# US 2024/0188261 A1 · METHOD OF PRODUCING LARGE EMI SHIELDED GaAs INFRARED WINDOWS

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0188261 A1
- Document ID: US20240188261A1
- Status: Published application
- Kind: A1
- Application number: 18/073,179
- Filed: 2022-12-01
- Published: 2024-06-06
- Earliest claimed: 2022-12-01
- Assignees: BAE Systems Information and Electronic Systems Integration Inc.
- Applicants: BAE SYSTEMS Information and Electronic Systems Integration Inc.
- Inventors: Peter G. Schunemann; Kevin T. Zawilski
- Web page: https://patentgrep.com/patent/US20240188261A1

## CPC

- H05K 9/0005: {Shielded windows}
- C09D 5/006: {Anti-reflective coatings}
- C23C 16/301: {AIII BV compounds, where A is Al, Ga, In or Tl and B is N, P, As, Sb or Bi}
- C23C 16/306: {AII BVI compounds, where A is Zn, Cd or Hg and B is S, Se or Te}
- C23C 16/52: Controlling or regulating the coating process {(C23C16/45557, C23C16/279 take precedence)}
- C30B 11/00: Single-crystal growth by normal freezing or freezing under temperature gradient, e.g. Bridgman-Stockbarger method (C30B13/00, C30B15/00, C30B17/00, C30B19/00 take precedence; under a protective fluid C30B27/00)
- C30B 17/00: Single-crystal growth onto a seed which remains in the melt during growth, e.g. Nacken-Kyropoulos method (C30B15/00 takes precedence)
- C30B 29/42: Gallium arsenide
- C30B 29/602: {Nanotubes}
- C30B 35/002: {Crucibles or containers}
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

GaAs IR window slabs having largest dimensions that are greater than 8 inches, and preferably greater than 12 inches, are grown using the Horizontal Gradient Freeze (HGF) method. Heat extraction is simplified by using a shallow horizontal boat that is only slightly deeper than the desired window thickness, thereby enabling growth of large slabs while also minimizing material waste and fabrication cost as compared to slicing and shaping thick plates from large, melt-grown boules. Single crystal seeds can be used to optimize the final orientation of the slabs and minimize secondary nucleation, thereby maximizing yield. A conductive doped GaAs layer can be applied to the IR window slab to provide EMI shielding. The temperature gradient during HGF can be between 1° C./cm and 3° C./cm, and the directional solidification can be at a rate of between 0.25 mm/h and 2.5 mm/h.

## Claims

### Claim 1

A method of producing a GaAs slab having a largest dimension that is greater than eight inches, the slab being suitable for forming an infrared (IR) transparent window having a largest dimension that is greater than eight inches, the method comprising:
providing a boat having a seed crystal region in contact with a crystal growing region, the crystal growing region having a largest dimension that is greater than eight inches;
placing a single crystal of GaAs as a seed crystal in the seed crystal region of the boat;
placing a polycrystalline charge of GaAs in the crystal growing region;
placing the boat within an interior of a horizontal furnace, at least two heating elements of the horizontal furnace being configured to separately control temperatures of the seed crystal region and the crystal growing region;
causing the heating elements to establish and maintain a horizontal temperature gradient across the interior of the furnace, said temperature gradient causing the seed crystal to be lower in temperature than the polycrystalline charge;
heating the interior of the furnace while maintaining said temperature gradient until the polycrystalline charge and a first portion of the seed crystal in contact with the polycrystalline charge are melted, a second portion of the seed crystal remaining solid, a solid/liquid interface being formed between the first and second portions of the seed crystal;
gradually cooling the interior of the furnace while maintaining the horizontal temperature gradient within the interior, so that the solid/liquid interface moves continuously across the crystal growing region, thereby causing directional solidification of the GaAs whereby the solidifying GaAs at the solid/liquid interface attaches to and extends the seed crystal;
removing the boat from the furnace;
removing the grown crystal from the crystal growing region of the boat; and
forming the GaAs IR window slab from the grown crystal.

### Claim 2 (depends on 1)

The method of claim 1, wherein the crystal growing region has a largest dimension of at least 12 inches.

### Claim 3 (depends on 1)

The method of claim 1, wherein the growing region of the boat is substantially rectangular.

### Claim 4 (depends on 1)

The method of claim 1, wherein a size and shape of the crystal growing region approximate a desired size and shape of the GaAs slab.

### Claim 5 (depends on 1)

The method of claim 1, wherein the temperature gradient is between 1° C./cm and 3° C./cm.

### Claim 6 (depends on 1)

The method of claim 1, wherein the boat is a pyrolytic boron nitride (PBN) boat.

### Claim 7 (depends on 1)

The method of claim 1, wherein the directional solidification is at a rate of between 0.25 mm/h and 2.5 mm/h.

### Claim 8 (depends on 1)

The method of claim 1, further comprising encapsulating the boat in an ampoule before placing the boat within an interior of the horizontal furnace.

### Claim 9 (depends on 1)

The method of claim 1, further comprising applying a conductive doped GaAs layer to the IR window slab.

### Claim 10 (depends on 9)

The method of claim 9, wherein the conductive doped GaAs layer is applied to the IR window slab by a vacuum deposition process.

### Claim 11 (depends on 10)

The method of claim 10, wherein the vacuum deposition process is LP-HVPE.

### Claim 12 (depends on 1)

The method of claim 1, further comprising maintaining an arsenic or inert gas over-pressure over the boat while the furnace interior is heated and cooled.

### Claim 13

Apparatus for growing a GaAs slab having a largest dimension that is greater than eight inches, the slab being suitable for forming an infrared (IR) transparent window having a largest dimension that is greater than eight inches, the apparatus comprising:
a boat having a seed crystal region in contact with a crystal growing region, the crystal growing region having a largest dimension that is greater than eight inches;
a horizontal furnace having a furnace interior configured to receive and surround the boat while the boat is oriented horizontally;
at least two heating elements configured to separately control temperatures of the seed crystal region and the crystal growing region;
a plurality of temperature sensors providing temperature measurements at a plurality of locations within the furnace; and
a controller in electrical communication with the heating elements and with the temperature sensors, the controller being configured to cause the heating elements to heat and then to cool the interior of the furnace, while establishing and maintaining a horizontal temperature gradient across the interior of the furnace, such that a temperature of the crystal growing region of the boat within the interior of the furnace is caused to be always higher than a temperature of the seed crystal region throughout the heating and cooling.

### Claim 14 (depends on 13)

The apparatus of claim 13, wherein the crystal growing region has a largest dimension of at least 12 inches.

### Claim 15 (depends on 13)

The apparatus of claim 13, wherein the growing region of the boat is substantially rectangular.

### Claim 16 (depends on 13)

The apparatus of claim 13, wherein a size and shape of the crystal growing region approximate a desired size and shape of the GaAs slab.

### Claim 17 (depends on 13)

The apparatus of claim 13, wherein the boat is a pyrolytic boron nitride (PBN) boat.

### Claim 18 (depends on 13)

The apparatus of claim 13, further comprising an ampoule configured to receive and contain the boat.

### Claim 19

An infrared window comprising a GaAs slab having a slab largest dimension that is greater than eight inches, said slab being formed by:
placing a seed crystal in a seed crystal region of a boat, said seed crystal region being in contact with a crystal growing region of the boat, the crystal growing region having a largest dimension that is greater than eight inches;
placing a polycrystalline charge of GaAs in the crystal growing region;
heating the boat while maintaining a horizontal temperature gradient across the boat, whereby the seed crystal region is maintained at a lower temperature than the crystal growing region, the polycrystalline charge and a first portion of the seed crystal in contact with the polycrystalline charge being thereby melted while a second portion of the seed crystal remains solid; and
gradually cooling the boat while maintaining the horizontal temperature gradient, so that a solid/liquid interface of the polycrystalline charge moves continuously across the crystal growing region, thereby causing directional solidification of the GaAs whereby the solidifying GaAs at the solid/liquid interface attaches to and extends the seed crystal.

### Claim 20 (depends on 19)

The infrared window of claim 19, wherein the slab largest dimension is greater than twelve inches.

### Claim 21 (depends on 19)

The infrared window of claim 19, further comprising an electrically conductive layer of doped GaAs applied to the slab.

### Claim 22 (depends on 19)

The infrared window of claim 19, further comprising an anti-reflective coating applied to the slab.