# US 2024/0182304 A1 · Method for the high efficiency recycling of iron phosphate black powder slag

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0182304 A1
- Document ID: US20240182304A1
- Status: Published application
- Kind: A1
- Application number: 18/074,501
- Filed: 2022-12-04
- Published: 2024-06-06
- Earliest claimed: 2022-12-04
- Assignees: Watix Technology LLC
- Inventors: Robert Brian Huang; Richard Brian Huang
- Web page: https://patentgrep.com/patent/US20240182304A1

## CPC

- C01B 25/375: {of iron}
- B01J 20/06: comprising oxides or hydroxides of metals not provided for in group B01J20/04
- C01B 25/303: {with elimination of impurities}
- C01B 25/36: Aluminium phosphates
- C22B 7/04: Working-up slag
- C22B 21/0023: {from waste materials}
- C22B 21/04: with alkali metals {earth alkali metals included}
- C22B 26/12: Obtaining lithium
- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- Y02W 30/84: Recycling of batteries or fuel cells
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

This method recycles iron phosphate slag, which is produced as waste during lithium iron phosphate battery recycling processes that contain leaching or crushing for the sole extraction of lithium. This method extracts aluminum phosphate, iron phosphate, and lithium phosphate from the waste slag. The recycling process comprises these steps: (a) extraction of aluminum phosphate through addition of sodium hydroxide; (b) removal of carbon additives, graphite and other organic compounds through solvation of solely lithium, iron, and phosphate compounds through addition of sulfuric acid; (c) precipitation of iron phosphate by addition of hydrogen peroxide; (d) extraction of lithium phosphate from the mother liquor; (e) recycling of mother liquor into water and sodium sulfate. This process wastes few chemicals while still having a high reclamation efficiency in terms of purity and quantity. Furthermore, due to its relatively low costs, the profit margin of this process is very good.

## Claims

### Claim 1

A method for recycling iron phosphate slag, comprising the following sequential steps:
(S1) extracting the aluminum phosphate in the iron phosphate slag by sequentially:
a) mixing iron phosphate slag, sodium hydroxide, and water to solvate the aluminum present in the slag as sodium aluminum oxide;
b) filtering the resulting solution from a) to remove the solid slag (the solid slag of which is characterized primarily by iron phosphate, lithium compounds, and carbon, and henceforth known as Soli-1) from the filtrate (the filtrate of which is characterized primarily by sodium aluminum oxide, and henceforth known as Solu-1);
c) mixing Solu-1 and phosphoric acid to precipitate aluminum phosphate;
d) filtering the resulting solution from c) to extract the aluminum phosphate from the filtrate (the filtrate of which is characterized primarily by phosphate compounds with very little lithium compounds, and henceforth known as Solu-2);
(S2) removing carbon additives, graphite and other organic compounds by sequentially:
e) mixing Soli-1, sulfuric acid, and water to solvate the lithium, iron, and phosphate compounds;
f) filtering the resulting solution from e) to remove the solid carbon slag from the filtrate (the filtrate of which is characterized primarily by lithium sulfate, iron sulfate, and phosphoric acid, and henceforth known as Solu-3);
(S3) extracting the iron phosphate by sequentially:
g) mixing Solu-2, Solu-3, and hydrogen peroxide to precipitate iron phosphate;
h) filtering the resulting solution of g) to obtain the impure iron phosphate from the filtrate (the filtrate of which is characterized primarily by lithium sulfate, and henceforth known as Solu-4);
i) mixing the impure iron phosphate with a low concentration solution of phosphoric acid;
j) filtering the resulting solution of i) to obtain the iron phosphate from the filtrate, the filtrate of which is added to Solu-4;
k) washing the obtained iron phosphate of j) by mixing the iron phosphate with water and filtering the resulting solution to extract the wet iron phosphate;
l) subjecting the wet iron phosphate to be sequentially dried in an air atmosphere, calcined at a high temperature, crushed, and sieved;
(S4) extracting lithium phosphate from the mother liquor by sequentially:
m) mixing Solu-4 and sodium hydroxide to precipitate unreacted slag waste;
n) filtering the resulting solution of m) to remove the unreacted slag waste from the lithium sulfate solution;
o) placing a lithium adsorbent into the resulting lithium sulfate solution of n) to extract lithium ions into or onto the adsorbent;
p) taking the adsorbent out of the solution (the solution of which is characterized primarily by sulfate compounds, and henceforth known as Solu-5) and placing the adsorbent into a high concentration of sulfuric acid to solvate the lithium ions into lithium sulfate;
q) mixing the resulting lithium sulfate solution of step p) with sodium phosphate to precipitate lithium phosphate;
r) filtering the resulting solution of q) to obtain the lithium phosphate from the filtrate (the filtrate of which is characterized primarily by sodium sulfate, and henceforth known as Solu-6);
s) drying the lithium phosphate in an air atmosphere;
(S5) Recycling the mother liquor into water and sodium sulfate by sequentially:
t) mixing Solu-5 and Solu-6 and feeding the resulting solution into a mechanical vapor recompression (henceforth known as MVR) system;
u) centrifuging and drying any recovered solid materials from t) in an air atmosphere to extract sodium sulfate.

### Claim 2 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein, in step S1 (a), sodium hydroxide and water is mixed with the slag such that the resulting solution's pH is 8-10 and its liquid mass percentage content is 30-80%.

### Claim 3 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein, whenever a filtering step is conducted, a machine or tool is used primarily to separate the solid material in a solution from the liquid portion or to separate the liquid portion of a solution from the solid material; this does not include embodiments wherein the machine or tool performs another primary function that benefits the final product.

### Claim 4 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein, whenever a filtering step is conducted, the step is replaced by two or more sequential filtering steps, whereby the filtrates from a preceding step are sequentially fed into a subsequent filtering step and, during these multiple steps, the residual solids from each step are collated while only the final filtrate is collected.

### Claim 5 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein each mixing step is performed at 30° C.-80° C. under rapid stirring for at least 1 min.

### Claim 6 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein, in step S1 (c), phosphoric acid is added to the sodium aluminum oxide solution to control the pH to 4.5-5.5.

### Claim 7 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein, in step S2 (e), sulfuric acid and water is mixed with the slag such that the resulting solution's pH is 3-4 and its liquid mass percentage content is 30-80%.

### Claim 8 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein, in step S3 (g), hydrogen peroxide is added to Solu-3 to control the pH to 3-4.

### Claim 9 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein, in step S3, an aging step is performed directly after (g) mixing Solu-2, Solu-3, and hydrogen peroxide to precipitate iron phosphate; this aging step of which may utilize a stirring, heating, or cooling step, or a combination of one or multiple stirring, heating and cooling steps, but the overall aging step takes no more than 5 hours to precipitate the iron phosphate.

### Claim 10 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein, in step S3 (i), the low concentration phosphoric acid has a concentration between 0.05M-0.3M and has an overall mass equal to 50%-200% of the impure iron phosphate's mass.

### Claim 11 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein, in step S3 (k), the iron phosphate washing with water step is either not performed, or is performed multiple times, whereby the resulting wet iron phosphate after a preceding washing step is fed into the subsequent step as the next step's iron phosphate.

### Claim 12 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein, in step S3, S4, and S5, during drying steps (l) (s) (u), the material is dried at 100° C.-200° ° C. for 1 to 24 hours.

### Claim 13 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein, in step S3 (l), the iron phosphate is calcined at 350-550° C. for 1 to 9 hours.

### Claim 14 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein, in step S3 (l), the crushing and sieving can be replaced by two or more sequential grinding or milling steps, whereby in each step, a machine or tool is used primarily to evenly or unevenly apply force to the iron phosphate such that the material either becomes smaller or has less or smaller clumps; this does not include embodiments wherein the machine or tool performs another primary function that benefits the final product.

### Claim 15 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein, in step S4 (m), sodium hydroxide is added to Solu-4 to control the pH to 7-8.

### Claim 16 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein, in step S4 (o), the lithium adsorbent is one or a combination of cellulose nanocrystal, lithium ion sieve, lithium manganese oxide, lithium titanium oxide, hydrogen titanium oxide, and hydrogen manganese oxide, wherein the mass of the lithium adsorbent is 2% to 20% of the mass of the lithium sulfate solution and the adsorption process takes 15 minutes to 5 hours.

### Claim 17 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein, in step S4 (p), the high concentration sulfuric acid has a concentration between 0.5M-3M and has an overall mass equal to 10%-100% of the adsorbent's mass, and the desorption process takes 15 minutes to 5 hours.

### Claim 18 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein, in step S4 (q), the sodium phosphate has a mass equal to 5%-50% of the adsorbent's mass.

### Claim 19 (depends on 1)

The method for recycling iron phosphate slag of claim 1, wherein one of or a combination of Solu-2, the filtrate produced after filtering the low concentration phosphoric acid and iron phosphate solution in step S3, and Solu-5 is thrown away as waste or recycled directly in an MVR system and not later mixed with their respective solutions.