# US 2024/0191142 A1 · Process for stable blend of waste plastic with petroleum feed for feeding to oil refinery units and process of preparing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0191142 A1
- Document ID: US20240191142A1
- Status: Published application
- Kind: A1
- Application number: 18/349,333
- Filed: 2023-07-10
- Published: 2024-06-13
- Earliest claimed: 2022-12-12
- Assignees: Chevron U.S.A. Inc.
- Applicants: Chevron U.S.A. Inc.
- Inventors: Hye-Kyung C. Timken; Joel E. Schmidt; Tengfei Liu
- Web page: https://patentgrep.com/patent/US20240191142A1

## CPC

- C10G 1/10: from rubber or rubber waste
- C10G 1/002: {in combination with oil conversion- or refining processes}
- C10G 2300/1003: Waste materials
- C10G 2300/1092: C2-C4 olefins
- C10G 2300/201: Impurities
- C10G 2300/4006: Temperature
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES

## Abstract

Provided is a blend of a petroleum feedstock and 1-20 wt. % of plastic, based on the weight of the blend, with the plastic comprising polyethylene and/or polypropylene, and the plastic in the blend comprising finely dispersed microcrystalline particles having an average particle size of 10 micron to less than 100 microns, and less than 10 ppm chloride. A process for preparing a blend of plastic and petroleum is provided, comprising mixing together a petroleum feed and a plastic comprising polyethylene and/or polypropylene and heating the mixture above the melting point of the plastic, but less than 500° F. The blend mixture is then hot filtered with the resulting filtered blend mixture being heated to at least 500° F. The heated mixture can then be treated with a chloride removal guard bed. The resulting blend can then be cooled and stored or sent directly to a refinery conversion unit.

## Claims

### Claim 1

A blend of a petroleum feedstock and 1-20 wt. % of plastic, based on the weight of the blend, with the plastic comprising polyethylene and/or polypropylene, and the plastic in the blend comprising finely dispersed micron-size particles having an average particle size of 10 micron to less than 100 microns, and the blend comprises less than 100 ppm chloride.

### Claim 2 (depends on 1)

The blend of claim 1, prepared by the process of:
(a) heating a mixture of a petroleum based feed and the plastic together at a temperature above the melting point of the plastic but less than 500° F.;
(b) recovering a product from step (a) and hot filtering the product to remove contaminants and product a filtered blend;
(c) heating the filtered blend to a temperature of 550 to 700° F. (288 to 371° C.) to thereby decompose PVC to produce a liquid product; and
(d) optionally treating the liquid product with a chloride removal guard bed catalyst.

### Claim 3 (depends on 2)

The blend of claim 2, wherein the amount of plastic in the blend comprises from 1-10 wt. % of the blend.

### Claim 4 (depends on 2)

The blend of claim 2, wherein the plastic comprises low density polyethylene.

### Claim 5 (depends on 2)

The blend of claim 2, wherein the plastic comprises high density polyethylene.

### Claim 6 (depends on 2)

The blend of claim 2, wherein the plastic comprises multi-layer films comprising a metal barrier layer, polyethylene and/or polypropylene.

### Claim 7 (depends on 6)

The blend of claim 6, wherein the metal barrier layer is comprised of aluminum.

### Claim 8 (depends on 5)

The blend of claim 5, wherein the blend comprises from 1-10 wt. % of the high density polyethylene.

### Claim 9 (depends on 2)

The blend of claim 2, wherein the plastic comprises polypropylene having an average molecular weight, Mw, in the range of 5,000 to 150,000.

### Claim 10 (depends on 2)

The blend of claim 2, wherein the plastic comprises polypropylene having an average molecular weight, Mw, in the range of 150,000 to 400,000.

### Claim 11 (depends on 10)

The blend of claim 10, wherein the blend comprises from 1-10 wt. % of the polypropylene.

### Claim 12 (depends on 2)

The blend of claim 2, wherein the plastic comprises a mixture of polyethylene and polypropylene.

### Claim 13 (depends on 2)

The blend of claim 2, wherein the heating is conducted while stripping the liquid using gases such as nitrogen, hydrogen, steam, or light offgas from a conversion unit.

### Claim 14 (depends on 2)

The blend of claim 2, wherein the finely dispersed particles have an average particle size in the range of 10-50 microns.

### Claim 15 (depends on 2)

The blend of claim 2, wherein the finely dispersed particles have an average particle size in the range of 10 to less than 100 microns.

### Claim 16 (depends on 2)

The blend of claim 2, wherein the petroleum feedstock in the blend comprises vacuum gas oil, atmospheric gas oil, reformate, light cycle oil, heavy fuel oil, refinery hydrocarbon streams containing toluene, xylene, heptane or benzene, coker naphtha, C5-C6 isomerized paraffinic naphtha, FCC naphtha, hydrocracker bottom, gasoline, jet fuel, diesel or mixtures thereof.

### Claim 17 (depends on 2)

The blend of claim 2, wherein the petroleum feedstock is chosen for preferred dissolution of polyethylene and polypropylene.

### Claim 18 (depends on 17)

The blend of claim 17, wherein the petroleum feedstock chosen is VGO.

### Claim 19 (depends on 2)

The blend of claim 2, wherein the petroleum feedstock in the blend comprises gas oil or heavy reformate.

### Claim 20 (depends on 16)

The blend of claim 16, wherein the blend comprises light cycle oil, gasoline, or diesel.

### Claim 21 (depends on 19)

The blend of claim 19, wherein the blend comprises light cycle oil, gasoline, or diesel.

### Claim 22 (depends on 16)

The blend of claim 16, wherein the blend comprises benzene, toluene, xylene or heptane.

### Claim 23 (depends on 19)

The blend of claim 19, wherein the blend comprises benzene, toluene, xylene or heptane.

### Claim 24 (depends on 2)

The blend of claim 2, wherein the blend is at a temperature above the melting point of the plastic and is a hot, homogenous liquid blend.

### Claim 25 (depends on 24)

The blend of claim 24, further comprising petroleum feedstock added to the blend.

### Claim 26

A process for preparing a blend of plastic and petroleum comprising:
(a) mixing a petroleum feed and a plastic comprising polyethylene and/or polypropylene together and heating the mixture above the melting point of the plastic, but less than 500° F., while mixing;
(b) recovering a product from step (a) and hot filtering the product to remove contaminants and product a filtered blend;
(c) heating the filtered blend to a temperature of 550° to 700° F. (288° to 371° C.) to thereby decompose PVC to produce a liquid product; and
(d) optionally treating the liquid product with a chloride removal guard bed catalyst.

### Claim 27 (depends on 26)

The process of claim 26, wherein the heating is conducted at a temperature of 550°-700° F. (288° to 371° C.) with a residence time of 5-240 minutes at a final heating temperature.

### Claim 28 (depends on 26)

The process of claim 26, wherein the heating is conducted while stripping the liquid using a gas such as nitrogen, hydrogen, steam, or light offgas from a conversion unit.

### Claim 29

A process for preparing a blend of plastic and petroleum comprising:
a) mixing a petroleum feed and a plastic comprising polyethylene and/or polypropylene together and heating the mixture above the melting point of the plastic, but less than 500° F., while mixing;
b) recovering a product from step (a) and hot filtering the product to remove contaminants and produce a filtered blend; and
c) treating the liquid product with a chloride removal guard bed catalyst at a temperature of 250°) to 700° F. (121° to 371° C.) to thereby decompose PVC to produce a liquid product.

### Claim 30 (depends on 29)

The process of claim 29, wherein the treating is conducted at a temperature of 250°-700° F. (121° to 371° C.) with a residence time of 5-240 minutes at a final treating temperature.