# US 2024/0189801 A1 · Tetrametallic bulk hydroprocessing catalysts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0189801 A1
- Document ID: US20240189801A1
- Status: Published application
- Kind: A1
- Application number: 18/344,380
- Filed: 2023-06-29
- Published: 2024-06-13
- Earliest claimed: 2020-05-04
- Assignees: Chevron U.S.A. Inc.
- Applicants: Chevron U.S.A. Inc.
- Inventors: Xiaoying OUYANG; Viorel DUMA; Alexander KUPERMAN; Ibrahim UCKUNG; Theodorus Ludovicus Michael MAESEN; Axel BRAIT; Charles WILSON
- Web page: https://patentgrep.com/patent/US20240189801A1

## CPC

- B01J 23/8993: {with chromium, molybdenum or tungsten}
- B01J 35/613: {10-100 m2/g}
- B01J 21/063: {Titanium; Oxides or hydroxides thereof}
- B01J 23/002: {Mixed oxides other than spinels, e.g. perovskite}
- B01J 23/8885: {containing also molybdenum}
- B01J 27/0515: {with iron group metals or platinum group metals}
- B01J 35/31: Density
- B01J 35/615: {100-500 m2/g}
- B01J 35/633: {less than 0.5 ml/g}
- B01J 35/635: {0.5-1.0 ml/g}
- B01J 37/0009: {Use of binding agents; Moulding; Pressing; Powdering; Granulating; Addition of materials ameliorating the mechanical properties of the product catalyst}
- B01J 37/0045: {Drying a slurry, e.g. spray drying}
- B01J 37/031: {Precipitation}
- B01J 37/033: {Using Hydrolysis}
- B01J 37/036: {to form a gel or a cogel}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/20: Sulfiding
- C07C 5/10: of aromatic six-membered rings
- C10G 45/00: Refining of hydrocarbon oils using hydrogen or hydrogen-generating compounds
- C10G 47/00: Cracking of hydrocarbon oils, in the presence of hydrogen or hydrogen- generating compounds, to obtain lower boiling fractions (C10G15/00 takes precedence; destructive hydrogenation of non-melting solid carbonaceous or similar materials C10G1/06)
- C10G 49/00: Treatment of hydrocarbon oils, in the presence of hydrogen or hydrogen-generating compounds, not provided for in a single one of groups C10G45/02, C10G45/32, C10G45/44, C10G45/58 or C10G47/00
- C10G 49/04: containing nickel, cobalt, chromium, molybdenum, or tungsten metals, or compounds thereof
- B01J 2235/15: X-ray diffraction
- B01J 2235/30: Scanning electron microscopy; Transmission electron microscopy
- B01J 2523/00: Constitutive chemical elements of heterogeneous catalysts
- C10G 2300/1055: Diesel having a boiling range of about 230 - 330 °C
- C10G 2300/1074: Vacuum distillates
- C10G 2300/4006: Temperature
- C10G 2300/4012: Pressure
- C10G 2300/4018: Spatial velocity, e.g. LHSV, WHSV
- C10G 2300/42: Hydrogen of special source or of special composition
- C10G 2300/70: Catalyst aspects
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES

## Abstract

Bulk catalysts comprised of nickel, molybdenum, tungsten and titanium and methods for synthesizing bulk catalysts are provided. The catalysts are useful for hydroprocessing, particularly hydrodesulfurization and hydrodenitrogenation, of hydrocarbon feedstocks.

## Claims

### Claim at position 1

-28. (canceled)

### Claim 29

A method for preparing a bulk catalyst precursor having a formula of
Av[Ni(OH)x(L)py]z[MomW1-mO4][Ti(OH)nO2-n/2]w
wherein:
(i) A is an alkali metal cation, a rare earth metal cation, an ammonium cation, an organic ammonium cation, phosphonium cation, or a combination thereof;
(ii) L is an organic compound-based component; and
(iii) 0≤y≤−2/p; 0≤x<2; 0≤v<2; 0<z; 0<m<1; 0<<4; 0.1<w/(z+1)<10;
the method comprising:
(a) combining in a reaction mixture;
(i) a Ni-containing precursor;
(ii) a Mo-containing precursor;
(iii) a W-containing precursor;
(iv) a Ti-containing precursor;
(v) an organic compound-based component; and
(vi) a protic liquid; and
(b) reacting the mixture under conditions sufficient to cause precipitation of the bulk catalyst precursor;
with the steps to prepare the bulk catalyst precursor carried out at a temperature of no more than 200° C.; and
recovering a bulk catalyst precursor defined by a region of a quaternary phase diagram wherein the region is defined by ten points ABCDEFGHIJ and wherein the ten points, on a metal oxide basis (wt. %), are: A (Ni=39, Mo=1, W=41, Ti=20), B (Ni=39, Mo=1, W=72, Ti=20), C (Ni=9, Mo=17, W=54, Ti=20), D (Ni=31, Mo=25, W=24, Ti=20), E (Ni=40, Mo=14, W=26, Ti=20), F (Ni=34, Mo=1, W=36, Ti=30), G (Ni=7, Mo=1, W=63, Ti=30), H (Ni=8, Mo=15, W=48, Ti=30), I (Ni=27, Mo=22, W=21, Ti=30), and J (Ni=35, Mo=12, W=23, Ti=30).

### Claim 30 (depends on 29)

The method of claim 29, wherein the reaction mixture is prepared by:
preparing a first mixture comprising a Ni-containing precursor, a protic liquid, and an organic compound-based component;
preparing a second mixture comprising a Mo-containing precursor, a W-containing precursor, and a protic liquid;
adding a Ti-containing precursor to the first mixture, the second mixture, or a combination thereof;
heating both the first and second mixtures to a temperature of from 60° C. to 150° C.;
combining the first and second mixtures together.

### Claim 31 (depends on 30)

The method of claim 30, wherein the Ti-containing precursor is selected from TiO2 nanoparticles, colloidal TiO2, fumed TiO2, titanium hydroxide, organotitanium compounds, titanium halides, organotitanium halides, water-soluble titanium salts, or a combination thereof.

### Claim 32 (depends on 29)

The method of claim 29, wherein the reacting is carried out at one or more temperatures either (a) in a range of 60° C. to 100° C. under atmospheric pressure or (b) above 100° C. under autogenous pressure.

### Claim 33 (depends on 29)

The method of claim 29, wherein the organic compound-based component is selected from an organic acid or salt thereof, a sugar, a sugar alcohol, or a combination thereof.

### Claim 34 (depends on 33)

The method of claim 33, wherein the organic compound-based component is selected from glyoxylic acid, pyruvic acid, lactic acid, malonic acid, oxaloacetic acid, malic acid, fumaric acid, maleic acid, tartaric acid, gluconic acid, citric acid, oxamic acid, serine, aspartic acid, glutamic acid, iminodiacetic acid, ethylenediaminetetraacetic acid, fructose, glucose, galactose, mannose, sucrose, lactose, maltose, erythritol, xylitol, mannitol, sorbitol, or a combination thereof.

### Claim 35 (depends on 29)

The method of claim 29, further comprising one or more of the following steps:
compositing the bulk catalyst precursor with 0 to 40 wt. % with a material selected from the group of binder materials, conventional hydroprocessing catalysts, cracking compounds, or mixtures thereof;
spray-drying, (flash) drying, milling, kneading, slurry-mixing, dry or wet mixing, or combinations thereof;
shaping,
drying and/or thermally treating at a temperature of no more than 200° C.; or
sulfiding.

### Claim 36

A method for preparing a bulk catalyst precursor having a formula of
Av[Ni(OH)x(L)py]z[MomW1-mO4][Ti(OH)nO2-n/2]w
wherein:
(i) A is an alkali metal cation, a rare earth metal cation, an ammonium cation, an organic ammonium cation, phosphonium cation, or a combination thereof;
(ii) L is an organic compound-based component; and
(iii) 0≤y≤−2/p; 0≤x<2; 0≤v<2; 0<z; 0<m<1; 0<<4; 0.1<w/(z+1)<10;
the method comprising:
(a) combining in a reaction mixture;
(i) a Ni-containing precursor;
(ii) a Mo-containing precursor;
(iii) a W-containing precursor;
(iv) an organic compound-based component; and
(v) a protic liquid; and
(b) reacting the mixture under conditions sufficient to cause precipitation of an intermediate bulk catalyst precursor; and
(c) compositing the intermediate bulk catalyst precursor with a Ti-containing precursor to form the bulk catalyst precursor;
wherein the steps to prepare the bulk catalyst precursor are carried out at a temperature of no more than 200° C.; and
recovering a bulk catalyst precursor defined by a region of a quaternary phase diagram wherein the region is defined by ten points ABCDEFGHIJ and wherein the ten points, on a metal oxide basis (wt. %), are: A (Ni=39, Mo=1, W=41, Ti=20), B (Ni=39, Mo=1, W=72, Ti=20), C (Ni=9, Mo=17, W=54, Ti=20), D (Ni=31, Mo=25, W=24, Ti=20), E (Ni=40, Mo=14, W=26, Ti=20), F (Ni=34, Mo=1, W=36, Ti=30), G (Ni=7, Mo=1, W=63, Ti=30), H (Ni=8, Mo=15, W=48, Ti=30), I (Ni=27, Mo=22, W=21, Ti=30), and J (Ni=35, Mo=12, W=23, Ti=30).

### Claim 37 (depends on 36)

The method of claim 36, wherein the reaction mixture is prepared by:
preparing a first mixture comprising a Ni-containing precursor, a protic liquid, and, optionally, an organic compound-based component;
preparing a second mixture comprising a Mo-containing precursor, a W-containing precursor, and a protic liquid;
heating both the first and second mixtures to a temperature of from 60° C. to 150° C.; and
combining the first and second mixtures together.

### Claim 38 (depends on 36)

The method of claim 36, wherein the Ti-containing precursor is selected from TiO2 nanoparticles, fumed TiO2, or a combination thereof.

### Claim 39 (depends on 36)

The method of claim 36, wherein the intermediate bulk catalyst precursor is a Ni—Mo—W bulk catalyst precursor.

### Claim 40 (depends on 36)

The method of claim 36, wherein the reacting is carried out at one or more temperatures either (a) in a range of 60° C. to 100° C. under atmospheric pressure or (b) above 100° C. under autogenous pressure.

### Claim 41 (depends on 36)

The method of claim 36, wherein the organic compound-based component is selected from an organic acid or salt thereof, a sugar, a sugar alcohol, or a combination thereof.

### Claim 42 (depends on 41)

The method of claim 41, wherein the organic compound-based component is selected from glyoxylic acid, pyruvic acid, lactic acid, malonic acid, oxaloacetic acid, malic acid, fumaric acid, maleic acid, tartaric acid, gluconic acid, citric acid, oxamic acid, serine, aspartic acid, glutamic acid, iminodiacetic acid, ethylenediaminetetraacetic acid, fructose, glucose, galactose, mannose, sucrose, lactose, maltose, erythritol, xylitol, mannitol, sorbitol, or a combination thereof.

### Claim 43 (depends on 36)

The method of claim 36, further comprising one or more of the following steps:
compositing the bulk catalyst precursor with 0 to 40 wt. % with a material selected from the group of binder materials, conventional hydroprocessing catalysts, cracking compounds, or mixtures thereof;
spray-drying, (flash) drying, milling, kneading, slurry-mixing, dry or wet mixing, or combinations thereof;
shaping,
drying and/or thermally treating at a temperature of no more than 200° C.; or
sulfiding.

### Claim 44 (depends on 29)

The method of claim 29, wherein the Ti-containing precursor is an organotitanium precursor.

### Claim 45 (depends on 44)

The method of claim 44, wherein the organotitanium precursor comprises a titanium alkoxide.

### Claim 46 (depends on 36)

The method of claim 36, wherein the Ti-containing precursor is an organotitanium precursor.

### Claim 47 (depends on 46)

The method of claim 46, wherein the organotitanium precursor comprises a titanium alkoxide.

### Claim 48 (depends on 36)

The method of claim 36, wherein the organic compound-based component is selected from the group consisting of an organic acid or salt thereof, a sugar, a sugar alcohol, and a combination thereof.

### Claim 49 (depends on 36)

The method of claim 36, wherein the organic compound-based component is selected from the group consisting of glyoxylic acid, pyruvic acid, lactic acid, malonic acid, oxaloacetic acid, malic acid, fumaric acid, maleic acid, tartaric acid, gluconic acid, citric acid, oxamic acid, serine, aspartic acid, glutamic acid, iminodiacetic acid, ethylenediaminetetraacetic acid, fructose, glucose, galactose, mannose, sucrose, lactose, maltose, erythritol, xylitol, mannitol, sorbitol, and a combination thereof.

### Claim 50

A method for preparing a bulk catalyst precursor having a formula of
Av[Ni(OH)x(L)py]z[MomW1-mO4][Ti(OH)nO2-n/2]w
wherein:
(i) A is an alkali metal cation, a rare earth metal cation, an ammonium cation, an organic ammonium cation, phosphonium cation, or a combination thereof;
(ii) L is an organic compound-based component; and
(iii) 0≤y≤−2/p; 0≤x<2; 0≤v<2; 0<z; 0<m<1; 0<<4; 0.1<w/(z+1)<10;
the method comprising:
(a) combining in a reaction mixture;
(i) a Ni-containing precursor;
(ii) a Mo-containing precursor;
(iii) a W-containing precursor;
(iv) a Ti-containing precursor;
(v) an organic compound-based component; and
(vi) a protic liquid; and
(b) reacting the mixture under conditions sufficient to cause precipitation of the bulk catalyst precursor;
with the steps to prepare the bulk catalyst precursor carried out at a temperature of no more than 200° C.; and
recovering a bulk catalyst precursor is defined by a region of a quaternary phase diagram defined by eight points ABCDEFGH and wherein the eight points, on a metal oxide basis (wt. %), are: A (Ni=52.5, Mo=3.5, W=14, Ti=30), B (Ni=38.5, Mo=17.5, W=14, Ti=30), C (Ni=21, Mo=17.5, W=31.5, Ti=30), D (Ni=35, Mo=3.5, W=31.5, Ti=30), E (Ni=60, Mo=4, W=16, Ti=20), F (Ni=44, Mo=20, W=16, Ti=20), G (Ni=24, Mo=20, W=36, Ti=20), and H (Ni=40, Mo=4, W=36, Ti=20).

### Claim 51 (depends on 50)

The method of claim 50, wherein the reaction mixture is prepared by:
preparing a first mixture comprising a Ni-containing precursor, a protic liquid, and, optionally, an organic compound-based component;
preparing a second mixture comprising a Mo-containing precursor, a W-containing precursor, and a protic liquid;
adding a Ti-containing precursor to the first mixture, the second mixture, or a combination thereof;
heating both the first and second mixtures to a temperature of from 60° C. to 150° C.;
combining the first and second mixtures together.

### Claim 52 (depends on 51)

The method of claim 51, wherein the Ti-containing precursor is selected from TiO2 nanoparticles, colloidal TiO2, fumed TiO2, titanium hydroxide, organotitanium compounds, titanium halides, organotitanium halides, water-soluble titanium salts, or a combination thereof.

### Claim 53 (depends on 50)

The method of claim 50, wherein the reacting is carried out at one or more temperatures either (a) in a range of 60° C. to 100° C. under atmospheric pressure or (b) above 100° C. under autogenous pressure.

### Claim 54 (depends on 50)

The method of claim 50, wherein the organic compound-based component is selected from an organic acid or salt thereof, a sugar, a sugar alcohol, or a combination thereof.

### Claim 55 (depends on 50)

The method of claim 50, wherein the organic compound-based component is selected from glyoxylic acid, pyruvic acid, lactic acid, malonic acid, oxaloacetic acid, malic acid, fumaric acid, maleic acid, tartaric acid, gluconic acid, citric acid, oxamic acid, serine, aspartic acid, glutamic acid, iminodiacetic acid, ethylenediaminetetraacetic acid, fructose, glucose, galactose, mannose, sucrose, lactose, maltose, erythritol, xylitol, mannitol, sorbitol, or a combination thereof.

### Claim 56 (depends on 50)

The method of claim 50, further comprising one or more of the following steps:
compositing the bulk catalyst precursor with 0 to 40 wt. % with a material selected from the group of binder materials, conventional hydroprocessing catalysts, cracking compounds, or mixtures thereof;
spray-drying, (flash) drying, milling, kneading, slurry-mixing, dry or wet mixing, or combinations thereof;
shaping,
drying and/or thermally treating at a temperature of no more than 200° C.; or
sulfiding.

### Claim 57

A method for preparing a bulk catalyst precursor having a formula of
Av[Ni(OH)x(L)py]z[MomW1-mO4][Ti(OH)nO2-n/2]w
wherein:
(i) A is an alkali metal cation, a rare earth metal cation, an ammonium cation, an organic ammonium cation, phosphonium cation, or a combination thereof;
(ii) L is an organic compound-based component; and
(iii) 0≤y≤−2/p; 0≤x<2; 0≤v<2; 0<z; 0<m<1; 0<<4; 0.1<w/(z+1)<10;
the method comprising:
(a) combining in a reaction mixture;
(i) a Ni-containing precursor;
(ii) a Mo-containing precursor;
(iii) a W-containing precursor;
(iv) an organic compound-based component; and
(v) a protic liquid; and
(b) reacting the mixture under conditions sufficient to cause precipitation of an intermediate bulk catalyst precursor; and
(c) compositing the intermediate bulk catalyst precursor with a Ti-containing precursor to form the bulk catalyst precursor;
wherein the steps to prepare the bulk catalyst precursor are carried out at a temperature of no more than 200° C.; and
recovering a bulk catalyst precursor defined by a region of a quaternary phase diagram wherein the region is defined by ten points ABCDEFGHIJ and wherein the ten points, on a metal oxide basis (wt. %), are: A (Ni=39, Mo=1, W=41, Ti=20), B (Ni=39, Mo=1, W=72, Ti=20), C (Ni=9, Mo=17, W=54, Ti=20), D (Ni=31, Mo=25, W=24, Ti=20), E (Ni=40, Mo=14, W=26, Ti=20), F (Ni=34, Mo=1, W=36, Ti=30), G (Ni=7, Mo=1, W=63, Ti=30), H (Ni=8, Mo=15, W=48, Ti=30), I (Ni=27, Mo=22, W=21, Ti=30), and J (Ni=35, Mo=12, W=23, Ti=30).

### Claim 58 (depends on 57)

The method of claim 57, wherein the reaction mixture is prepared by:
preparing a first mixture comprising a Ni-containing precursor, a protic liquid, and, optionally, an organic compound-based component;
preparing a second mixture comprising a Mo-containing precursor, a W-containing precursor, and a protic liquid;
heating both the first and second mixtures to a temperature of from 60° C. to 150° C.; and
combining the first and second mixtures together.

### Claim 59 (depends on 57)

The method of claim 57, wherein the Ti-containing precursor is selected from TiO2 nanoparticles, fumed TiO2, or a combination thereof.

### Claim 60 (depends on 57)

The method of claim 57, wherein the intermediate bulk catalyst precursor is a Ni—Mo—W bulk catalyst precursor.

### Claim 61 (depends on 57)

The method of claim 57, wherein the reacting is carried out at one or more temperatures either (a) in a range of 60° C. to 100° C. under atmospheric pressure or (b) above 100° C. under autogenous pressure.

### Claim 62 (depends on 57)

The method of claim 57, wherein the organic compound-based component is selected from an organic acid or salt thereof, a sugar, a sugar alcohol, or a combination thereof.

### Claim 63 (depends on 62)

The method of claim 62, wherein the organic compound-based component is selected from glyoxylic acid, pyruvic acid, lactic acid, malonic acid, oxaloacetic acid, malic acid, fumaric acid, maleic acid, tartaric acid, gluconic acid, citric acid, oxamic acid, serine, aspartic acid, glutamic acid, iminodiacetic acid, ethylenediaminetetraacetic acid, fructose, glucose, galactose, mannose, sucrose, lactose, maltose, erythritol, xylitol, mannitol, sorbitol, or a combination thereof.

### Claim 64 (depends on 57)

The method of claim 57, further comprising one or more of the following steps:
compositing the bulk catalyst precursor with 0 to 40 wt. % with a material selected from the group of binder materials, conventional hydroprocessing catalysts, cracking compounds, or mixtures thereof;
spray-drying, (flash) drying, milling, kneading, slurry-mixing, dry or wet mixing, or combinations thereof;
shaping,
drying and/or thermally treating at a temperature of no more than 200° C.; or
sulfiding.

### Claim 65 (depends on 50)

The method of claim 50, wherein the Ti-containing precursor is an organotitanium precursor.

### Claim 66 (depends on 65)

The method of claim 65, wherein the organotitanium precursor comprises a titanium alkoxide.

### Claim 67 (depends on 57)

The method of claim 57, wherein the Ti-containing precursor is an organotitanium precursor.

### Claim 68 (depends on 67)

The method of claim 67, wherein the organotitanium precursor comprises a titanium alkoxide.