# US 2024/0182667 A1 · Filler composition, composite material and composite material layer with thermal barrier properties

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0182667 A1
- Document ID: US20240182667A1
- Status: Published application
- Kind: A1
- Application number: 18/524,338
- Filed: 2023-11-30
- Published: 2024-06-06
- Earliest claimed: 2022-12-02
- Assignees: Saint-Gobain Performance Plastics Corporation
- Applicants: Saint-Gobain Performance Plastics Corporation
- Inventors: Yangdi LI; Shifang ZHAO; Yue DONG
- Web page: https://patentgrep.com/patent/US20240182667A1

## CPC

- C08K 3/016: Flame-proofing or flame-retarding additives
- C08K 3/22: of metals
- C08K 3/36: Silica
- C09D 5/18: Fireproof paints {including high temperature resistant paints}
- C09D 7/61: inorganic
- C08K 3/2279: {of antimony}
- C08K 2003/2206: {of calcium, strontium or barium}
- C08K 2003/2227: {of aluminium}
- C08K 2003/2296: {of zinc}
- C08K 2201/005: Additives being defined by their particle size in general
- C08K 2201/014: Additives containing two or more different additives of the same subgroup in C08K
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

The subject application relates to a filler composition, composite material and composite material layer with thermal barrier properties. The present disclosure relates to a filler composition may include a ceramization filler component at a content of at least about 75 wt. % and not greater than about 95 wt. % for a total weight of the filler composition, a structure promoter component at a content of at least about 0.1 wt. % and not greater than about 7.0 wt. % for a total weight of the filler composition, a flux component at a content of at least about 0.1 wt. % and not greater than about 7.0 wt. % for a total weight of the filler composition, and a flame retardant component at least about 5.0 wt. % and not greater than about 20.0 wt. % for a total weight of the filler composition.

## Claims

### Claim 1

A filler composition comprising:
a ceramization filler component at a content of at least about 75 wt. % and not greater than about 95 wt. % for a total weight of the filler composition,
a structure promoter component at a content of at least about 0.1 wt. % and not greater than about 7.0 wt. % for a total weight of the filler composition,
a flux component at a content of at least about 0.1 wt. % and not greater than about 7.0 wt. % for a total weight of the filler composition, and
a flame retardant component at least about 5.0 wt. % and not greater than about 20.0 wt. % for a total weight of the filler composition.

### Claim 2

A composite material comprising:
a polymer-based matrix component, and
a filler composition distributed within the polymer-based component,
wherein the filler composition comprises:
a ceramization filler component,
a structure promoter component,
a flux component, and
a flame retardant component.

### Claim 3 (depends on 2)

The composite material of claim 2, wherein the composite material comprises a 5 minute HPE cold side temperature of not greater than about 800° C. as measured after 5 minutes of a hotplate test conducted at 800° C.

### Claim 4 (depends on 2)

The composite material of claim 2, wherein the composite material comprises a 15 minute HPE cold side temperature of not greater than about 800° C. as measured after 15 minutes of a hotplate test conducted at 800° C.

### Claim 5 (depends on 2)

The composite material of claim 2, wherein the composite material comprises a 30 minute HPE cold side temperature of not greater than about 800° C. as measured after 30 minutes of a hotplate test conducted at 800° C.

### Claim 6 (depends on 2)

The composite material of claim 2, wherein the composite material comprises a 5 minute TE cold side temperature of not greater than about 800° C. as measured at 5 minutes of a torch test conducted at 1300° C.

### Claim 7 (depends on 2)

The composite material of claim 2, wherein the composite material comprises a 15 minute TE cold side temperature of not greater than about 800° C. as measured at 15 minutes of a torch test conducted at 1300° C.

### Claim 8 (depends on 2)

The composite material of claim 2, wherein the composite material comprises a 30 minute TE cold side temperature of not greater than about 800° C. as measured at 30 minutes of a torch test conducted at 1300° C.

### Claim 9 (depends on 2)

The composite material of claim 2, wherein the composite material comprises a V-0 flammability rating as measured according to ASTM D3801.

### Claim 10 (depends on 2)

The composite material of claim 2, wherein the polymer-based component comprises a component selected from the group consisting of silicone, polyurethane, epoxy, acrylic resin or any combination thereof.

### Claim 11 (depends on 2)

The composite material of claim 2, wherein the composite material comprises a polymer-based component content of at least about 30 wt. % for a total weight of the composite material.

### Claim 12 (depends on 2)

The composite material of claim 2, wherein the composite material comprises a polymer-based component content of not greater than about 60 wt. % for a total weight of the composite material.

### Claim 13 (depends on 2)

The composite material of claim 2, wherein the composite material comprises a filler composition content of at least about 40 wt. % for a total weight of the composite material.

### Claim 14 (depends on 2)

The composite material of claim 2, wherein the composite material comprises a filler composition content of not greater than about 70 wt. % for a total weight of the composite material.

### Claim 15

A composite material layer comprising:
a polymer-based matrix component, and
a filler composition distributed within the polymer-based component,
wherein the filler composition comprises:
a ceramization filler component,
a structure promoter component,
a flux component, and
a flame retardant component.

### Claim 16 (depends on 15)

The composite material layer of claim 15, wherein the composite material layer comprises a 5 minute HPE cold side temperature of not greater than about 800° C. as measured after 5 minutes of a hotplate test conducted at 800° C.

### Claim 17 (depends on 15)

The composite material layer of claim 15, wherein the composite material layer comprises a 15 minute HPE cold side temperature of not greater than about 800° C. as measured after 15 minutes of a hotplate test conducted at 800° C.

### Claim 18 (depends on 15)

The composite material layer of claim 15, wherein the composite material layer comprises a 30 minute HPE cold side temperature of not greater than about 800° C. as measured after 30 minutes of a hotplate test conducted at 800° C.

### Claim 19 (depends on 15)

The composite material layer of claim 15, wherein the composite material layer comprises a 5 minute TE cold side temperature of not greater than about 800° C. as measured at 5 minutes of a torch test conducted at 1300° C.

### Claim 20 (depends on 2)

The composite material of claim 2, wherein the composite material comprises a 15 minute TE cold side temperature of not greater than about 800° C. as measured at 15 minutes of a torch test conducted at 1300° C.