# US 2024/0182357 A1 · Glass and ceramic structures, and methods for fabrication and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0182357 A1
- Document ID: US20240182357A1
- Status: Published application
- Kind: A1
- Application number: 18/529,626
- Filed: 2023-12-05
- Published: 2024-06-06
- Earliest claimed: 2022-12-05
- Applicants: University of Maryland, College Park
- Inventors: Liangbing HU; Xinpeng ZHAO
- Web page: https://patentgrep.com/patent/US20240182357A1

## CPC

- C03C 17/007: {containing a dispersed phase, e.g. particles, fibres or flakes, in a continuous phase}
- C03C 17/25: by deposition from the liquid phase
- C03C 3/06: with more than 90% silica by weight, e.g. quartz {(C03C3/045 takes precedence)}
- C03C 4/02: for coloured glass
- C03C 2201/02: Pure silica glass, e.g. pure fused quartz
- C03C 2201/11: containing chlorine
- C03C 2201/40: containing transition metals other than rare earth metals, e.g. Zr, Nb, Ta or Zn
- C03C 2203/50: After-treatment
- C03C 2204/00: Glasses, glazes or enamels with special properties
- C03C 2217/45: Inorganic continuous phases
- C03C 2217/475: Inorganic materials
- C03C 2218/11: from solutions or suspensions
- C03C 2218/32: After-treatment
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A structure can comprise a substrate and a composite coating. The composite coating can be formed over a surface of the substrate. The composite coating can include one or more nanoparticles within an oxide matrix. The nanoparticles can be formed of a temperature-dependent Mott insulator having a phase transition temperature. At a temperature below the phase transition temperature, the composite coating can transmit light in a first wavelength range, and at a temperature above the phase transition temperature, the composite coating can block light in the first wavelength range. For example, the structure can be used as a smart 10 window to help regulate heating of building interiors due to solar radiation. The composite coating can be formed via a short-duration, high-temperature heating pulse, for example, at least 1500 K for less than 60 seconds.

## Claims

### Claim 1

A structure comprising:
a substrate; and
a composite coating formed over a surface of the substrate, the composite coating comprising an oxide matrix and one or more nanoparticles within the oxide matrix,
wherein the one or more nanoparticles comprise a temperature-dependent Mott insulator having a phase transition temperature,
when at a temperature below the phase transition temperature, the composite coating transmits light in a first wavelength range, and
when at a temperature above the phase transition temperature, the composite coating reflects and/or absorbs the light in the first wavelength range.

### Claim 2 (depends on 1)

The structure of claim 1, wherein the first wavelength range is 780-2500 nm.

### Claim 3 (depends on 1)

The structure of claim 1, wherein the composite coating transmits light in a second wavelength range regardless of a temperature of the composite coating.

### Claim 4 (depends on 3)

The structure of claim 3, wherein the second wavelength range is 400-700 nm.

### Claim 5 (depends on 3)

The structure of claim 3, wherein:
(a) the substrate is substantially transparent to light in the first and second wavelength ranges;
(b) the oxide matrix is substantially transparent to light in the first and second wavelength ranges; or
(c) both (a) and (b).

### Claim 6 (depends on 1)

The structure of claim 1, wherein the one or more nanoparticles are formed of vanadium dioxide (VO2).

### Claim 7 (depends on 1)

The structure of claim 1, wherein the substrate comprises silica glass.

### Claim 8 (depends on 1)

The structure of claim 1, wherein the oxide matrix comprises Al2O3, B2O3, BaO, Bi2O3, CaO, H3BO3, K2O, Li2O, MgO, Na2CO3, Na2O, P2O5, PbO, Sb2O3, Sb2O5, SiO2, SnF2, TeO2, TiO2, ZnO, or any combination of the foregoing.

### Claim 9 (depends on 1)

The structure of claim 1, wherein:
(a) the composite coating has a thickness less than or equal to 50 μm;
(b) the composite coating has a relative density of at least 95%; or
(c) both (a) and (b).

### Claim 10 (depends on 1)

The structure of claim 1, wherein a concentration of the one or more nanoparticles in the composite coating is less than or equal to 0.1 wt %.

### Claim 11

A method comprising:
(i) forming a precursor coating by dispensing a slurry over a surface of a substrate, the slurry comprising a precursor powder and one or more nanoparticles in a solution, the one or more nanoparticles comprising a temperature-dependent Mott insulator having a phase transition temperature; and
(ii) after (i), subjecting the precursor coating to a high temperature heating pulse so as to convert the precursor coating into a composite coating, the high temperature heating pulse comprising exposure to a temperature of at least 1500 K for a duration of less than 60 seconds,
wherein, after (ii), the composite coating has a porosity and/or density greater than the precursor coating,
the composite coating comprises an oxide matrix formed from the precursor powder and the one or more nanoparticles within the oxide matrix,
when at a temperature below the phase transition temperature, the composite coating transmits light in a first wavelength range, and
when at a temperature above the phase transition temperature, the composite coating reflects and/or absorbs the light in the first wavelength range.

### Claim 12 (depends on 11)

The method of claim 11, wherein, after (ii), the composite coating transmits light in a second wavelength range regardless of a temperature of the composite coating.

### Claim 13 (depends on 12)

The method of claim 12, wherein:
(a) the first wavelength range is 780-2500 nm;
(b) the second wavelength range is 400-700 nm; or
(c) both (a) and (b).

### Claim 14 (depends on 12)

The method of claim 12, wherein:
(a) the substrate is substantially transparent to light in the first and second wavelength ranges;
(b) after (ii), the oxide matrix is substantially transparent to light in the first and second wavelength ranges; or
(c) both (a) and (b).

### Claim 15 (depends on 11)

The method of claim 11, wherein the one or more nanoparticles are formed of vanadium dioxide (VO2).

### Claim 16 (depends on 11)

The method of claim 11, wherein:
(a) the substrate comprises silica glass;
(b) the precursor powder comprises Al2O3, B2O3, BaO, Bi2O3, CaO, H3BO3, K2O, Li2O, MgO, Na2CO3, Na2O, P2O5, PbO, Sb2O3, Sb2O5, SiO2, SnF2, TeO2, TiO2, ZnO, or any combination of the foregoing;
(c) a particle size of the precursor powder is less than or equal to 100 μm; or
(d) any combination of (a)-(c).

### Claim 17 (depends on 11)

The method of claim 11, wherein, after (ii):
(a) the composite coating has a thickness less than or equal to 50 μm;
(b) the composite coating has a relative density of at least 95%;
(c) a concentration of the one or more nanoparticles in the composite coating is less than or equal to 0.1 wt %; or
(d) any combination of (a)-(c).

### Claim 18 (depends on 11)

The method of claim 11, wherein:
(a) the temperature of the high temperature heating pulse is in a range of 1500-1700 K, inclusive;
(b) the duration of the high temperature heating pulse is in a range of 3-30 seconds, inclusive; or
(c) both (a) and (b).

### Claim 19 (depends on 11)

The method of claim 11, wherein the high temperature heating pulse further comprises:
prior to the duration, heating to the temperature at a heating rate of at least 102 K/s; and
after the duration, cooling from the duration at a cooling rate of a least 102K/s.

### Claim 20 (depends on 11)

The method of claim 11, wherein the high temperature heating pulse is generated by passing an electrical current through a Joule heating element spaced from the precursor coating.