# US 2024/0182774 A1 · Cement slurry compositions comprising pozzolanic cement additives and methods for improving development of compressive strengths in the cement slurry compositions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0182774 A1
- Document ID: US20240182774A1
- Status: Published application
- Kind: A1
- Application number: 18/073,650
- Filed: 2022-12-02
- Published: 2024-06-06
- Earliest claimed: 2022-12-02
- Assignees: Schlumberger Technology Corporation
- Applicants: Schlumberger Technology Corporation
- Inventors: Bernardo Engelke; Lynn Foster; Valerie Lafitte
- Web page: https://patentgrep.com/patent/US20240182774A1

## CPC

- C09K 8/467: containing additives for specific purposes
- C04B 14/045: {Alkali-metal containing silicates, e.g. petalite (waterglass C04B12/04)}
- C04B 14/047: {Zeolites}
- C04B 14/104: {Bentonite, e.g. montmorillonite}
- C04B 14/106: {Kaolin}
- C04B 14/22: Glass {; Devitrified glass}
- C04B 18/08: Flue dust {, i.e. fly ash}
- C04B 18/141: {Slags}
- C04B 18/248: {from specific plants, e.g. hemp fibres}
- C04B 28/04: Portland cements
- C09K 8/473: Density reducing additives, e.g. for obtaining foamed cement compositions
- E21B 33/14: for cementing casings into boreholes
- C04B 2111/00146: {Sprayable or pumpable mixtures}
- C04B 2201/20: for the density
- C04B 2201/50: for the mechanical strength
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

Pumpable slurry compositions comprising at least one aluminosilicate additive and optional pozzolanic cement additives and methods for improving development of compressive strengths in the pumpable cement slurry compositions are disclosed herein. The methods utilize one or more pumpable cement slurry compositions comprising at least one cement component, water, at least one first aluminosilicate additive, at least one optional second aluminosilicate additive, and one or more optional pozzolanic additives, wherein the at least one first aluminosilicate additive has an amorphous phase of greater than about 50% and a weight ratio of silica oxide to aluminum oxide of about 1.0 to about 2.5, and the at least one optional second aluminosilicate additive has a weight ratio of silica oxide to aluminum oxide of about 1.7 to about 3.3.

## Claims

### Claim 1

A pumpable cement slurry composition comprising:
at least one cement component comprising cement particles;
water;
a first aluminosilicate additive comprising metakaolin and having an amorphous phase of greater than 50%; and
a second aluminosilicate additive comprising rice husk ash,
wherein the first and second aluminosilicate additives are each present at a concentration of about 10% to about 15% by weight of the at least one cement component and comprise a weight ratio of silica to aluminum oxide (Si/Al weight ratio) of about 1.0 to about 2.5, and
wherein the pumpable cement slurry composition comprises a density of about 10 ppg to about 11.5 ppg and a solid volume fraction of less than about 40%.

### Claim at position 2

2-5. (canceled)

### Claim 6 (depends on 1)

The pumpable cement slurry composition of claim 1, wherein the amorphous phase of the first aluminosilicate additive is greater than or equal to about 90% and the weight ratio of silica to aluminum oxide of the first aluminosilicate additive is about 1.1 to about 2.3.

### Claim 7 (depends on 1)

The pumpable cement slurry composition of claim 1, wherein the at least one cement component is Portland cement or ordinary Portland cement, construction cement, or a combination thereof.

### Claim at position 5

8-11. (canceled)

### Claim 12 (depends on 1)

The pumpable cement slurry composition of claim 1, wherein particle sizes of the first and the second aluminosilicate additives are each less than particle sizes of the cement particles.

### Claim 13 (depends on 1)

The pumpable cement slurry composition of claim 1, wherein a and a viscosity of the pumpable cement slurry composition is less than about 400 cP.

### Claim at position 8

14-15. (canceled)

### Claim 16

A method for cementing a subterranean well comprising of a borehole, the method comprising:
preparing a pumpable cement slurry composition comprising:
at least one cement component comprising a cement particles;
water present at a concentration of at least about 200% by weight of the cement component;
a first aluminosilicate additive comprising metakaolin and having an amorphous phase of greater than about 50% and a silica to aluminum ratio (Si/Al ratio) of about 1.0 to about 2.5;
a second aluminosilicate additive comprising rice husk ash; and
at least one cement additive selected from one or more dispersants, at least one antifoam, one or more retarders, one or more accelerators, silica, or at least one combination thereof;
wherein the first and second aluminosilicate additives are each present at a concentration of about 10% to about 15% by weight of the at least one cement component and comprise a weight ratio of silica to aluminum oxide (Si/Al weight ratio) of about 1.0 to about 2.5, and
wherein the density of the pumpable cement slurry composition comprises a density of about 10 ppg to about 11.5 ppg and a solid volume fraction of less than about 40%;
pumping the pumpable cement slurry composition into the subterranean well such that the pumpable cement slurry composition is disposed at or in a zone of the subterranean well; and
allowing the pumpable cement slurry composition to set and form a solid mass in the zone.

### Claim 17

(canceled)

### Claim 18 (depends on 16)

The method of claim 16, wherein the second aluminosilicate additive is present at a concentration of about 10% to about 15% by weight of the cement component and has a weight ratio of silica to aluminum oxide of about 1.7 to about 2.5.

### Claim 19 (depends on 18)

The method of claim 18, wherein a viscosity of the pumpable cement slurry composition is less than about 400 cP.

### Claim 20

(canceled)

### Claim 21 (depends on 1)

The method of claim 1, wherein the density of the pumpable cement slurry composition is about 10 ppg to about 11 ppg.

### Claim 22 (depends on 13)

The method of claim 13, wherein the viscosity of the pumpable cement slurry composition is less than about 350 cP.

### Claim 23 (depends on 13)

The method of claim 13, wherein the viscosity of the pumpable cement slurry composition is less than about 300 cP.

### Claim 24 (depends on 15)

The method of claim 15, wherein a solid volume fraction of the pumpable cement slurry composition is less than about 35%.

### Claim 25 (depends on 24)

The method of claim 24, wherein a solid volume fraction of the pumpable cement slurry composition is less than about 25%.

### Claim 26 (depends on 24)

The method of claim 24, wherein the at least one cement component is Portland cement.

### Claim 27 (depends on 24)

The method of claim 24, wherein the at least one cement component is ordinary Portland cement.