# US 2024/0194876 A1 · Positive electrode additive for a lithium secondary battery, a method of manufacturing same, and a positive electrode for a lithium secondary battery including same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0194876 A1
- Document ID: US20240194876A1
- Status: Published application
- Kind: A1
- Application number: 18/384,736
- Filed: 2023-10-27
- Published: 2024-06-13
- Earliest claimed: 2022-12-08
- Assignees: Hyundai Motor Company; Kia Corporation; University-Industry Cooperation Group of Kyung Hee University
- Applicants: Hyundai Motor Company; Kia Corporation; University-Industry Cooperation Group of Kyung Hee University
- Inventors: Da Bin Jang; Sung Ho Ban; Sang Hun Lee; Yong Hoon Kim; Ha Eun Lee; Seung Min Oh; Chang Hoon Song; Sung Min Park; Hyo Bin Lee; Tae Hee Kim; Min Sik Park
- Web page: https://patentgrep.com/patent/US20240194876A1

## CPC

- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/366: {as layered products}
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/052: Li-accumulators
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive electrode additive for a lithium secondary battery can improve atmospheric stability. A method of manufacturing the same and a positive electrode for a lithium secondary battery includes the same. The positive electrode additive for a lithium secondary battery is used to manufacture the positive electrode for a lithium secondary battery and includes a lithium (Li)-based additive core and a coating layer of NbOXCy (0≤x≤2.5 and 0≤y≤1; where Nb=niobium, O=oxygen, C=carbon) formed on a surface of the additive core.

## Claims

### Claim 1

A positive electrode additive, which is used to prepare a positive electrode for a lithium secondary battery, the positive electrode additive comprising:
a lithium (Li)-based additive core; and
a coating layer of NbOXCy (0≤x≤2.5 and 0≤y≤1; where Nb=niobium, O=oxygen, C=carbon) formed on a surface of the additive core.

### Claim 2 (depends on 1)

The positive electrode additive of claim 1, wherein the additive core is formed of Li2MO2 (M=Ni, Cu; where Ni=nickel, Cu=copper).

### Claim 3 (depends on 1)

The positive electrode additive of claim 1, wherein the coating layer ranges from 1 to 10 wt % based on 100 wt % of the additive core.

### Claim 4

A method of manufacturing a positive electrode additive for a lithium secondary battery, which is used to manufacture a positive electrode for a lithium secondary battery, the method comprising:
a core preparation operation of preparing a lithium (Li)-based additive core;
a coating solution preparation operation of preparing a coating solution to form a coating layer composed of NbOXCy (0≤x≤2.5 and 0≤y≤1; where Nb=niobium, O=oxygen, C=carbon); and
a coating operation of coating a surface of the additive core with the coating solution and forming a coating layer.

### Claim 5 (depends on 4)

The method of claim 4, wherein, in the core preparation operation, lithium dioxide (Li2O) is reacted with a MO precursor (M=Ni, Cu) to prepare a powdered additive core of Li2MO2 (M=Ni, Cu; where Ni=nickel, Cu=copper).

### Claim 6 (depends on 5)

The method of claim 5, wherein the core preparation operation includes:
a core pelletization process of mixing and pelletizing Li2O and the MO precursors (M=Ni, Cu); and
a core sintering process of heating and sintering the pelletized core material in an inert atmosphere to obtain the additive core.

### Claim 7 (depends on 4)

The method of claim 4, wherein, in the coating solution preparation operation, the coating solution is prepared by dispersing niobium ethoxide (Nb(OC2H5)5) and urea (CH4N2O) at the same molar ratio in a solvent.

### Claim 8 (depends on 7)

The method of claim 7, wherein the coating operation includes:
a dispersion operation of dispersing the additive core in the prepared coating solution;
a reaction operation of generating a reactant forming the coating layer on the surface of the additive core by stirring and reacting the additive core dispersed in the solvent with Nb(OC2H5)5 and CH4N2O;
a drying operation of drying the solvent in which the reactant is generated in an inert atmosphere; and
a sintering operation of sintering the dried reactant and producing an additive in the form of a powder.

### Claim 9 (depends on 8)

The method of claim 8, wherein, in the reaction operation, the additive core dispersed in the solvent, Nb(OC2H5)5, and CH4N2O are stirred ranging from 300 to 400 revolutions-per-minute (rpm) for ap period of time ranging from 1 to 2 hours at room temperature, and the solvent is evaporated while reacting with Nb(OC2H5)5 and CH4N2O on the surface of the additive core.

### Claim 10 (depends on 8)

The method of claim 8, wherein, in the drying operation, the additive core having the reactant formed on the surface thereof is dried at a temperature ranging from 110 to 130° C. for a period of time ranging from 11 to 13 hours in a vacuum oven.

### Claim 11 (depends on 8)

The method of claim 8, wherein, in the sintering operation, the coating layer is formed on the surface of the additive core by performing heat treatment on the additive core having the reactant generated on the surface thereof at a temperature ranging from 250 to 350° C. for a period of time ranging from 3 to 5 hours in a sintering furnace in an argon (Ar) atmosphere.

### Claim 12

A positive electrode for a lithium secondary battery, the positive electrode including a positive electrode additive comprising:
a lithium (Li)-based additive core; and
a coating layer of NbOXCy (0≤x≤2.5 and 0≤y≤1; where Nb=niobium, O=oxygen, C=carbon) formed on a surface of the additive core.

### Claim 13 (depends on 12)

The positive electrode of claim 12, further comprising:
a conductive material and a binder.

### Claim 14 (depends on 12)

A lithium secondary battery comprising the positive electrode according to claim 12.

### Claim 15 (depends on 14)

The lithium secondary battery of claim 14, further comprising:
a negative electrode including a negative electrode active material; and
an electrolyte.