# US 2024/0178398 A1 · Water based binder composition and application thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0178398 A1
- Document ID: US20240178398A1
- Status: Published application
- Kind: A1
- Application number: 18/284,901
- Filed: 2022-05-12
- Published: 2024-05-30
- Earliest claimed: 2021-05-14
- Assignees: Arkema Inc.
- Applicants: Arkema Inc.
- Inventors: Ramin AMIN-SANAYEI; Jean-Marc SUAU; Wenjun WU; Jinbao CAO; Marine DUVER
- Web page: https://patentgrep.com/patent/US20240178398A1

## CPC

- H01G 11/38: Carbon pastes or blends; Binders or additives therein
- H01M 4/622: {being polymers}
- H01G 11/32: Carbon-based
- H01G 11/50: specially adapted for lithium-ion capacitors, e.g. for lithium-doping or for intercalation
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/387: {Tin or alloys based on tin}
- H01M 4/48: of inorganic oxides or hydroxides
- H01M 4/483: {for non-aqueous cells (H01M4/485 takes precedence)}
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/625: {Carbon or graphite}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01G 11/86: specially adapted for electrodes (carbonisation or activation of carbon for the manufacture of electrodes H01G11/34)
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- H01M 2300/0025: Organic electrolyte
- Y02E 60/10: Energy storage using batteries
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An electrode forming slurry composition is provided. The electrode-forming slurry compositions include a) from 10 to 300 parts of one or more particulate electrode-forming materials; b) from 0.1 to 60 parts of polymeric latex particles; and c) 100 parts water. The electrode forming slurry compositions can form an electrode, an anode for a non-aqueous secondary battery, in particular a lithium ion battery. The polymeric latex particles b) include i) at least one ethylenically unsaturated monomer comprising at least one acid functional group; and include ii) no fluorinated monomer or butadiene monomer polymerized therein. Also provided is an anode including the electrode forming slurry composition in dried form.

## Claims

### Claim 1

A electrode forming slurry composition comprising;
a) from 10 to 300 parts of one or more particulate anode-forming materials;
b) from 0.1 to 60 parts of polymeric latex particles comprising:
i) at least one ethylenically unsaturated monomer comprising at least one acid functional group; and
ii) no fluorinated monomer or monomer containing conjugated double bonds polymerized therein;
wherein the polymeric latex particles b) have:
a Tg of 55° C. or less and/or a minimum film forming temperature of 25° C. or less;
a volume average particle size of less than 500 nm; and
an acid number of from 40 to 400 mg of KOH equivalent such that at least 10% of the acid functional groups of the at least one ethylenically unsaturated monomer comprising at least one acid functional group are neutralized,
and wherein 5% by weight of the polymeric latex particles b) in water have a viscosity of at least 1000 cP at a shear rate of 10 s-1 and 25° C. at a pH of from 3 to 7;
c) 100 parts water;
d) optionally from 0 to 5 parts of one or more wetting agents;
e) optionally from 0 to 5 parts of one or more dispersing agents;
f) optionally from 0 to 5 parts of one or more VOCs, and/or adhesion promoters and/or coalescent agents;
g) optionally from 0 to 5 parts of rheology modifier additives; and
h) optionally from 0 to 10 parts of one or more additives selected from the group consisting of anti-settling agents, surfactants, and mixtures thereof;
wherein the electrode forming slurry composition is capable of forming an electrode.

### Claim 2 (depends on 1)

The electrode forming slurry composition of claim 1, wherein the polymeric latex particles b) comprise, as polymerized monomers:
from 10% to 60% by weight of the total polymerized monomers, of the i) at least one ethylenically unsaturated monomer comprising at least one acid functional group, and
further comprise from 40 to 90%, by weight of the total polymerized monomers, of ii) at least one non-ionic ethylenically unsaturated monomer.

### Claim 3 (depends on 1)

The electrode forming slurry composition of claim 1, wherein the i) ethylenically unsaturated monomers comprising at least one acid functional group are selected from the group consisting of (meth) acrylic acid, beta-polycarboxy ethyl acrylate, 4-styrene sulfonic acid, 2-acrylamido-2-methylpropane sulfonic acid, vinyl phosphonic acid, vinyl sulfonic acid, mono-esters of itaconic acid, maleic acid, fumaric acid, and mixtures thereof.

### Claim 4 (depends on 1)

The electrode forming slurry composition of claim 1, wherein the ii) at least one non-ionic ethylenically unsaturated monomer is selected from the group consisting of C1 to C12 (meth)acrylates, (meth)acrylamides, (meth)acrylonitriles, vinyl acetate, styrene and derivatives thereof, diisobutylene, vinylpyrrolidone, vinylcaprolactam, and mixtures thereof.

### Claim 5 (depends on 1)

The electrode forming slurry composition of claim 1, wherein the polymeric latex particles b) further comprise, as polymerized monomers:
iii) from 0.05% to 5%, by weight of total polymerized monomers, of at least one monomer comprising at least two free radical polymerizable ethylenic unsaturations.

### Claim 6 (depends on 1)

The electrode forming slurry composition of claim 1, wherein the at least one monomer comprising at least two free radical polymerizable ethylenic unsaturations iii) is selected from the group consisting of allylic ethers derived from polyols selected from pentaerythritol, sorbitol, or sucrose; diacrylic or dimethacrylic esters derived from polyols selected from pentaerythritol, sorbitol, or sucrose; divinyl naphthalene, trivinylbenzene, 1,2,4-trivinylcyclohexane, triallyl pentaerythritol, diallyl pentaerythritol, diallyl sucrose, trimethylolpropane diallyl ether, 1,6-hexanediol di(meth)acrylate, allyl (meth)acrylate, diallyl itaconate, diallyl fumarate, diallyl maleate, butanediol dimethacrylate, ethylene di(meth)acrylate, poly(ethylene glycol) di(meth)acrylate, trimethylolpropane tri(meth)acrylate, methylenebis(meth)acrylamide, triallylcyanurates, diallyl phthalate, divinylbenzene and mixtures thereof in the polymeric latex particles b) at from 0.05 to 10% by weight of the total polymerized monomers in the polymeric latex particles b).

### Claim 7 (depends on 1)

The electrode forming slurry composition of claim 1, wherein the polymeric latex particles b) further comprise, as polymerized monomers:
iv) from 0.1 to 15 to wt % of at least one oxyalkylated monomer with ethylenic unsaturation and terminated by a hydrogen or hydrophobic aryl or alkyl chain with 1 to 60 carbon atoms, having the following formulae-:
wherein:
m and p represent a number of alkylene oxide units of from 0 and 150,
n represents a number of ethylene oxide units of from 5 and 150,
q represents a whole number at least equal to 1 and such that 5 (m+n+p)q 150, R1 and R2 represent hydrogen, methyl or ethyl,
R represents a group comprising at least one polymerizable olefinic unsaturation, and mixtures thereof, and
R′ represents a hydrogen or hydrophobic aryl or alkyl chain end with 1 to 60 carbon atoms.

### Claim 8 (depends on 7)

The electrode forming slurry composition of claim 7, wherein q represents a whole number at least equal to 1 and such that 15≤(m+n+p)q≤120.

### Claim 9 (depends on 7)

The electrode forming slurry composition of claim 7, wherein R represents a group selected from the group consisting of acrylate, methacrylate, acrylurethane, methacrylurethane, vinyl, allyl, methallyl, isoprenyl, an unsaturated urethane group, and combinations thereof.

### Claim 10 (depends on 7)

The electrode forming slurry composition of claim 7, wherein R represents a group selected from the group consisting of acrylurethane, methacrylurethane, α-α′-dimethyl-isopropenyl-benzylurethane, allylurethane, and combinations thereof.

### Claim 11 (depends on 7)

The electrode forming slurry composition of claim 7, wherein R represents a group selected from the group consisting of acrylate, methacrylate, acrylurethane, methacrylurethane, vinyl, allyl, methallyl and isoprenyl, esters of maleic acid, esters of itaconic acid, esters of crotonic acid, and combinations thereof.

### Claim 12 (depends on 7)

The electrode forming slurry composition of claim 7, wherein R represents a methacrylate group.

### Claim 13 (depends on 1)

The electrode forming slurry composition of claim 1, wherein 5 wt % of the latex particles b) in water have a viscosity of at least 2000 cP at a shear rate of 10 s-1 and 25° C. and a pH of 3 to 7.

### Claim 14 (depends on 1)

The electrode forming slurry composition of claim 1, wherein the polymeric latex particles b) are self-thickening such that under a pH equal to or less than 4, an emulsion consisting of 5 wt % of the polymeric latex particles in water have a viscosity of less than 100 cP at a shear rate of 10 s-1 and 25° C., and upon addition of a base such that the pH is from 3 to 7, the viscosity of the emulsion increases to at least 1000 cP at shear rate of 10 s-1 and 25° C.

### Claim 15 (depends on 1)

The electrode forming slurry composition of claim 1, wherein the pH of the slurry composition is less than 7.

### Claim 16 (depends on 1)

The electrode forming slurry composition of claim 1, further comprising lithium hydroxide.

### Claim 17 (depends on 1)

The electrode forming slurry composition of claim 1, wherein the polymeric latex particles b) have a volume average particle size less than 250 nanometers.

### Claim 18 (depends on 1)

The electrode forming slurry composition of claim 1, wherein the composition is free of carboxymethyl cellulose (CMC).

### Claim 19 (depends on 1)

The electrode forming slurry composition of claim 1, wherein the composition is free of polymers comprising, as polymerized monomers, monomers comprising conjugated double bonds.

### Claim 20 (depends on 1)

The electrode forming slurry composition of claim 1 wherein a VOC content of the composition is from 0 to less than 1 wt %.

### Claim 21 (depends on 1)

The electrode forming slurry composition of claim 1, wherein the polymeric latex particles b) have a Tg of 25° C. or less.

### Claim 22 (depends on 1)

The electrode forming slurry composition of claim 1, wherein the particulate anode-forming materials a) comprise one or more materials selected from the group consisting of furnace black, acetylene black, Ketjen carbon black, carbon nanotubes (CNTs), synthetic graphite, natural graphite, hard carbon, activated soft carbon, carbon black, graphene, mesoporous carbon, amorphous silicon, semi-crystalline silicon, silicon oxides, silicon nanowires, tin, tin oxides, germanium, lithium titanate, and mixtures or composites thereof.

### Claim 23 (depends on 1)

An anode for use within an electrical energy storage device comprising a current collector coated on at least one surface with the electrode forming slurry composition of claim 1 in dried form, wherein the anode has a thickness of at least 10 microns and exhibits resistivity less than 100 Ω·cm in the z-direction.

### Claim 24 (depends on 21)

An electrical energy storage device containing a non-aqueous electrolyte, the electrical energy storage device comprising at least one anode of claim 21, wherein the electrical energy storage device is selected from the group consisting of a non-aqueous-type battery, a capacitor, and a membrane electrode assembly.