# US 2024/0189806 A1 · Defect engineering and modification of substrates for supported metal/metal oxide catalysts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0189806 A1
- Document ID: US20240189806A1
- Status: Published application
- Kind: A1
- Application number: 18/390,793
- Filed: 2023-12-20
- Published: 2024-06-13
- Earliest claimed: 2020-01-17
- Assignees: University of Central Florida Research Foundation, Inc.
- Applicants: University of Central Florida Research Foundation, Inc.
- Inventors: Fudong Liu; Shaohua Xie
- Web page: https://patentgrep.com/patent/US20240189806A1

## CPC

- B01J 37/0201: {Impregnation}
- B01J 37/0244: {Coatings comprising several layers}
- B01J 23/42: Platinum
- B01J 23/63: with rare earths or actinides
- B01J 23/83: with rare earths or actinides
- B01J 37/0242: {Coating followed by impregnation}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/16: Reducing
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

A catalyst support structure may include a base material and a metal oxide support structure. The metal oxide support structure may be formed by loading a first concentration of precursors of a metal oxide onto the base material using incipient wetness impregnation (IWI) to form the catalyst support structure, performing a first calcination process on the catalyst support structure at a first temperature to produce first structures of the metal oxide, loading a second concentration of precursors of the metal oxide onto the catalyst support structure using IWI to at least partially cover the first structures of the metal oxide, and performing a second calcination process on the catalyst support structure at a second temperature lower than the first temperature to produce second structures of the metal oxide.

## Claims

### Claim 1

A catalyst support structure comprising:
a base material; and
a metal oxide support structure, wherein the metal oxide support structure is formed by:
loading a first concentration of precursors of a metal oxide onto the base material using incipient wetness impregnation (IWI) to form the catalyst support structure;
performing a first calcination process on the catalyst support structure at a first temperature to produce first structures of the metal oxide, wherein at least one of the first concentration or the first temperature are selected to produce mixed oxide species at an interface with the base material;
loading a second concentration of precursors of the metal oxide onto the catalyst support structure using IWI to at least partially cover the first structures of the metal oxide, wherein the second concentration is higher than the first concentration; and
performing a second calcination process on the catalyst support structure at a second temperature lower than the first temperature to produce second structures of the metal oxide, wherein at least one of the second concentration or the second temperature are selected to produce the second structures of the metal oxide with a size scale smaller than a size scale of the first structures of the metal oxide.

### Claim 2 (depends on 1)

The catalyst support structure of claim 1, wherein the metal oxide comprises:
a reducible metal oxide.

### Claim 3 (depends on 2)

The catalyst support structure of claim 2, wherein the reducible metal oxide comprises:
at least one of a single metal oxide or a mixed metal oxide.

### Claim 4 (depends on 1)

The catalyst support structure of claim 1, wherein in the metal oxide comprises:
at least of ceria, iron oxide, manganese oxide, or copper oxide, as well as their mixed metal oxides including ceria-zirconia, copper-cerium oxide, or iron-cobalt oxide.

### Claim 5 (depends on 1)

The catalyst support structure of claim 1, wherein the base material comprises:
an irreducible metal oxide support.

### Claim 6 (depends on 5)

The catalyst support structure of claim 5, wherein the irreducible metal oxide support comprises:
at least one of a single metal oxide support or a mixed metal oxide support.

### Claim 7 (depends on 1)

The catalyst support structure of claim 1, wherein the base material comprises:
at least one of one of Al2O3, SiO2, MgO, ZrO2, MgAl2O4, or La2O3—Al2O3.

### Claim 8 (depends on 1)

The catalyst support structure of claim 1, wherein at least one of the first calcination process or the second calcination process comprises:
heating the catalyst support structure in an atmosphere including oxygen at a temperature in a range from 350° C. to 900° C.

### Claim 9 (depends on 8)

The catalyst support structure of claim 8, wherein heating the catalyst support structure in the atmosphere including oxygen comprises:
heating the catalyst support structure in the atmosphere including oxygen for at least an hour.

### Claim 10 (depends on 1)

The catalyst support structure of claim 1, further comprising:
at least one of a metal or a metal oxide disposed on the metal oxide support structure.

### Claim 11 (depends on 10)

The catalyst support structure of claim 10, wherein the at least one of the metal or the metal oxide is formed by:
loading the at least one of the metal or the metal oxide on the metal oxide support structure after the second calcination process to form a catalyst structure; and
performing a calcination process on the catalyst structure.

### Claim 12 (depends on 10)

The catalyst support structure of claim 10, wherein the at least one of the metal or the metal oxide is formed by:
reducing the metal oxide support structure with a gas-phase reducing agent to generate a plurality of defect sites on a surface of the metal oxide support;
loading the at least one of the metal or the metal oxide onto the metal oxide support structure to generate a catalyst structure, wherein at least a portion of the metal or metal oxide attaches to the plurality of defect sites; and
performing a calcination process on the catalyst structure.

### Claim 13 (depends on 10)

The catalyst support structure of claim 10, wherein the metal comprises:
at least one of Pt, Pd, Rh, Ir, or Au, or a transition metal.

### Claim 14 (depends on 10)

The catalyst support structure of claim 10, wherein the metal oxide comprises:
at least one of copper oxide, nickel oxide, iron oxide or cobalt oxide.

### Claim 15 (depends on 1)

The catalyst support structure of claim 1, wherein the first temperature is greater than 550° C.

### Claim 16 (depends on 1)

The catalyst support structure of claim 1, wherein the first temperature is approximately 800° C. wherein the second temperature is approximately 550° C.

### Claim 17 (depends on 1)

The catalyst support structure of claim 1, wherein the first temperature is in a range of 550 to 1050° C., wherein the second temperature is in a range of 350 to 1050° C.