# US 2024/0182790 A1 · Method for preparing aromatic hydrocarbon-rich pyrolytic oil by catalytic pyrolysis of waste mask

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0182790 A1
- Document ID: US20240182790A1
- Status: Published application
- Kind: A1
- Application number: 18/214,777
- Filed: 2023-06-27
- Published: 2024-06-06
- Earliest claimed: 2022-12-06
- Assignees: Tianjin University
- Applicants: Tianjin University
- Inventors: Zhanjun Cheng; Hui Zhou; Beibei Yan; Guanyi Chen
- Web page: https://patentgrep.com/patent/US20240182790A1

## CPC

- C10G 1/00: Production of liquid hydrocarbon mixtures from oil-shale, oil-sand, or non-melting solid carbonaceous or similar materials, e.g. wood, coal (mechanical winning of oil from oil-shales, oil-sand, or the like B03B)
- B01J 29/405: {containing rare earth elements, titanium, zirconium, hafnium, zinc, cadmium, mercury, gallium, indium, thallium, tin or lead}
- B01J 29/46: Iron group metals or copper
- B01J 37/0201: {Impregnation}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/088: {Decomposition of a metal salt}
- B01J 2229/186: not in framework positions
- C10G 2300/1003: Waste materials
- C10G 2300/70: Catalyst aspects
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

Provided is a method for preparing an aromatic hydrocarbon-rich pyrolytic oil by catalytic pyrolysis of a waste mask, which relates to the technical field of waste treatment and resource utilization. The method includes: mixing the waste mask with a metal supported HZSM-5 molecular sieve catalyst to form a mixture; and subjecting the mixture to a catalytic pyrolysis reaction in a protective atmosphere to obtain the aromatic hydrocarbon-rich pyrolytic oil.

## Claims

### Claim 1

A method for preparing an aromatic hydrocarbon-rich pyrolytic oil by catalytic pyrolysis of a waste mask, comprising the steps of:
mixing the waste mask with a catalyst to form a mixture; and
subjecting the mixture to a catalytic pyrolysis reaction in a protective atmosphere to obtain the aromatic hydrocarbon-rich pyrolytic oil;
wherein the catalyst is a metal supported HZSM-5 molecular sieve catalyst.

### Claim 2 (depends on 1)

The method according to claim 1, wherein a metal in the metal supported HZSM-5 molecular sieve catalyst is one or more selected from the group consisting of gallium, zinc, nickel, iron and copper, and has a loading amount of 1-20 wt %.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the metal supported HZSM-5 molecular sieve catalyst is prepared by a process comprising
subjecting an HZSM-5 molecular sieve to impregnation in a metal salt solution to obtain an impregnated HZSM-5 molecular sieve; and
subjecting the impregnated HZSM-5 molecular sieve to drying and calcination sequentially to obtain the metal supported HZSM-5 molecular sieve catalyst.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the metal salt solution is prepared from a metal salt and water, wherein a solid-liquid ratio of the metal salt to water is in a range of (3-12) g: (150-250) mL, and the metal salt is one or more selected from the group consisting of gallium nitrate, zinc nitrate, nickel nitrate, iron nitrate and copper nitrate.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the impregnation is conducted at a temperature of 60-85° C. for 4-6 h.

### Claim 6 (depends on 3)

The method according to claim 3, wherein the drying is conducted at a temperature of 100-120° C. for 12-24 h.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the calcination is conducted at a temperature of 500-600° C. for 4-8 h.

### Claim 8 (depends on 1)

The method according to claim 1, wherein a mass ratio of the waste mask to the catalyst is in a range of 1:1 to 10:1.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the protective atmosphere is provided by nitrogen or argon, with a flow rate of 100-400 mL/min.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the catalytic pyrolysis reaction is conducted at a temperature of 500-700° C. for 5-30 min.

### Claim 11 (depends on 4)

The method according to claim 4, wherein the drying is conducted at a temperature of 100-120° C. for 12-24 h.

### Claim 12 (depends on 5)

The method according to claim 5, wherein the drying is conducted at a temperature of 100-120° C. for 12-24 h.

### Claim 13 (depends on 2)

The method according to claim 2, wherein a mass ratio of the waste mask to the catalyst is in a range of 1:1 to 10:1.

### Claim 14 (depends on 4)

The method according to claim 4, wherein a mass ratio of the waste mask to the catalyst is in a range of 1:1 to 10:1.

### Claim 15 (depends on 5)

The method according to claim 5, wherein a mass ratio of the waste mask to the catalyst is in a range of 1:1 to 10:1.

### Claim 16 (depends on 7)