# US 2024/0191113 A1 · A binder composition free of phenol compound

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0191113 A1
- Document ID: US20240191113A1
- Status: Published application
- Kind: A1
- Application number: 18/286,587
- Filed: 2021-04-15
- Published: 2024-06-13
- Earliest claimed: 2021-04-15
- Applicants: Upm-Kymmene Corporation
- Inventors: Sanna VALKONEN
- Web page: https://patentgrep.com/patent/US20240191113A1

## CPC

- C09J 197/005: {Lignin}
- C08G 16/0225: {containing oxygen}
- C08H 6/00: {Macromolecular compounds derived from lignin, e.g. tannins, humic acids}
- C08L 97/005: {Lignin}
- B27D 1/04: to produce plywood or articles made therefrom; Plywood sheets {(making a layered veneer cutting block B27L5/00)}
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08H: DERIVATIVES OF NATURAL MACROMOLECULAR COMPOUNDS (polysaccharides C08B; natural rubber C08C; natural resins or their derivatives C09F; bituminous materials C10)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B27D: WORKING VENEER OR PLYWOOD (applying liquids or other fluent materials to surface in general B05; grinding, sanding, or polishing of wood B24; applying adhesives or glue to surfaces of wood B27G11/00; manufacture of veneer B27L5/00)

## Abstract

A method for producing a binder composition without using a compound selected from the class of phenols, is disclosed. The method comprises: (i) heating an aqueous composition comprising lignin and lignin oligomer in the presence of a catalyst at a temperature of 50-95° ° C. for 0.25-5 hours; (ii) mixing a cross-linking agent with the aqueous composition from (i) and heating the same at a temperature of 60-95° C. for polymerizing lignin, lignin oligomers, and cross-linking agent until a binder composition with a predetermined viscosity value is formed; wherein the molar ratio of crosslinking agent to lignin and lignin oligomer is 0.5-1.8.

## Claims

### Claim 1

A method for producing a binder composition without using a compound selected from the class of phenols, wherein the method comprises:
(i) heating an aqueous composition comprising lignin having a weight average molecular weight (Mw) of 2700-9000 g/mol and lignin oligomer having a weight average molecular weight (Mw) of 800-2500 g/mol in the presence of a catalyst at a temperature of 50-95° C. for 0.25-5 hours; and
(ii) mixing a crosslinking agent with the aqueous composition from (i) and heating the same at a temperature of 60-95° C. for polymerizing lignin, lignin oligomers, and crosslinking agent until a binder composition with a predetermined viscosity value is formed,
wherein the molar ratio of crosslinking agent to lignin and lignin oligomer is 0.5-1.8.

### Claim 2 (depends on 1)

The method of claim 1, wherein the total amount of crosslinking agent used for producing the binder composition is 3-8 weight-%, based on the total weight of the binder composition.

### Claim 3 (depends on 1)

The method of claim 1, wherein the molar ratio of crosslinking agent to lignin and lignin oligomer is 0.9-1.7.

### Claim 4 (depends on 1)

The method of claim 1, wherein the weight ratio of catalyst to lignin and lignin oligomer is 0.20-0.37.

### Claim 5 (depends on 1)

The method of claim 1, wherein the weight ratio of lignin oligomer to lignin is 0.05-1.0.

### Claim 6 (depends on 1)

The method of claim 1, wherein step (ii) comprises heating at a temperature of 75-90° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the lignin is softwood Kraft lignin having a weight average molecular weight (Mw) of 2700 9000 g/mol.

### Claim 8 (depends on 1)

The method of claim 1, wherein the crosslinking agent is an aldehyde prepared from bio-methanol.

### Claim 9 (depends on 1)

The method of claim 1, wherein heating in step (ii) is continued until a binder composition with a viscosity value of 200-1000 cp, as measured at 25° C., is formed.

### Claim 10

A binder composition obtainable by a method comprising:
(i) heating an aqueous composition comprising lignin having a weight average molecular weight (Mw) of 2700-9000 g/mol and lignin oligomer having a weight average molecular weight (Mw) of 800-2500 g/mol in the presence of a catalyst at a temperature of 50-95° C. for 0.25-5 hours; and
(ii) mixing a crosslinking agent with the aqueous composition from (i) and heating the same at a temperature of 60-95° C. for polymerizing lignin, lignin oligomers, and crosslinking agent until a binder composition with a predetermined viscosity value is formed,
wherein the molar ratio of crosslinking agent to lignin and lignin oligomer is 0.5-1.8.

### Claim 11 (depends on 10)

An adhesive composition comprising the binder composition of claim 10.

### Claim 12 (depends on 10)

The binder composition of claim 10, wherein the binder composition is configured to be used in an impregnation application, for gluing a wood product or layered wood product or wood panel, for producing a laminate, shuttering film, mineral wool, nonwoven fiber product, molded fiber product, or extruded fiber product.

### Claim 13

A product comprising:
a binder composition obtained by the method comprising (i) heating an aqueous composition comprising lignin having a weight average molecular weight (Mw) of 2700-9000 g/mol and lignin oligomer having a weight average molecular weight (Mw) of 800-2500 g/mol in the presence of a catalyst at a temperature of 50-95° C. for 0.25-5 hours, and (ii) mixing a crosslinking agent with the aqueous composition from (i) and heating the same at a temperature of 60-95° C. for polymerizing lignin, lignin oligomers, and crosslinking agent until a binder composition with a predetermined viscosity value is formed, wherein the molar ratio of crosslinking agent to lignin and lignin oligomer is 0.5-1.8,
wherein the product has one or more of the following properties:
the amount of formaldehyde emissions being 0.01-0.5 mg/l, when measured by desiccator method EN ISO 12460-4,
the amount of formaldehyde emissions being 0.01-0.40 mg/m2*h, when measured by gas analysis EN ISO 12460-3, and
fulfilling the minimum bonding class 1-4, when measured by bonding quality test method EN 314-1 & EN314-2.