# US 2024/0189804 A1 · Cu-SAPO-34 CATALYST AND PREPARATION METHOD AND USE THEREOF

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0189804 A1
- Document ID: US20240189804A1
- Status: Published application
- Kind: A1
- Application number: 18/172,132
- Filed: 2023-02-21
- Published: 2024-06-13
- Earliest claimed: 2022-12-12
- Assignees: Dalian Maritime University
- Applicants: Dalian Maritime University
- Inventors: Xiaofeng WANG; Mengyue QIN; Qingbo LI
- Web page: https://patentgrep.com/patent/US20240189804A1

## CPC

- B01J 29/85: Silicoaluminophosphates [SAPO compounds]
- B01J 37/0018: {Addition of a binding agent or of material, later completely removed among others as result of heat treatment, leaching or washing,(e.g. forming of pores; protective layer, desintegrating by heat)}
- B01J 37/031: {Precipitation}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/088: {Decomposition of a metal salt}
- Y02T 10/12: Improving ICE efficiencies
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

The present disclosure belongs to the technical field of denitration catalysts, and provides a Cu-SAPO-34 catalyst and a preparation method and use thereof. In the preparation method provided by the present disclosure, during crystallization growth, an aluminum precursor, a phosphorus precursor, a silicon precursor, and a copper complex form a Cu-SAPO-34 molecular sieve catalyst under the guiding action of a template morpholine, and the template in the Cu-SAPO-34 molecular sieve catalyst is removed by roasting to obtain the Cu-SAPO-34 catalyst. In the preparation method, a molar ratio of phosphorus and aluminum in the Cu-SAPO-34 catalyst is controlled at (0.1-5):1, thereby increasing a particle size and a specific surface area of the Cu-SAPO-34 catalyst, which is conducive to adsorption of a reaction gas to improve a denitration efficiency. Meanwhile, aggregation of Cu2+ after hydrothermal aging of the Cu-SAPO-34 catalyst is suppressed, thereby improving a hydrothermal stability of the Cu-SAPO-34 catalyst.

## Claims

### Claim at position 1

-10. (canceled)

### Claim 11

A preparation method of a Cu-SAPO-34 catalyst, comprising the following steps:
mixing an aluminum precursor, a phosphorus precursor, a silicon precursor, and a template with water to obtain a molecular sieve precursor solution;
mixing a copper precursor with a ligand, and conducting complexation to obtain a copper complex;
mixing the molecular sieve precursor solution with the copper complex, and conducting crystallization growth to obtain a catalyst precursor; and
roasting the catalyst precursor to obtain the Cu-SAPO-34 catalyst; wherein
phosphorus in the phosphorus precursor and aluminum in the aluminum precursor have a molar ratio of (0.1-5):1; and
the template comprises morpholine.

### Claim 12 (depends on 11)

The preparation method according to claim 11, wherein the aluminum precursor is one or more selected from the group consisting of aluminum hydroxide, aluminum chloride, aluminum sulfate, aluminum nitrate, pseudoboehmite, and aluminum isopropoxide; the phosphorus precursor is one or more selected from the group consisting of aluminum phosphate, phosphoric acid, and phosphorus pentoxide; and the silicon precursor is one or more selected from the group consisting of silica sol, white carbon black, silica, and silicic acid.

### Claim 13 (depends on 11)

The preparation method according to claim 11, wherein silicon in the silicon precursor and the aluminum in the aluminum precursor have a molar ratio of (0.1-1.5):1.

### Claim 14 (depends on 12)

The preparation method according to claim 12, wherein silicon in the silicon precursor and the aluminum in the aluminum precursor have a molar ratio of (0.1-1.5):1.

### Claim 15 (depends on 11)

The preparation method according to claim 11, wherein the template and the aluminum in the aluminum precursor have a molar ratio of (0.1-2):1.

### Claim 16 (depends on 12)

The preparation method according to claim 12, wherein the template and the aluminum in the aluminum precursor have a molar ratio of (0.1-2):1.

### Claim 17 (depends on 11)

The preparation method according to claim 11, wherein the copper precursor is one or more selected from the group consisting of copper nitrate, copper chloride, and copper sulfate; the ligand is tetraethylenepentamine; the copper precursor and the ligand have a molar ratio of (0.01-0.5):1; and the complexation is conducted at 20° C. to 50° C. for 1 h to 4 h.

### Claim 18 (depends on 11)

The preparation method according to claim 11, wherein the copper complex and the aluminum in the aluminum precursor have a molar ratio of (0.01-0.3):1.

### Claim 19 (depends on 11)

The preparation method according to claim 11, wherein the copper complex and the aluminum in the aluminum precursor have a molar ratio of (0.01-0.3):1.

### Claim 20 (depends on 11)

The preparation method according to claim 11, wherein the crystallization growth is conducted at 150° C. to 250° C. for 12 h to 48 h.

### Claim 21 (depends on 11)

The preparation method according to claim 11, wherein the roasting is conducted at 300° C. to 550° C. for 5 h to 10 h.

### Claim 22 (depends on 11)

A Cu-SAPO-34 catalyst prepared by the preparation method according to claim 11.

### Claim 23 (depends on 22)

The Cu-SAPO-34 catalyst according to claim 22, wherein the aluminum precursor is one or more selected from the group consisting of aluminum hydroxide, aluminum chloride, aluminum sulfate, aluminum nitrate, pseudoboehmite, and aluminum isopropoxide; the phosphorus precursor is one or more selected from the group consisting of aluminum phosphate, phosphoric acid, and phosphorus pentoxide; and the silicon precursor is one or more selected from the group consisting of silica sol, white carbon black, silica, and silicic acid.

### Claim 24 (depends on 22)

The Cu-SAPO-34 catalyst according to claim 22, wherein silicon in the silicon precursor and the aluminum in the aluminum precursor have a molar ratio of (0.1-1.5):1.

### Claim 25 (depends on 23)

The Cu-SAPO-34 catalyst according to claim 23, wherein silicon in the silicon precursor and the aluminum in the aluminum precursor have a molar ratio of (0.1-1.5):1.

### Claim 26 (depends on 22)

The Cu-SAPO-34 catalyst according to claim 22, wherein the template and the aluminum in the aluminum precursor have a molar ratio of (0.1-2):1.

### Claim 27 (depends on 22)

The Cu-SAPO-34 catalyst according to claim 22, wherein the copper precursor is one or more selected from the group consisting of copper nitrate, copper chloride, and copper sulfate; the ligand is tetraethylenepentamine; the copper precursor and the ligand have a molar ratio of (0.01-0.5):1; and the complexation is conducted at 20° C. to 50° C. for 1 h to 4 h.

### Claim 28 (depends on 22)

The Cu-SAPO-34 catalyst according to claim 22, wherein the copper complex and the aluminum in the aluminum precursor have a molar ratio of (0.01-0.3):1.

### Claim 29 (depends on 22)

The Cu-SAPO-34 catalyst according to claim 22, wherein the crystallization growth is conducted at 150° C. to 250° C. for 12 h to 48 h.

### Claim 30 (depends on 22)

The Cu-SAPO-34 catalyst according to claim 22, wherein the roasting is conducted at 300° C. to 550° C. for 5 h to 10 h.