# US 2024/0198318 A1 · Iron-based catalyst and method of hydrogenating carbon dioxide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0198318 A1
- Document ID: US20240198318A1
- Status: Published application
- Kind: A1
- Application number: 18/433,005
- Filed: 2024-02-05
- Published: 2024-06-20
- Earliest claimed: 2022-12-16
- Assignees: Industrial Technology Research Institute
- Applicants: Industrial Technology Research Institute
- Inventors: Kuo-Ching WU; Pao-Tsern LIN; Hsi-Yen HSU; Chao-Huang CHEN
- Web page: https://patentgrep.com/patent/US20240198318A1

## CPC

- B01J 23/745: Iron
- B01J 23/78: with alkali- or alkaline earth metals
- B01J 35/615: {100-500 m2/g}
- B01J 35/633: {less than 0.5 ml/g}
- B01J 35/647: {2-50 nm}
- C07C 1/12: from carbon dioxide with hydrogen
- C10G 2/50: {from carbon dioxide with hydrogen}
- B01J 2235/05: Nuclear magnetic resonance [NMR]
- C07C 2523/745: Iron
- C07C 2523/78: with alkali- or alkaline earth metals or beryllium
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES

## Abstract

A method of hydrogenating carbon dioxide, including contacting carbon dioxide and hydrogen with an iron-based catalyst to form a liquid and a gas. The liquid includes CnH2n, CnH2n+2, or a combination thereof and water, wherein n is 5 to 18. The gas includes CH4, CmH2m, CmH2m+2, or a combination thereof, hydrogen, and carbon dioxide, wherein m is 2 to 9. The iron-based catalyst includes 70 mol % to 97 mol % of porous FeO(OH)x (wherein 1<x<2), and 3 mol % to 30 mol % of alkaline metal compound loaded onto the porous FeO(OH)x.

## Claims

### Claim 1

An iron-based catalyst, comprising:
70 mol % to 97 mol % of porous FeO(OH)x, wherein 1<x<2; and
3 mol % to 30 mol % of alkaline metal compound loaded on the porous FeO(OH)x.

### Claim 2 (depends on 1)

The iron-based catalyst as claimed in claim 1, wherein the porous FeO(OH)x has a specific surface area of at least 100 m2/g.

### Claim 3 (depends on 1)

The iron-based catalyst as claimed in claim 1, wherein the porous FeO(OH)x has a pore volume of 0.2 cm3/g to 0.5 cm3/g.

### Claim 4 (depends on 1)

The iron-based catalyst as claimed in claim 1, wherein the porous FeO(OH)x has an average pore size of 40 Å to 70 Å.

### Claim 5 (depends on 1)

The iron-based catalyst as claimed in claim 1, wherein the alkaline metal compound comprises sodium carbonate, potassium carbonate, sodium hydroxide, potassium hydroxide, sodium oxide, potassium oxide, or a combination thereof.

### Claim 6

A method of hydrogenating carbon dioxide, comprising:
(i) contacting carbon dioxide and hydrogen with an iron-based catalyst to form a liquid and a gas,
wherein the liquid comprises CnH2n, CnH2n+2, or a combination thereof and water, and n is 5 to 18,
wherein the gas comprises CH4, CmH2m, CmH2m+2, or a combination thereof, hydrogen, and carbon dioxide, and m is 2 to 9,
wherein the iron-based catalyst comprises:
70 mol % to 97 mol % of porous FeO(OH)x, wherein 1<x<2; and
3 mol % to 30 mol % of alkaline metal compound loaded on the porous FeO(OH)x.

### Claim 7 (depends on 6)

The method as claimed in claim 6, wherein the hydrogen and the carbon dioxide contacting the iron-based catalyst have a ratio of 2:1 to 4:1, and the hydrogen and the carbon dioxide contacting the iron-based catalyst have a gas hourly space velocity of 300 hr−1 to 3000 hr−1.

### Claim 8 (depends on 6)

The method as claimed in claim 6, wherein the step of contacting the carbon dioxide and the hydrogen with the iron-based catalyst is performed under a pressure of 50 psi to 400 psi at a temperature of 260° C. to 360° C.

### Claim 9 (depends on 6)

The method as claimed in claim 6, further comprising:
(ii) separating the gas and the liquid; and
(iii) contacting the gas with another iron-based catalyst to form another liquid and another gas,
wherein the other liquid comprises CnH2n, CnH2n+2, or a combination thereof and water, and n is 5 to 18,
wherein the other gas comprises CH4, CmH2m, CmH2m+2, or a combination thereof, hydrogen, and carbon dioxide, and m is 2 to 9,
wherein the other iron-based catalyst comprises:
70 mol % to 97 mol % of another porous FeO(OH)x, wherein 1<x<2; and
3 mol % to 30 mol % of another alkaline metal compound loaded on the other porous FeO(OH)x.

### Claim 10 (depends on 9)

The method as claimed in claim 9, wherein the conversion rate of carbon dioxide in step (iii) is higher than the conversion rate of carbon dioxide in step (i).

### Claim 11 (depends on 9)

The method as claimed in claim 9, further comprising repeating step (ii) and step (iii) several times.