# US 2024/0183082 A1 · Method for manufacturing elastic fiber and elastic fiber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0183082 A1
- Document ID: US20240183082A1
- Status: Published application
- Kind: A1
- Application number: 18/384,557
- Filed: 2023-10-27
- Published: 2024-06-06
- Earliest claimed: 2022-12-06
- Assignees: San Fang Chemical Industry Co., Ltd.
- Applicants: San Fang Chemical Industry Co., Ltd.
- Inventors: CHIH-YI LIN; KUO-KUANG CHENG; LI-YUAN CHEN; CHI-WEI CHANG; CHIA-CHUN YANG
- Web page: https://patentgrep.com/patent/US20240183082A1

## CPC

- D01D 5/088: Cooling filaments, threads or the like, leaving the spinnerettes
- D01D 5/16: using rollers, or like mechanical devices, e.g. snubbing pins
- D01D 5/24: with a hollow structure; Spinnerette packs therefor (D01D5/38 takes precedence; producing tubes of plastic material B29D; addition of agents forming hollow filaments D01F1/08)
- D01D 7/00: Collecting the newly-spun products ({D01D5/0076 takes precedence;} collecting newly-spun products with the imparting of twist D01H)
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS

## Abstract

A method for manufacturing an elastic fiber and the elastic fiber are provided. The method includes: providing a thermoplastic polyester elastomer; drying the thermoplastic polyester elastomer; melting the thermoplastic polyester elastomer by an extruder to form a melt; extruding the melt by a spinneret plate to form a plurality of filamentous streams; feeding the filamentous streams into a spinning channel for cooling and curing to form a plurality of monofilaments; and bundling and oiling the monofilaments by an oil wheel, after extending and guiding the monofilaments by a first godet roller and a second godet roller, and winding the monofilaments by a winder to obtain a thermoplastic polyester elastic fiber.

## Claims

### Claim 1

A method for manufacturing an elastic fiber, comprising:
providing a thermoplastic polyester elastomer;
drying the thermoplastic polyester elastomer;
melting the thermoplastic polyester elastomer by an extruder to form a melt;
extruding the melt by a spinneret plate to form a plurality of filamentous streams;
feeding the filamentous streams into a spinning channel for cooling and curing to form a plurality of monofilaments; and
bundling and oiling the monofilaments by an oil wheel, after extending and guiding the monofilaments by a first godet roller and a second godet roller, and winding the monofilaments by a winder to obtain a thermoplastic polyester elastic fiber.

### Claim 2 (depends on 1)

The method of claim 1, wherein the thermoplastic polyester elastomer contains a linear block copolymer of polybutylene terephthalate and polyester or polyether.

### Claim 3 (depends on 1)

The method of claim 1, wherein a Shore hardness of the thermoplastic polyester elastomer is 20 D to 60 D.

### Claim 4 (depends on 1)

The method of claim 1, wherein a temperature of the extruder is 200° ° C. to 230° C., and a speed of the winder is 600 to 1,500 M/min.

### Claim 5 (depends on 1)

The method of claim 1, wherein a temperature of the first godet roller is 30 to 50° C., a speed of the first godet roller is 600 to 1,500 M/min, a temperature of the second godet roller is 30 to 50° C., and a speed of the second godet roller is 600 to 1,500 M/min.

### Claim 6 (depends on 1)

An elastic fiber, which is manufactured by the method according to claim 1 and includes a multifilament structure.

### Claim 7 (depends on 6)

The elastic fiber of claim 6, wherein a cross section of the multifilament structure is in a shape formed by stacking a plurality of perfect circles or non-perfect circles.

### Claim 8 (depends on 6)

The elastic fiber of claim 6, wherein the multifilament structure includes 6 to 48 monofilaments.

### Claim 9 (depends on 6)

The elastic fiber of claim 6, wherein the elastic fiber has a denier of 40 D to 500 D, a breaking strength of 0.8 to 1.5 g/D, an elongation at break of 360% to 900%, a permanent deformation value under 100% fixed elongation of 3 to 10 mm, and a permanent deformation value under 200% fixed elongation of 10 to 40 mm.