# US 2024/0188422 A1 · Rapid fabrication of semiconductor thin films

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0188422 A1
- Document ID: US20240188422A1
- Status: Published application
- Kind: A1
- Application number: 18/562,679
- Filed: 2022-05-26
- Published: 2024-06-06
- Earliest claimed: 2021-05-26
- Assignees: Massachusetts Institute of Technology
- Applicants: Massachusetts Institute of Technology
- Inventors: Vladimir Bulovic; Richard Swartwout
- Web page: https://patentgrep.com/patent/US20240188422A1

## CPC

- H10K 71/15: characterised by the solvent used
- C07F 19/005: {without metal-C linkages}
- C09D 11/033: characterised by the solvent
- C09D 11/037: characterised by the pigment
- C09D 11/52: Electrically conductive inks
- H10K 30/50: Photovoltaic [PV] devices
- H10K 71/40: Thermal treatment, e.g. annealing in the presence of a solvent vapour
- H10K 85/50: Organic perovskites; Hybrid organic-inorganic perovskites [HOIP], e.g. CH3NH3PbI3
- Y02E 10/549: Organic PV cells
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- C07F: ACYCLIC, CARBOCYCLIC OR HETEROCYCLIC COMPOUNDS CONTAINING ELEMENTS OTHER THAN CARBON, HYDROGEN, HALOGEN, OXYGEN, NITROGEN, SULFUR, SELENIUM OR TELLURIUM (metal-containing porphyrins C07D487/22)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Semiconductor thin films and rapid methods of fabrication can include mixed cations created through recrystalization.

## Claims

### Claim 1

A method of fabricating a semiconductor thin film comprising:
depositing a perovskite precursor in a first solvent on a substrate, the precursor forming a first perovskite layer on a surface of the substrate;
applying a recrystallization additive in a second solvent to the layer on the surface of the substrate to form a second layer on the substrate; and
annealing the first layer and the second layer to exchange a cation of the recrystallization additive with a cation of the perovskite precursor to form a perovskite alloy film and a volatile byproduct.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first perovskite layer is a 2D perovskite layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the perovskite precursor includes an alkyl ammonium lead halide.

### Claim 4 (depends on 3)

The method of claim 3, wherein the halide is a chloride, a bromide or an iodide.

### Claim 5 (depends on 1)

The method of claim 1, wherein the perovskite precursor includes a methylammonium lead iodide.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first solvent includes tetrahydrofuran, 2-methyltetrahydrofuran, a glycol ether, acetonitrile, methanol, ethanol, propanol, butanol, tris(dimethylamino)silane, bis(dimethylamino)dimethylsilane, hexamethyldisilazane, hexamethylphosphoramide (HMPA), dimethylformamide, dimethylsulfoxide, propylene carbonate, gamma butyrolactone, 1,3-dimethyl-2-imidazolidinone, N,N′-dimethylpropyleneurea, N-butylpyrrolidinone, or combinations thereof.

### Claim 7 (depends on 1)

The method of claim 1, wherein the second solvent includes isopropanol, butanol, or a glycol ether.

### Claim 8 (depends on 7)

The method of claim 7, wherein the glycol ether is propylene glycol propyl ether, propylene glycol methyl ether, propylene glycol butyl ether, ethylene glycol propyl ether, ethylene glycol methyl ether, ethylene glycol butyl ether, or combinations thereof

### Claim 9 (depends on 1)

The method of claim 1, wherein the recrystallization additive includes a formate salt, an acetate salt, or combinations thereof.

### Claim 10 (depends on 1)

The method of claim 1, wherein the recrystallization additive includes a formamidinium formate, formamidinium acetate, cesium formate, cesium acetate, strontium formate, strontium acetate, ytterbium formate, ytterbium acetate, cerium formate, cerium acetate, germanium formate, germanium acetate, or combinations thereof.

### Claim 11 (depends on 1)

The method of claim 1, wherein the perovskite alloy film includes a material having the formula (I)
(A:A′)(Pb:B′)X3 (I)
where A is an organic cation, A′ is an organic or an inorganic cation different from A′, B′ is a divalent metal cation or missing, and X is a halide ion.

### Claim 12 (depends on 11)

The method of claim 11, wherein A′ is cesium or formamidimium.

### Claim 13 (depends on 11)

The method of claim 11, wherein a ratio of A:A′ is tuned based on a cation content of the perovskite precursor and a cation content of the recrystallization additive.

### Claim 14 (depends on 11)

The method of claim 11, wherein the volatile byproduct includes an ammonium acetate or an ammonium formate.

### Claim 15 (depends on 14)

The method of claim 14, wherein the ammonium is methylammonium.

### Claim 16 (depends on 11)

The method of claim 11, wherein depositing includes spin-coating, ink-jet printing, roll-to-roll printing, slot die coating, blade coating, or spray coating.

### Claim 17 (depends on 11)

The method of any one of claim 11, wherein applying includes spin-coating, ink-jet printing, roll-to-roll printing, slot die coating, blade coating, or spray coating.

### Claim 18 (depends on 11)

The method of claim 11, wherein annealing includes applying heat at an annealing temperature for an annealing time.

### Claim 19 (depends on 18)

The method of claim 18, wherein the annealing temperature is between 30° C. and 200° C.

### Claim 20 (depends on 18)

The method of claim 18, wherein the annealing time is between 20 seconds and 60 minutes.

### Claim 21 (depends on 1)

The method of claim 1, wherein the time between the applying and the annealing is less than 60 minutes.

### Claim 22 (depends on 1)

The method of claim 1, further comprising treating the layer with an annealing ink including an alkylammonium chloride in a third solvent that is not a solvent for the semiconductor film.

### Claim 23 (depends on 22)

The method of claim 22, wherein the alkylammonium chloride includes methylammonium chloride.

### Claim 24 (depends on 22)

The ink formulation of claim 22, wherein the third solvent includes propylene glycol methyl ether.

### Claim 25 (depends on 22)

The ink formulation of claim 22, wherein the first solvent includes tetrahydrofuran.

### Claim 26 (depends on 22)

The ink formulation of claim 22, wherein the second solvent includes an alcohol.

### Claim 27

A semiconductor film comprising a perovskite alloy including a material having the formula (I)
(A:A′)(Pb:B′)X3 (I)
where A is an organic cation, A′ is an organic or an inorganic cation different from A, B′ is a divalent metal cation or missing, and X is a halide ion.

### Claim 28 (depends on 27)

The semiconductor film of claim 27, wherein A′ is cesium or formamidimium.

### Claim 29 (depends on 27)

The semiconductor film of claim 27, wherein grains of the perovskite alloy are substantially oriented to [100] rather than [010].

### Claim 30 (depends on 27)

The semiconductor film of claim 27, wherein the grains are greater than one micron.

### Claim 31 (depends on 28)

The semiconductor film of claim 28, wherein an x-ray diffraction peak is shifted approximated 0.025 degrees from a predicted x-ray diffraction peak.

### Claim 32

A photovoltaic device comprising:
a first electrode;
a second electrode; and
a perovskite layer between the first electrode and the second electrode,
wherein the perovskite layer includes a perovskite alloy including a material having the formula (I)
(A:A′)(Pb:B′)X3 (I)
where A is an organic cation, A′ is an organic or an inorganic cation different from A, B′ is a divalent metal cation or missing, and X is a halide ion.

### Claim 33 (depends on 32)

The device of claim 32, wherein the device has a power conversion efficiency of over 15%.

### Claim 34

An ink formulation system for producing a semiconductor film comprising:
a first ink including a perovskite precursor in a first solvent; and
a second ink including a recrystallization additive in a second solvent.

### Claim 35 (depends on 34)

The ink formulation of claim 34, further comprising an annealing ink including an alkylammonium chloride in a third solvent that is not a solvent for the semiconductor film.

### Claim 36 (depends on 34)

The ink formulation of claim 34, wherein the alkylammonium chloride includes methylammonium chloride.

### Claim 37 (depends on 35)

The ink formulation of claim 35, wherein the third solvent includes propylene glycol methyl ether.

### Claim 38 (depends on 34)

The ink formulation of claim 34, wherein the first solvent includes tetrahydrofuran.

### Claim 39 (depends on 34)

The ink formulation of claim 34, wherein the second solvent includes an alcohol.