# US 2024/0182675 A1 · Flame retardant polypropylene composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0182675 A1
- Document ID: US20240182675A1
- Status: Published application
- Kind: A1
- Application number: 18/549,210
- Filed: 2022-03-11
- Published: 2024-06-06
- Earliest claimed: 2021-03-11
- Applicants: Borealis AG
- Inventors: Wolfgang Stockreiter; Roberta Pellecchia; Bettina Friedl; Paulina Sariomaa; Florian Schütz; Francis Reny Costa; Antonios Gitsas; Anton Sageder
- Web page: https://patentgrep.com/patent/US20240182675A1

## CPC

- C08K 3/32: Phosphorus-containing compounds
- C08L 23/12: Polypropene
- C08K 3/40: Glass
- C08K 7/14: Glass
- C08K 2003/321: {Phosphates}
- C08L 2201/02: Flame or fire retardant/resistant
- C08L 2203/20: use in electrical or conductive gadgets
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present invention is directed to a polypropylene composition (C) comprising a propylene polymer (PP), a flame retardant (FR), fibers (F) and optionally an adhesion promoter (AP) as well as an article comprising said polypropylene composition (C).

## Claims

### Claim 1

A polypropylene composition (C), comprising
i) 20.0 to 80.0 wt. % of a propylene polymer (PP) having a melt flow rate MFR2 (230° C., 2.16 kg) determined according to ISO 1133 of at least 45.0 g/10 min,
ii) 10.0 to 40.0 wt. % of a nitrogen-containing flame retardant (FR),
iii) 10.0 to 40.0 wt. % of fibers (F), and
iv) 0.0 to 5.0 wt. % of an adhesion promoter (AP),
based on the overall weight of the polypropylene composition (C).

### Claim 2 (depends on 1)

The polypropylene composition (C) according to claim 1, wherein the propylene polymer (PP) has a melt flow rate MFR2 (230° C., 2.16 kg) determined according to ISO 1133 in a range of 50.0 to 600 g/10 min.

### Claim 3 (depends on 2)

The polypropylene composition (C) according to claim 2, wherein the propylene polymer (PP) has a melt flow rate MFR2 (230° C., 2.16 kg) determined according to ISO 1133 in a range of 60.0 to 300 g/10 min.

### Claim 4 (depends on 1)

The polypropylene composition (C) according to claim 1, having a melt flow rate MFR2 (230° C., 2.16 kg) determined according to ISO 1133 in a range of 6.0 to 40.0 g/10 min.

### Claim 5 (depends on 1)

The polypropylene composition (C) according to claim 1, wherein:
i) the polypropylene composition (C) is free of fluoropolymers, and/or
ii) the nitrogen-containing flame retardant (FR) is free of halogens.

### Claim 6 (depends on 1)

The polypropylene composition (C) according to claim 1, wherein the nitrogen-containing flame retardant (FR) comprises a first nitrogen-containing phosphate (FR1) and a second nitrogen-containing phosphate (FR2), and optionally wherein a weight ratio between the first nitrogen-containing phosphate (FR1) and the second nitrogen-containing phosphate (FR2) is in a range of 60:40 to 40:60.

### Claim 7 (depends on 6)

The polypropylene composition (C) according to claim 6, wherein the first nitrogen-containing phosphate (FR1) is melamine polyphosphate and the second nitrogen-containing phosphate (FR2) is piperazine pyrophosphate.

### Claim 8 (depends on 1)

The polypropylene composition (C) according to claim 1, wherein the propylene polymer (PP) is a copolymer of propylene and ethylene and/or a C4 to C8 α-olefin having a comonomer content in a range of 2.0 to 25.0 mol-%.

### Claim 9 (depends on 1)

The polypropylene composition (C) according to claim 1, wherein the propylene polymer (PP) is a heterophasic propylene copolymer (HECO) comprising
i) a matrix (M) being a polymer of propylene, and
ii) an elastomer (E) being a copolymer comprising units derived from propylene and ethylene and/or C4 to C20 α-olefin.

### Claim 10 (depends on 9)

The polypropylene composition (C) according to claim 9, wherein the heterophasic propylene copolymer (HECO) has a xylene cold soluble fraction (XCS) in a range of 7.0 to 25.0 wt. %, based on the overall weight of the heterophasic propylene copolymer (HECO).

### Claim 11 (depends on 9)

The polypropylene composition (C) according to claim 9, wherein the xylene soluble fraction (XCS) of the heterophasic propylene copolymer (HECO) has:
i) a comonomer content above 35.0 mol. %, and/or
ii) an intrinsic viscosity (IV) measured according to ISO 1628/1 (at 135° ° C. in decalin) below 3.5 dl/g.

### Claim 12 (depends on 1)

The polypropylene composition (C) according to claim 1, wherein the propylene polymer (PP) is a homopolymer of propylene.

### Claim 13 (depends on 1)

The polypropylene composition (C) according to claim 1, wherein the propylene polymer (PP) has a melt flow rate MFR2 (230° C., 2.16 kg) determined according to ISO 1133 in a range of 105 to 600 g/10 min.

### Claim 14 (depends on 1)

The polypropylene composition (C) according to claim 1, wherein the fibers (F) are glass fibers (GF).

### Claim 15 (depends on 1)

The polypropylene composition (C) according to claim 1, wherein the adhesion promoter (AP) is a polar modified polypropylene (PM-PP) being a propylene homo- or copolymer grafted with maleic anhydride having a melt flow rate MFR2 (230° C., 2.16 kg) determined according to ISO 1133 of at least 20.0 g/10 min.

### Claim 16 (depends on 1)

The polypropylene composition (C) according to claim 1, wherein the overall amounts of the propylene polymer (PP), the nitrogen-containing flame retardant (FR), the fibers (F) and optionally the adhesion promoter (AP) together make up at least 90 wt. % of the polypropylene composition (C).

### Claim 17 (depends on 1)

An article, comprising the polypropylene composition (C) according to claim 1.

### Claim 18 (depends on 17)

The article according to claim 17, having a shrinkage in flow and cross flow, determined as described in the description in section “Measuring methods”, of below 2.0%.

### Claim 19 (depends on 14)

The polypropylene composition (C) according to claim 14, wherein the glass fibers (GF) are short glass fibers (SGF) having a weight average fiber length in a range of 0.2 to 1.2 mm, as determined according to the FASEP method as described in the description in section “Measuring methods” after injection moulding according to EN ISO 1873-2.