# US 2024/0186493 A1 · Manufacturing of an electrode laminate with a treated carrier foil

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0186493 A1
- Document ID: US20240186493A1
- Status: Published application
- Kind: A1
- Application number: 18/527,059
- Filed: 2023-12-01
- Published: 2024-06-06
- Earliest claimed: 2022-12-01
- Assignees: Solid Power Operating, Inc.
- Applicants: Solid Power Operating, Inc.
- Inventors: Brandon KELLY; Uday KASAVAJJULA; A. YANG
- Web page: https://patentgrep.com/patent/US20240186493A1

## CPC

- H01M 4/366: {as layered products}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/043: {involving compressing or compaction}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 10/052: Li-accumulators
- H01M 10/0562: Solid materials
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Aspects of the present disclosure involve utilizing layers, such as an outer carrier foil layer, that provide a surface energy sufficient to prevent separation of the layers of the stack during lamination while allowing for the proper densification of the solid-electrolyte separator layer. In one particular example, a Corona-treated or carbon coated outer foil layer may be used during manufacturing of the electrode stack that provides a sufficient surface energy to adhere to the solid-electrolyte separator layer during the lamination process, while allowing for subsequent peeling of the Corona-treated outer foil from the electrode stack after densification without damaging the remaining layers of the stack. The electrode laminate discussed herein may be utilized in any type of battery or electrochemical cell, including solid, semi-solid, or liquid-based batteries.

## Claims

### Claim 1

A method for manufacturing a battery electrode, the method comprising:
casting a solid-state electrolyte (SSE) layer onto a treated carrier foil, the treated carrier foil comprising a surface energy adhering the SSE layer to the treated carrier foil;
layering a conductive layer adjacent to the first SSE layer to form an electrode stack; and
densifying the SSE layer by applying a densifying pressure to the SSE layer, wherein the surface energy retains the adherence of the SSE layer to the treated carrier foil following the densifying of the electrode stack.

### Claim 2 (depends on 1)

The method of claim 1, wherein the treated carrier foil comprises a Corona treatment, the Corona treatment generating the surface energy of the treated carrier foil.

### Claim 3 (depends on 1)

The method of claim 1, wherein the treated carrier foil comprises a carbon-coating treatment, the carbon-coating treatment generating the surface energy of the treated carrier foil.

### Claim 4 (depends on 1)

The method of claim 1, wherein the conductive layer comprises a silicon anode layer adjacent the SSE layer on a surface opposite the treated carrier foil.

### Claim 5 (depends on 1)

The method of claim 1, wherein the conductive layer comprises a lithium foil layer.

### Claim 6 (depends on 1)

The method of claim 1 further comprising:
casting a second SSE layer onto a second treated carrier foil; and
layering the second SSE layer adjacent to the conductive layer on an opposite side of the SSE layer to form the electrode stack.

### Claim 7 (depends on 6)

The method of claim 6, wherein the conductive layer comprises a first silicon anode layer, an electrically conductive layer, and a second silicon anode layer adjacent the electrically conductive layer opposite the first silicon anode layer.

### Claim 8 (depends on 1)

The method of claim 1, wherein densifying the SSE layer comprises passing the electrode stack through a pressing device at the densifying pressure laminates the SSE layer to the conductive layer.

### Claim 9 (depends on 8)

The method of claim 8, wherein the pressing device is a calender press comprising a first roller and a second roller, the first roller oriented above the second roller and separated by a pressing gap corresponding to the densifying pressure.

### Claim 10 (depends on 1)

The method of claim 1, wherein densifying the SSE layer lowers a first adhesion property between the SSE layer and the carrier foil and increases a second adhesion property between the SSE layer and the conductive layer.

### Claim 11 (depends on 10)

The method of claim 10, wherein the surface energy of the treated carrier foil is less than the adhesion property between the SSE layer and the conductive layer to provide for removing, using a peeling device, the treated carrier foil from the SSE layer as the SSE layer remains adhered to the conductive layer via the second adhesion property.

### Claim 12

A method for a laminated electrode, the method comprising:
layering a first side of a solid-state electrolyte (SSE) layer adjacent to a conductive electrode as an electrode stack, wherein the SSE layer is cast onto a carrier foil on a second side opposite the first side;
laminating the SSE layer to the conductive electrode by applying a laminating pressure to the electrode stack;
removing the carrier foil from the second side of the SSE layer;
layering the second side of the SSE layer with a treated carrier foil comprising a surface energy for adhering the SSE layer to the treated carrier foil; and
densifying the SSE layer by applying a densifying pressure to the electrode stack, wherein the densifying pressure is greater than the laminating pressure.

### Claim 13 (depends on 12)

The method of claim 12 further comprising:
removing the treated carrier foil from the second side of the SSE layer after densifying the SSE layer.

### Claim 14 (depends on 12)

The method of claim 12, wherein the treated carrier foil layer comprises a Corona treatment on a surface of the foil adjacent to the SSE layer.

### Claim 15 (depends on 12)

The method of claim 12, wherein the treated carrier foil comprises a carbon-coating treatment on a of the foil adjacent to the SSE layer.

### Claim 16

A solid-state electrochemical cell comprising;
a solid-state electrolyte (SSE) layer the first electrode;
a treated carrier foil cast onto the SSE layer, the treated carrier foil comprising a surface energy for adhering to the SSE layer; and
a conductive layer adjacent the SSE layer to form an electrode stack.

### Claim 17 (depends on 16)

The solid-state electrochemical cell of claim 16, wherein the treated carrier foil comprises a Corona treatment, the Corona treatment generating the surface energy of the treated carrier foil.

### Claim 18 (depends on 16)

The solid-state electrochemical cell of claim 16, wherein the treated carrier foil comprises a carbon-coating treatment, the carbon-coating treatment generating the surface energy of the treated carrier foil.

### Claim 19 (depends on 16)

The solid-state electrochemical cell of claim 16, wherein the conductive layer comprises a silicon anode layer adjacent the SSE layer on a surface opposite the treated carrier foil.

### Claim 20 (depends on 16)

The solid-state electrochemical cell of claim 16, wherein the conductive layer comprises a lithium foil layer.

### Claim 21 (depends on 16)

The solid-state electrochemical cell of claim 16 wherein the surface energy is greater than 25 dyne/cm and a surface roughness of the treated carrier foil is less than 1 um.

### Claim 22

A method for manufacturing a battery electrode, the method comprising:
coating an electrode layer onto a carrier foil;
layering a treated carrier foil on the coated electrode layer, the treated carrier foil comprising a surface energy to adhere to the electrode layer; and
densifying the layered electrode layer by applying a densifying pressure to the layered electrode layer, wherein the surface energy retains the adherence of the electrode layer to the treated carrier foil following the densifying of the layered electrode layer.

### Claim 23 (depends on 21)

The method of manufacturing a battery electrode of claim 21 wherein the surface energy is greater than 25 dyne/cm.

### Claim 24 (depends on 21)

The method of manufacturing a battery electrode of claim 21 wherein the treated carrier foil has a surface roughness of less than 1 um.