# US 2024/0189894 A1 · Oxidation resistant al-mg high strength die casting foundry alloys

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0189894 A1
- Document ID: US20240189894A1
- Status: Published application
- Kind: A1
- Application number: 18/286,532
- Filed: 2022-04-01
- Published: 2024-06-13
- Earliest claimed: 2021-04-14
- Assignees: Rio Tinto Alcan International Limited
- Applicants: Rio Tinto Alcan International Limited
- Inventors: Lei Pan; Francis Breton; Martin Morel
- Web page: https://patentgrep.com/patent/US20240189894A1

## CPC

- B22D 21/007: {with low melting point, e.g. Al 659 degrees C, Mg 650 degrees C}
- B22D 21/04: Casting aluminium or magnesium {(no material; see B22D21/007)}
- B22D 17/14: Machines with evacuated die cavity
- C22C 21/06: with magnesium as the next major constituent
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The present disclosure concerns a foundry alloy suitable for casting operations which lack beryllium. The foundry alloy comprises, in weight percent, Mg (between about 1.0 and about 17.0), Fe (between about 0.5 and about 1.8), one of Ca (between about 0.003 and about 6.0) or Sr (between about 0.003 and about 2.5), optionally a grain refiner and the balance being aluminum and unavoidable impurities. The foundry alloy can be used in a process for making a cast aluminum product, for reducing Mg loss and/or dross generation during the casting operation.

## Claims

### Claim 1

A foundry alloy comprising, in weight percent:
Mg between about 1.0 and about 17.0;
Fe between about 0.5 and about 1.8;
one of Ca between about 0.003 and about 6.0 or Sr between about 0.003 and about 2.5; and
the balance being aluminum and unavoidable impurities,
wherein the foundry alloy lacks Be as an alloying element.

### Claim 2 (depends on 1)

The foundry alloy of claim 1, further comprising a grain refiner.

### Claim 3

(canceled)

### Claim 4 (depends on 1)

The foundry alloy of claim 1, comprising between about 0.01 and about 0.3 Ca.

### Claim 5 (depends on 1)

The foundry alloy of claim 1, comprising between about 3.0 to about 8.0 Mg, optionally between about 4.0 and about 6.0 Mg.

### Claim 6 (depends on 1)

The foundry alloy of claim 1, comprising between about 4.0 and about 6.0 Mg.

### Claim at position 7

7-8. (canceled)

### Claim 9 (depends on 1)

A process for making a cast aluminum product, the process comprising casting the foundry aluminum alloy of claim 1 in a mold.

### Claim 10 (depends on 9)

The process of claim 9, further comprising submitting the cast aluminum alloy to high-pressure vacuum die casting, optionally lacking a post-cast thermal treatment step.

### Claim at position 10

11-18. (canceled)

### Claim 19 (depends on 9)

The process of claim 9, wherein the process further compromises limiting Mg loss and dross generation by adding one of Ca between about 0.003 and about 6.0 or Sr between about 0.003 and about 2.5 to a first aluminum alloy to obtain a foundry alloy intended to be cast, the first aluminum alloy comprising, in weight percent:
Mg between about 1.0 and about 17.0;
Fe between about 0.5 and about 1.8; and
the balance being aluminum and unavoidable impurities,
wherein the first aluminum alloy and the foundry alloy lack Be as an alloying element.

### Claim 20 (depends on 19)

The process of claim 19, wherein the first aluminum alloy further comprises a grain refiner.

### Claim 21 (depends on 19)

The process of claim 19, further comprising melting the foundry alloy to obtain a molten foundry alloy.

### Claim 22 (depends on 21)

The process of claim 21, for reducing Mg loss lower than about 12 weight percent, when the molten foundry alloy is held for a period of at least 6 hours.

### Claim 23 (depends on 21)

The process of claim 21, for reducing dross generation lower than about 7 weight percent, when the molten foundry alloy is held for a period of at least 6 hours.

### Claim 24 (depends on 21)

The process of claim 21, further comprising casting the molten foundry alloy to obtain a cast aluminum alloy.

### Claim 25 (depends on 24)

The process of claim 24, further comprising submitting the cast aluminum alloy to high-pressure vacuum die casting.

### Claim 26 (depends on 19)

The process of claim 19, lacking a post-cast heat treatment step.

### Claim 27 (depends on 19)

The process of claim 19, wherein the first aluminum alloy comprises Ca.

### Claim 28 (depends on 27)

The process of claim 27, wherein the first aluminum alloy comprises between about 0.01 and about 0.3 Ca.

### Claim 29 (depends on 19)

The process of claim 19, wherein the first aluminum alloy comprises between about 3.0 and about 8.0 Mg.

### Claim 30 (depends on 19)

The process of claim 19, wherein the first aluminum alloy comprises between about 4.0 and about 6.0 Mg.

### Claim 31 (depends on 19)

The process of claim 19, wherein the first aluminum alloy comprises between about 0.8 and about 1.8 Fe.