# US 2024/0186527 A1 · Copper foil, electrode comprising the same, secondary battery comprising the same, and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0186527 A1
- Document ID: US20240186527A1
- Status: Published application
- Kind: A1
- Application number: 18/529,381
- Filed: 2023-12-05
- Published: 2024-06-06
- Earliest claimed: 2022-12-06
- Assignees: SK Nexilis Co., Ltd.
- Applicants: SK Nexilis Co., Ltd.
- Inventors: Shan Hua JIN; Min Seok YOON
- Web page: https://patentgrep.com/patent/US20240186527A1

## CPC

- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 4/75: Wires, rods or strips
- C25D 3/38: of copper
- C25D 5/04: Electroplating with moving electrodes
- C25D 7/0614: {Strips or foils}
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

According to one embodiment of the present disclosure, there is provided a copper foil including a copper film having 99.9 wt % or more of copper, wherein the copper foil has a color difference coefficient in a range of 0.38 to 0.7 based on the Lab color system.

## Claims

### Claim 1

A copper foil comprising a copper film including 99.9 wt % or more of copper,
wherein the copper foil has a color difference coefficient in a range of 0.38 to 0.7 based on the Lab color system,
wherein the color difference coefficient is calculated by Equation 1 below,
Color difference coefficient=|color difference E″ after stretching−color difference E′ before stretching| [Equation 1]
wherein the color difference (E′) before stretching of Equation 1 is calculated by Equation 2 below,
color difference (E′) before stretching=[(L*1)2+(a*1)2+(b*1)2]1/2 [Equation 2]
wherein L*1 in Equation 2 refers to L*1 before stretching,
a*1 in Equation 2 refers to a* before stretching, and
b*1 in Equation 2 refers to b* before stretching, and
the color difference (E″) after stretching of Equation 1 is calculated by Equation 3 below,
color difference (E″) after stretching=[(L*2)2+(a*2)2+b*2)2]1/2 [Equation 3]
wherein L*2 in Equation 3 refers to L*1 after stretching,
a*2 in Equation 3 refers to a* after stretching, and
b*2 in in Equation 3 refers to b* after stretching.

### Claim 2 (depends on 1)

The copper foil of claim 1, wherein the color difference (E′) before stretching is in a range of 80 to 85.

### Claim 3 (depends on 1)

The copper foil of claim 1, wherein the color difference (E″) after stretching is in a range of 80 to 85.

### Claim 4 (depends on 1)

The copper foil of claim 1, wherein the copper foil has a high-temperature elongation of 2% to 20%, wherein the high-temperature elongation is an elongation measured after heat treatment at 190° C. for one hour.

### Claim 5 (depends on 1)

The copper foil of claim 1, wherein the copper foil has an arithmetic mean roughness (Ra) of 0.1 μm to 0.3 μm.

### Claim 6 (depends on 1)

The copper foil of claim 1, further comprising a protective layer formed on the copper film.

### Claim 7 (depends on 6)

The copper foil of claim 6, wherein the protective layer includes at least one of a chromium compound, a silane compound, and a nitrogen compound.