# US 2024/0189897 A1 · Nickel-based superalloy formed by selective laser melting and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0189897 A1
- Document ID: US20240189897A1
- Status: Published application
- Kind: A1
- Application number: 17/685,824
- Filed: 2022-03-03
- Published: 2024-06-13
- Earliest claimed: 2021-03-03
- Assignees: Northwestern Polytechnical University
- Applicants: Northwestern Polytechnical University
- Inventors: Haijun SU; Yong ZHAO; Meng WANG; Jun ZHANG; Min GUO; Lin LIU; Hengzhi FU
- Web page: https://patentgrep.com/patent/US20240189897A1

## CPC

- B22F 1/05: Metallic powder characterised by the size or surface area of the particles
- B22F 1/142: Thermal or thermo-mechanical treatment
- B22F 3/1007: {Atmosphere (B22F3/1021 takes precedence)}
- B22F 3/105: by using electric current {other than for infrared radiant energy}, laser radiation or plasma (B22F3/11 takes precedence){; by ultrasonic bonding (B22F3/115 takes precedence)}
- B22F 10/28: Powder bed fusion, e.g. selective laser melting [SLM] or electron beam melting [EBM]
- B22F 10/36: of energy beam parameters
- B33Y 70/10: Composites of different types of material, e.g. mixtures of ceramics and polymers or mixtures of metals and biomaterials
- B33Y 80/00: Products made by additive manufacturing
- C22C 1/0433: {Nickel- or cobalt-based alloys}
- C22C 19/05: with chromium
- C22C 19/055: {with the maximum Cr content being at least 20% but less than 30%}
- C22C 19/056: {with the maximum Cr content being at least 10% but less than 20%}
- C22C 19/057: {with the maximum Cr content being less 10%}
- B22F 2009/043: {by ball milling}
- B22F 2201/11: Argon
- B22F 2301/155: Rare Earth - Co or -Ni intermetallic alloys
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- Y02P 10/25: Process efficiency
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed are a nickel-based superalloy formed by selective laser melting and a preparation method thereof, belonging to the technical field of an additive manufacturing from metal powder. In the disclosure, CrFeNb alloy powder is used as a grain refiner, and its element composition is within the composition range of a nickel-based superalloy powder to ensure that the prepared nickel-based superalloy has the same element composition with the original alloy; the grain size in the nickel-based superalloy could be refined by the addition of CrFeNb alloy powder, such that the anisotropic columnar grain structure in the alloy is transformed to equiaxed grain structure, thereby improving mechanical properties of the alloy. The results of the examples show that the nickel-based superalloy prepared in the disclosure exhibits a yield strength of not less than 710 MPa at room temperature, a tensile strength of not less than 1010 MPa, an elongation of not less than 19%, and a hardness of not less than 330 HV; after the heat treatment, the nickel-based superalloy exhibits a yield strength of not less than 1400 MPa, a tensile strength of not less than 1100 MPa, an elongation of not less than 5.09%, and a hardness of not less than 530 HV.

## Claims

### Claim at position 1

1-10. (canceled)

### Claim 11

A method for preparing a nickel-based superalloy formed by selective laser melting, comprising:
(1) ball milling and drying a nickel-based superalloy powder and a grain refiner in sequence to obtain a mixed powder, the nickel-based superalloy powder being an IN718 alloy powder, and the grain refiner being a CrFeNb alloy powder; and
(2) selective laser melting the mixed powder obtained in act (1) to obtain the nickel-based superalloy,
wherein the CrFeNb alloy powder in act (1) comprises, in percentages by mass, 24-28% of Cr, 25-30% of Fe, and 45-50% of Nb;
the grain refiner in the mixed powder in act (1) accounts for 2 wt. %-4 wt. %; and
the selective laser melting in act (2) is performed under conditions:
a laser power of 200-250 W, a scanning speed of 667-833 mm/s, and a layer thickness of 40-60 μm, a hatch distance of 50-90 μm, and a laser spot diameter of 75 μm.

### Claim 12 (depends on 11)

The method as claimed in claim 11, wherein in act (1), the nickel-based superalloy powder comprises, in percentages by mass, 18-19% of Fe, 52-53% of Ni, 19-20% of Cr, 3.0-3.5% of Mo, 0.2-0.3% of Al, 0.7-0.8% of Ti, 5.4-5.6% of Nb, 0.2-0.3% of Co, 0.01-0.02% of C, 0.04-0.05% of Mn, 0.1-0.2% of Si, 0.02-0.03% of Cu, not more than 0.0015% of S, and not more than 0.005% of B.

### Claim 13 (depends on 11)

The method as claimed in claim 11, wherein in act (1), the nickel-based superalloy powder has a particle size of not larger than 53 μm, an average particle size of 20-25 μm, an oxygen content of 300-310 ppm, an apparent density of 4.30-4.40 g/cm3, and a tap density of 5.00-5.10 g/cm3.

### Claim 14 (depends on 11)

The method as claimed in claim 11, wherein in act (1), the CrFeNb alloy powder has a particle size of not larger than 25 μm, and a theoretical density of 8.0-8.5 g/cm3.

### Claim 15 (depends on 11)

The method as claimed in claim 11, wherein the drying in act (1) is performed at a temperature of 60-80° C. for 12-24 h.

### Claim 16 (depends on 11)

The method as claimed in claim 11, wherein the selective laser melting in act (2) is performed in a protective atmosphere, and the protective atmosphere is provided by high-purity argon gas.

### Claim 17 (depends on 11)

A nickel-based superalloy prepared by the method as claimed in claim 11.