# US 2024/0178385 A1 · Positive electrode material, preparation method and uses thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0178385 A1
- Document ID: US20240178385A1
- Status: Published application
- Kind: A1
- Application number: 18/435,387
- Filed: 2024-02-07
- Published: 2024-05-30
- Earliest claimed: 2018-12-29
- Assignees: Contemporary Amperex Technology Co., Limited
- Applicants: Contemporary Amperex Technology Co., Limited
- Inventors: Rui Du; Yongchao Liu; Sihui Wang; Deyu Zhao; Na Liu
- Web page: https://patentgrep.com/patent/US20240178385A1

## CPC

- C01G 53/506: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.8, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.8
- H01M 4/366: {as layered products}
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/4235: {Safety or regulating additives or arrangements in electrodes, separators or electrolyte (H01M10/4242 takes precedence)}
- C01P 2002/52: containing elements as dopants
- C01P 2004/50: Agglomerated particles
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/84: one phase coated with the other
- C01P 2006/12: Surface area
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present application relates to the electrochemical field, and in particular, to a positive electrode material, and an electrochemical energy storage apparatus having thereof. The present application provides a positive electrode material, including a substrate. The substrate includes secondary particles containing primary particles. A surface of the substrate is coated with an oxide coating layer. The oxide coating layer comprises a coating element, and the coating element is selected from one or more of Al, Ba, Zn, Ti, Zr, Mg, W, Y, Si, Sn, B, Co, or P. The electrochemical energy storage apparatus comprises the foregoing positive electrode material.

## Claims

### Claim 1

A positive electrode material comprising:
a substrate comprising secondary particles, wherein each secondary particle comprises a plurality of primary particles packed together, a molecular formula of the substrate is LixNiyCozMkMepOrAm, 0.95≤x≤1.05, 0.50≤y≤0.98, 0≤z≤0.3, 0≤k≤0.4, 0≤p≤0.05, 1≤r≤2, 0≤m≤2, m+r≤2;
a coating layer disposed on a surface of the substrate, wherein the coating layer comprises an oxide of a coating element selected from Al, Ba, Zn, Ti, Zr, Mg, Y, Si, B, Co, P, and any combinations thereof,
wherein a powder resistivity ρ of the positive electrode material under a 12 MPa pressure is 500Ω*cm-2,000Ω*cm.

### Claim 2 (depends on 1)

The positive electrode material of claim 1, wherein the powder resistivity ρ of the positive electrode material under a 12 MPa pressure is 543Ω*cm-1,653Ω*cm.

### Claim 3 (depends on 1)

The positive electrode material of claim 1, wherein a content Mv of the coating element per unit volume of the positive electrode material is 400 μg/cm3 to 15,000 μg/cm3.

### Claim 4 (depends on 3)

The positive electrode material of claim 3, wherein the content Mv of the coating element per unit volume of the positive electrode material is 800 μg/cm3 to 10,000 μg/cm3.

### Claim 5 (depends on 3)

The positive electrode material of claim 3, wherein the powder resistivity ρ and the content Mv of the coating element satisfy: ρ/Mv≤1Ω*cm4/μg.

### Claim 6 (depends on 5)

The positive electrode material of claim 5, wherein the powder resistivity ρ and the content Mv of the coating element satisfy: ρ/Mv≤0.5Ω*cm4/μg.

### Claim 7 (depends on 1)

The positive electrode material of claim 1, wherein the coating element is selected from at least two of the group consisting of Al, Ba, Zn, Ti, Zr, Mg, Y, Si, B, Co, and P.

### Claim 8 (depends on 1)

The positive electrode material of claim 1, wherein the coating element is distributed on a surface of at least a part of the primary particles inside the secondary particles and distributed at grain boundaries between adjacent primary particles.

### Claim 9 (depends on 1)

The positive electrode material of claim 1, wherein a content of the coating element in the oxide coating layer is 60 wt % or more, based on a total content of the coating element in the positive electrode material.

### Claim 10 (depends on 1)

The positive electrode material of claim 1, wherein in the molecular formula of the substrate, 0.80≤y≤0.98, 0<z≤0.1, 0<k≤0.1, and 0≤p≤0.03.

### Claim 11 (depends on 1)

The positive electrode material of claim 1, wherein Dv50 of the secondary particles is 5 μm-18 μm, the primary particles have an average particle diameter of 0.1μm-1 μm.

### Claim 12 (depends on 1)

The positive electrode material of claim 1, wherein a specific surface area of the positive electrode material is 0.1 m2/g-0.8 m2/g.

### Claim 13 (depends on 1)

The positive electrode material of claim 1, wherein a content of Li2CO3 in residual lithium on a surface of the positive electrode material is less than 3,000 ppm, and a content of LiOH in the residual lithium on the surface of the positive electrode material is less than 5,000 ppm.

### Claim 14 (depends on 13)

The positive electrode material of claim 13, wherein in the residual lithium on the surface of the positive electrode material, the content of Li2CO3 is less than the content of LiOH.

### Claim 15

A method for preparing a positive electrode material, the method comprising:
forming a substrate, wherein the substrate comprises secondary particles, the secondary particle comprises a plurality of primary particles packed together, a molecular formula of the substrate is LixNiyCozMkMepOrAm, 0.95≤x≤1.05, 0.50≤y≤0.98, 0≤z≤0.3, 0≤k≤0.4, 0≤p≤0.05, 1≤r≤2, 0≤m≤2, m+r≤2; and
forming a coating layer on a surface of the substrate, wherein the coating layer comprises an oxide of a coating element selected from Al, Ba, Zn, Ti, Zr, Mg, Y, Si, B, Co, P, and any combinations thereof,
wherein a powder resistivity ρ of the positive electrode material under a 12 MPa pressure is 500Ω*cm-2,000Ω*cm.

### Claim 16 (depends on 15)

The method of claim 15, wherein forming the substrate further comprises:
forming a mixture of a lithium source and a metal source, wherein the metal source comprises a metal element selected from the group consisting of Ni, Co, Mn, Al, and any combinations thereof; and
sintering the mixture.

### Claim 17 (depends on 16)

The method of claim 16, wherein the metal source is selected from the group consisting of Ni0.5Co0.2Mn0.3(OH)2, Ni0.5Co0.25Mn0.25(OH)2, Ni0.55Co0.15Mn0.3(OH)2, Ni0.55Co0.1Mn0.35(OH)2, Ni0.55Co0.05Mn0.4(OH)2, Ni0.6Co0.2Mn0.2(OH)2, Ni0.75Co0.1Mn0.15(OH)2, Ni0.8Co0.1Mn0.1(OH)2, Ni0.88Co0.05Mn0.07(OH)2, 0.9Ni0.8Co0.2(OH)2·0.1Al2(OH)3, or 0.9Ni0.9Co0.05Mn0.05(OH)2·0.1Al2(OH)3, and any combinations thereof,
wherein the lithium source is selected from the group consisting of LiOH·H2O, LiOH, Li2CO3, Li2O, and any combinations thereof.

### Claim 18 (depends on 16)

The method of claim 16, wherein the sintering is performed at a temperature of 800° C. with an oxygen concentration greater than or equal to 20%.

### Claim 19 (depends on 15)

The method of claim 15, wherein forming the coating layer further comprises:
mixing the substrate with a compound containing the coating element, wherein the compound is selected from the group consisting of Al2O3, ZnO, ZrO2, TiO2, MgO, WO3, Y2O3, CO2O3, Ba(NO3)2, Co2O3, P2O5, H3BO3, and any combinations thereof; and
sintering the mixed substrate and compound.

### Claim 20 (depends on 19)

The method of claim 19, wherein the coating element has a dosage from 0.01 wt % to 0.5 wt %, based on a mass of the substrate, and sintering the mixed substrate and compound is performed at a temperature from 200° ° C.-700° C.