- Applicants: AAC Technologies (Nanjing) Co., Ltd.
- Inventors: Bo Zhang; Guochuang Huang; Hezhi Wang
- Web page: https://patentgrep.com/patent/US20240198418A1

## CPC

- B22F 1/10: Metallic powder containing lubricating or binding agents; Metallic powder containing organic material
- B22F 1/052: characterised by a mixture of particles of different sizes or by the particle size distribution
- B22F 1/107: containing organic material comprising solvents, e.g. for slip casting
- C09D 11/03: characterised by features other than the chemical nature of the binder
- C09D 11/033: characterised by the solvent
- C09D 11/037: characterised by the pigment
- C09D 11/102: containing macromolecular compounds obtained by reactions other than those only involving unsaturated carbon-to-carbon bonds
- C09D 11/106: containing macromolecular compounds obtained by reactions only involving carbon-to-carbon unsaturated bonds
- C09D 11/107: from unsaturated acids or derivatives thereof
- C09D 11/52: Electrically conductive inks
- C22C 1/0425: {Copper-based alloys}
- C22C 9/00: Alloys based on copper
- H01B 1/22: the conductive material comprising metals or alloys
- H01B 13/00: Apparatus or processes specially adapted for manufacturing conductors or cables
- H05K 7/20: Modifications to facilitate cooling, ventilating, or heating
- B22F 2301/10: Copper
- B22F 2304/058: Particle size above 300 nm up to 1 micrometer
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

The present invention discloses a copper paste for printing a capillary structure and a preparation method thereof. The copper paste consists of copper powder, a high molecular polymer, a solvent, a binder, a dispersant, a leveling agent, a tackifier and an antioxidant. Through the limitation on the copper powder and the high molecular polymer in the copper paste of the present invention, the prepared copper paste can be applied to a carrier of a vapor chamber by blade coating or screen printing, and then used as a wick after binder removal and sintering in hydrogen or hydrogen-nitrogen mixed gas, so as to reduce device investment and cost; and the thickness of the wick can be accurately controlled to be 10-100 μm, the structural strength is higher, the water absorption performance and the heat transfer performance are better, and the demand for miniaturization of electronic products is met.

## Claims

### Claim 1

A copper paste for printing a capillary structure, consisting of copper powder, a high molecular polymer, a solvent, a binder, a dispersant, a leveling agent, a tackifier and an antioxidant, wherein the particle size of the copper powder ranges from 0.5 μm to 10 μm, and the particle size of microspheres of the high molecular polymer ranges from 1 μm to 50 μm.

### Claim 2 (depends on 1)

The copper paste for printing a capillary structure according to claim 1, wherein the particle size of the microspheres of the high molecular polymer is one or more of 300-1000 meshes, 1000-3000 meshes and 5000-12000 meshes, and the porosity of the high molecular polymer is 35%-75%.

### Claim 3 (depends on 1)

The copper paste for printing a capillary structure according to claim 1, wherein the high molecular polymer is one or more of polymethyl methacrylate, polyisobutyl methacrylate, methyl methacrylate-isobutyl methacrylate copolymer, polyoxymethylene, polyurethane and polystyrene.

### Claim 4 (depends on 1)

The copper paste for printing a capillary structure according to claim 1, wherein the solvent is one or more of ethanol, propanol, isopropanol, n-butanol, ethylene glycol, 1,2-propanediol, 1,2-butanediol, 1,4-butanediol and water.

### Claim 5 (depends on 1)

The copper paste for printing a capillary structure according to claim 1, wherein the binder is one or more of polyvinylpyrrolidone (PVP), polyvinyl alcohol (PVA), polyvinyl butyral (PVB), polyurethane, hydroxymethyl cellulose and ethyl cellulose.

### Claim 6 (depends on 1)

The copper paste for printing a capillary structure according to claim 1, wherein the dispersant is one or more of methyl amyl alcohol, cellulose derivatives, polyacrylamide and polyethylene glycol fatty acid.

### Claim 7 (depends on 1)

The copper paste for printing a capillary structure according to claim 1, wherein the leveling agent is one or more of sodium dodecyl sulfate, sodium dodecyl benzene sulfonate, sodium tetradecyl sulfonate, sodium hexadecyl sulfonate, lecithin, triethanolamine, KH550, polyethylene glycol, triethanolamine, Tween 80 and Span 80.

### Claim 8 (depends on 1)

The copper paste for printing a capillary structure according to claim 1, wherein the tackifier is high-viscosity resin, and the high-viscosity resin is one or more of natural rubber, styrene-butadiene rubber, neoprene, and C5 and C9 petroleum resins.

### Claim 9 (depends on 1)

The copper paste for printing a capillary structure according to claim 1, wherein the antioxidant is one or more of citric acid, phytic acid, vitamins, oxalic acid, ascorbic acid and glucose.

### Claim 10 (depends on 1)

The copper paste for printing a capillary structure according to claim 1, wherein the mass ratio of the copper powder to the high molecular polymer is 8-9:1, the mass fraction of the solvent is 1%-70% of a mixture of the copper powder and the high molecular polymer, the mass fraction of the binder is 0.1%-30% of the mixture of the copper powder and the high molecular polymer, the mass fraction of the dispersant is 0.01%-5% of the mixture of the copper powder and the high molecular polymer, the mass fraction of the leveling agent is 0.01%-10% of the mixture of the copper powder and the high molecular polymer, the mass fraction of the tackifier is 0.01%-5% of the mixture of the copper powder and the high molecular polymer, and the mass fraction of the antioxidant is 0.01%-10% of the mixture of the copper powder and the high molecular polymer.

### Claim 11 (depends on 1)

The copper paste for printing a capillary structure according to claim 1, wherein the average particle size of the copper powder is 3 μm.

### Claim 12 (depends on 1)

A preparation method of the copper paste for printing a capillary structure according to claim 1, comprising the following steps:
uniformly mixing the high molecular polymer with the copper powder according to the composition of the copper paste; and
then adding the solvent, the binder, the dispersant, the leveling agent, the tackifier and the antioxidant and fully stirring them in a mixer for 0.5-6 h.