# US 2024/0178324 A1 · Crystalline inzno oxide semiconductor, method of forming the same, and semiconductor device including the crystalline inzno oxide semiconductor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0178324 A1
- Document ID: US20240178324A1
- Status: Published application
- Kind: A1
- Application number: 18/518,735
- Filed: 2023-11-24
- Published: 2024-05-30
- Earliest claimed: 2022-11-25
- Assignees: Samsung Electronics Co., Ltd.; Iucf-Hyu (Industry-University Cooperation Foundation Hanyang University)
- Applicants: Samsung Electronics Co., Ltd.; IUCF-HYU (Industry-University Cooperation Foundation Hanyang University)
- Inventors: Kwanghee LEE; Jinseong PARK; Sangwook KIM; Hyemi KIM; Seonghwan RYU
- Web page: https://patentgrep.com/patent/US20240178324A1

## CPC

- C30B 29/22: Complex oxides
- H10D 30/6755: {Oxide semiconductors, e.g. zinc oxide, copper aluminium oxide or cadmium stannate}
- C23C 16/407: {of zinc, germanium, cadmium, indium, tin, thallium or bismuth}
- C23C 16/45531: {specially adapted for making ternary or higher compositions}
- C30B 25/14: Feed and outlet means for the gases; Modifying the flow of the reactive gases
- C30B 25/165: {the flow of the reactive gases}
- H10D 30/0321: {comprising silicon, e.g. amorphous silicon or polysilicon}
- H10D 30/6729: {characterised by the electrodes}
- H10D 30/673: {characterised by the shapes, relative sizes or dispositions of the gate electrodes}
- H10D 30/6757: {characterised by the structure of the channel, e.g. transverse or longitudinal shape or doping profile (TFTs having channel structures for preventing kink or snapback effects H10D30/6708; TFTs having lightly-doped source or drain extensions H10D30/6715)}
- H10P 14/20: of semiconductor materials
- H10P 14/3238: {being insulating materials}
- H10P 14/3426: {Oxides}
- H10P 14/3434: {being oxide semiconductor materials (Group IIB-VIA semiconductor materials H10P14/3424)}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Provided are a crystalline InZnO oxide semiconductor, a method of forming the same, and a semiconductor device including the crystalline InZnO oxide semiconductor. The crystalline InZnO oxide semiconductor includes an oxide including In and Zn, wherein in Inductively Coupled Plasma-Mass Spectrometry (ICP-MS) analysis, a content of In among In and Zn is about 30 at % or more and about 75 at % or less, and the crystalline InZnO oxide semiconductor has a peak showing crystallinity at a 2-theta value between about 32.3 degrees and about 33.3 degrees in X-ray diffraction (XRD) analysis.

## Claims

### Claim 1

A crystalline InZnO oxide semiconductor comprising:
an oxide including In and Zn,
wherein, in Inductively Coupled Plasma-Mass Spectrometry (ICP-MS) analysis, a content of In among In and Zn is about 30 at % or more and about 75 at % or less, and
in an X-ray diffraction (XRD) analysis, the crystalline InZnO oxide semiconductor has a peak showing crystallinity at a 2-theta value between about 32.3 degrees and about 33.3 degrees.

### Claim 2 (depends on 1)

The crystalline InZnO oxide semiconductor of claim 1, wherein
a content of In among In and Zn is about 32 at % or more.

### Claim 3 (depends on 1)

The crystalline InZnO oxide semiconductor of claim 1, wherein
a content of In among In and Zn is about 33 at % or more.

### Claim 4 (depends on 1)

The crystalline InZnO oxide semiconductor of claim 1, wherein
a content of In among In and Zn is about 35 at % or more.

### Claim 5 (depends on 1)

The crystalline InZnO oxide semiconductor of claim 1, wherein
a content of In among In and Zn is about 70 at % or less.

### Claim 6 (depends on 1)

The crystalline InZnO oxide semiconductor of claim 1, wherein
a content of In among In and Zn is about 65 at % or more.

### Claim 7

A method of forming a crystalline InZnO oxide semiconductor, the method comprising:
co-depositing In and Zn on a substrate using atomic layer deposition (ALD), wherein
a ratio of a deposition cycle of In with respect to a deposition cycle of Zn is about 1 or more and about 8 or less, and
in an X-ray diffraction (XRD) analysis, the crystalline InZnO oxide semiconductor has a peak showing crystallinity at a 2-theta value between about 32.3 degrees and about 33.3 degrees.

### Claim 8 (depends on 7)

The method of claim 7, wherein,
a ratio of a deposition cycle of In with respect to a deposition cycle of Zn is about 1.5 or more.

### Claim 9 (depends on 7)

The method of claim 7, wherein,
a ratio of a deposition cycle of In with respect to a deposition cycle of Zn is about 2 or more.

### Claim 10 (depends on 7)

The method of claim 7, wherein,
a ratio of a deposition cycle of In with respect to a deposition cycle of Zn is about 6 or less.

### Claim 11 (depends on 7)

The method of claim 7, wherein,
a ratio of a deposition cycle of In with respect to a deposition cycle of Zn is about 5 or less.

### Claim 12 (depends on 7)

The method of claim 7, wherein,
a ratio of a deposition cycle of In with respect to a deposition cycle of Zn is about 4 or less.

### Claim 13 (depends on 7)

The method of claim 7, wherein,
in Inductively Coupled Plasma-Mass Spectrometry (ICP-MS) analysis of the crystalline InZnO oxide semiconductor, a content of In among In and Zn is about 30 at % or more and about 75 at % or less.

### Claim 14 (depends on 7)

The method of claim 7, wherein,
the co-depositing the In and Zn on the substrate is performed using a co-deposition process where a temperature of the substrate is about 200° ° C. or more and about 350° ° C. or less.

### Claim 15 (depends on 7)

The method of claim 7, wherein,
the co-depositing the In and Zn on the substrate is performed using a co-deposition process where a temperature of the substrate is about 200° ° C. or more and about 300° ° C. or less.

### Claim 16

A semiconductor device comprising:
a substrate;
a channel layer on the substrate, the channel layer including a crystalline InZnO oxide semiconductor;
a gate electrode on the channel layer; and
a source electrode and a drain electrode on both sides of the channel layer, respectively, wherein
in Inductively Coupled Plasma-Mass Spectrometry (ICP-MS) analysis of the crystalline InZnO oxide semiconductor, a content of In among In and Zn is about 30 at % or more and about 75 at % or less, and
in an X-ray diffraction (XRD) analysis, the crystalline InZnO oxide semiconductor has a peak showing crystallinity at a 2-theta value between about 32.3 degrees and about 33.3 degrees.

### Claim 17 (depends on 16)

The semiconductor device of claim 16, further comprising:
a gate insulating layer between the channel layer and the gate electrode.

### Claim 18 (depends on 16)

The semiconductor device of claim 16, wherein the channel layer is parallel to the substrate.

### Claim 19 (depends on 18)

The semiconductor device of claim 18, wherein the gate electrode is above the channel layer or the gate electrode is under the channel layer.