Building materials
AssigneeDmat S.R.L.
InventorsPaolo SABATINI, Michel DI TOMMASO
Life of this patent
Estimating the term…
Abstract
Disclosed herein are mixtures for cementitious building materials, methods of preparing same, and methods of cementing using same.
Claims31
A method of making a cementitious mixture for building materials comprising:
- (a) obtaining a cementitious mixture comprising a calcium compound and ordinary Portland cement (OPC) and optionally supplementary cementitious material (SCM), wherein the dosage of the calcium compound is about 3.1% to about 35% of the total binder content of the cementitious mixture;
- and
- (b) adding water to the cementitious mixture.
A method of making a cementitious mixture for building materials comprising obtaining a cementitious mixture comprising a calcium compound and ordinary Portland cement (OPC) and optionally supplementary cementitious material (SCM), and mixing the cementitious mixture, wherein the dosage of the calcium compound is about 3.1% to about 35% of the total binder content of the cementitious mixture.
A method of making a concrete mixture for building materials comprising:
- (a) obtaining a cementitious mixture comprising a calcium compound, ordinary Portland cement (OPC), fine aggregates, and coarse aggregates, and optionally supplementary cementitious material (SCM), wherein the dosage of the calcium compound is about 6.5% to about 15% of the total binder content of the cementitious mixture;
- and
- (b) adding water to the cementitious mixture.
A method of making a concrete mixture for building materials comprising obtaining a cementitious mixture comprising a calcium compound, ordinary Portland cement (OPC), fine aggregates, and coarse aggregates, and optionally supplementary cementitious material (SCM), and mixing the cementitious mixture, wherein the dosage of the calcium compound is about 6.5% to about 15% of the total binder content of the cementitious mixture.
A concrete for building materials comprising a cementitious mixture comprising a calcium compound, ordinary Portland cement (OPC), optionally supplementary cementitious material (SCM), fine aggregates, coarse aggregates, and water, optionally wherein the fine aggregates comprises one or more of one or more of sand, crushed stone, silt, stone dust, and clay, wherein the dosage of the calcium compound is about 3.1% to about 35% of the total binder content of the cementitious mixture, optionally comprising a reinforcement.