# US 2024/0183011 A1 · Method for producing grain-oriented electrical steel sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0183011 A1
- Document ID: US20240183011A1
- Status: Published application
- Kind: A1
- Application number: 18/284,109
- Filed: 2022-03-28
- Published: 2024-06-06
- Earliest claimed: 2021-03-31
- Assignees: Jfe Steel Corporation
- Applicants: JFE Steel Corporation
- Inventors: Ryosuke Tani; Takeshi Imamura; Shigehiro Takajo; Hiroi Yamaguchi
- Web page: https://patentgrep.com/patent/US20240183011A1

## CPC

- C22C 38/02: containing silicon
- C21D 1/76: Adjusting the composition of the atmosphere
- C21D 6/008: {containing Si}
- C21D 8/1222: {Hot rolling}
- C21D 8/1233: {Cold rolling}
- C21D 8/1255: {with diffusion of elements, e.g. decarburising, nitriding}
- C21D 8/1266: {between cold rolling steps}
- C21D 8/1272: {Final recrystallisation annealing}
- C21D 8/1277: involving a particular surface treatment (C21D8/1294 takes precedence)
- C21D 8/1283: {Application of a separating or insulating coating}
- C21D 9/46: for sheet metals
- C22C 38/04: containing manganese
- H01F 1/14783: {with insulating coating}
- H01F 1/18: with insulating coating
- C21D 8/1294: involving a localised treatment
- C21D 2201/05: Grain orientation
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/008: {containing tin}
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/22: with molybdenum or tungsten
- C22C 38/34: with more than 1.5% by weight of silicon
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- Y02P 10/20: Recycling
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for producing a grain-oriented electrical steel sheet comprises heating a steel material containing a certain composition to a temperature in a range of 1150 to 1250° C.; performing hot rolling, hot-band annealing, and cold rolling on the material to obtain a cold-rolled sheet with a final thickness; performing decarburization annealing also serving as primary recrystallization annealing on the cold-rolled sheet; subsequently applying an annealing separator to a surface of the steel sheet; and performing finishing annealing followed by applying an insulation coating. In the method, rapid heating is conducted from 500 and 700° C. in a heating process of the decarburization annealing at a rate of 100 to 1000° C./s while gradual heating is conducted from 800 to 900° C. in a heating process of the finishing annealing at a heating rate of 0.5 to 4.0° C./hr for at least 10 hours.

## Claims

### Claim 1

A method for producing a grain-oriented electrical steel sheet comprising
preparing a steel material having a component composition containing C: 0.002 to 0.10 mass %, Si: 2.0 to 8.0 mass %, and Mn: 0.005 to 1.0 mass % and further containing Al:
less than 0.010 mass %, N: less than 0.0050 mass %, Se: less than 0.0070 mass %, S: less than 0.0050 mass %, and a remaining part being Fe and inevitable impurities;
heating the steel material to a temperature in the range of 1150 to 1250° C.;
hot rolling the steel material to form a hot-rolled sheet;
subjecting the hot-rolled sheet to hot-band annealing and then to one cold rolling or two or more cold rollings with intermediate annealing between each rolling to form a cold-rolled sheet with a final sheet thickness;
subjecting the cold-rolled sheet to decarburization annealing serving as primary recrystallization annealing;
applying an annealing separator to the surface of the steel sheet; and
subjecting the steel sheet to finishing annealing followed by a formation of an insulation coating,
characterized in that
rapid heating is conducted from 500 to 700° C. in the heating process of the decarburization annealing at a rate of 100 to 1000° C./s while gradual heating is conducted from 800 to 900° C. in a heating process of the finishing annealing at a heating rate of 0.5 to 4.0° C./hr for at least 10 hours.

### Claim 2 (depends on 1)

The method for producing a grain-oriented electrical steel sheet according to claim 1, wherein
the steel material contains, in addition to the above component composition, at least one selected from the group consisting of: Ni: 0.01 to 1.50 mass %, Cr: 0.01 to 0.50 mass %, Cu: 0.005 to 1.000 mass %, P: 0.005 to 0.500 mass %, Sb: 0.005 to 0.500 mass %, Sn: 0.005 to 0.500 mass %, Bi: 0.005 to 0.500 mass %, Mo: 0.005 to 0.500 mass %, Nb: 0.0010 to 0.0100 mass %, Ta: 0.001 to 0.010 mass %, and Ti: 0.001 to 0.0100 mass %.

### Claim 3 (depends on 1)

The method for producing a grain-oriented electrical steel sheet according to claim 1, wherein
magnetic domain subdividing treatment is performed in any of the processes after the cold rolling by forming a groove on the surface of the steel sheet in a direction intersecting the rolling direction.

### Claim 4 (depends on 1)

The method for producing a grain-oriented electrical steel sheet according to claim 1, wherein
magnetic domain subdividing treatment is performed by irradiating an electron beam or a laser beam onto the surface of the steel sheet with the insulation coating formed thereon in a direction intersecting the rolling direction.

### Claim 5 (depends on 2)

The method for producing a grain-oriented electrical steel sheet according to claim 2, wherein
magnetic domain subdividing treatment is performed in any of the processes after the cold rolling by forming a groove on the surface of the steel sheet in a direction intersecting the rolling direction.

### Claim 6 (depends on 2)

The method for producing a grain-oriented electrical steel sheet according to claim 2, wherein
magnetic domain subdividing treatment is performed by irradiating an electron beam or a laser beam onto the surface of the steel sheet with the insulation coating formed thereon in a direction intersecting the rolling direction.