# US 2024/0189937 A1 · Friction stir welding tool and friction stir welding method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0189937 A1
- Document ID: US20240189937A1
- Status: Published application
- Kind: A1
- Application number: 18/285,965
- Filed: 2022-04-07
- Published: 2024-06-13
- Earliest claimed: 2021-04-08
- Assignees: Ntk Cutting Tools Co., Ltd.; Osaka University
- Applicants: Ntk Cutting Tools Co., Ltd.; Osaka University
- Inventors: Yuki Takeuchi; Jun Moteki; Hiroki Takeuchi; Yusuke Katsu; Yasushi Hara; Hidetoshi Fujii; Yoshiaki Morisada
- Web page: https://patentgrep.com/patent/US20240189937A1

## CPC

- B23K 20/1255: {Tools therefor, e.g. characterised by the shape of the probe}
- B23K 20/2333: {one layer being aluminium, magnesium or beryllium}
- B23K 2101/18: Sheet panels
- B23K 2103/10: Aluminium or alloys thereof
- B23K 2103/15: {Magnesium or alloys thereof}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A friction stir welding tool and a friction stir welding method that can increase the amount of heat generation, while reducing the amount of escaping heat are provided. The friction stir welding tool (1) has a shoulder portion (7) and a probe portion (5) provided on a bottom surface of the shoulder portion (7) . The base material of the friction stir welding tool (1) is a ceramic material whose main phase is silicon nitride or sialon. The shoulder portion (7) has a diameter of 35 mm or greater.

## Claims

### Claim 1

A friction stir welding tool having a shoulder portion and a probe portion provided on a bottom surface of the shoulder portion, wherein
a ceramic material whose main phase is silicon nitride or sialon is used as a base material, and
a diameter of the shoulder portion is 35 mm or greater.

### Claim 2 (depends on 1)

The friction stir welding tool according to claim 1, wherein a ratio of a height of the probe portion to the diameter of the shoulder portion is 0.5 or less.

### Claim 3 (depends on 1)

The friction stir welding tool according to claim 1, wherein a ratio of a diameter of the probe portion at its root to the diameter of the shoulder portion is 0.67 or less.

### Claim 4 (depends on 1)

The friction stir welding tool according to claim 1, having a coating layer formed of TiN.

### Claim 5 (depends on 1)

The friction stir welding tool according to claim 1, wherein the probe portion includes a skirt region that expands toward the bottom surface of the shoulder portion,
wherein the skirt region has a region where a ratio of increase in outer diameter to height is larger as compared with a region of the probe portion other than the skirt region, and
wherein, in a cross section containing a center axis of the probe portion, at least one pair of straight portions that are symmetric with respect to the center axis and that satisfy the following conditions (1) and (2) appear in visible outlines of the skirt region:
condition (1): in the cross section, a distance between a point of intersection where a straight line containing the straight portion intersects with a straight line containing a visible outline of the region of the probe portion other than the skirt region, and a straight line passing through two points where a pair of straight lines containing the visible outlines of the region of the probe portion other than the skirt region intersect with a straight line containing the bottom surface of the shoulder portion, is 12% or greater and 55% or less of the height of the probe portion; and
condition (2): a taper angle between the pair of straight portions is 60° or greater and 160° or less.

### Claim 6 (depends on 1)

A friction stir welding method in which plates having a thickness of 15 mm or greater are welded together by the friction stir welding tool set forth in claims 1.