# US 2024/0175814 A1 · Method for evaluating resist polymer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0175814 A1
- Document ID: US20240175814A1
- Status: Published application
- Kind: A1
- Application number: 18/548,961
- Filed: 2022-03-25
- Published: 2024-05-30
- Earliest claimed: 2021-03-31
- Assignees: Maruzen Petrochemical Co., Ltd.
- Applicants: Maruzen Petrochemical Co., Ltd.
- Inventors: Daisuke TABATA; Tatsuya TSUKAMOTO; Yoshiyuki FURUYA; Ryo SATO
- Web page: https://patentgrep.com/patent/US20240175814A1

## CPC

- G01N 21/59: Transmissivity (G01N21/25 takes precedence)
- G01N 21/82: producing a precipitate or turbidity
- C08F 220/1806: {C6-(meth)acrylate, e.g. (cyclo)hexyl (meth)acrylate or phenyl (meth)acrylate}
- C08F 220/283: {and containing one or more carboxylic moiety in the chain, e.g. acetoacetoxyethyl(meth)acrylate}
- G01N 15/075: by optical means
- G01N 21/272: {for following a reaction, e.g. for determining photometrically a reaction rate (photometric cinetic analysis)}
- G01N 21/94: Investigating contamination, e.g. dust (G01N21/85 takes precedence)
- G03F 7/038: Macromolecular compounds which are rendered insoluble or differentially wettable (G03F7/075 takes precedence; macromolecular azides G03F7/012; macromolecular diazonium compounds G03F7/021)
- G03F 7/039: Macromolecular compounds which are photodegradable, e.g. positive electron resists (G03F7/075 takes precedence; macromolecular quinonediazides G03F7/023)
- G03F 7/16: Coating processes; Apparatus therefor (applying coatings to base materials in general B05; applying photosensitive compositions to base for photographic purposes G03C1/74)
- G03F 7/0397: {the macromolecular compound having an alicyclic moiety in a side chain}
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

[Problem to be solved] An object of the present invention is to provide a method for evaluating the dissolution properties of a resist polymer, which method allows for an easy evaluation without requiring complicated processes, and with a high sensitivity. [Solution] The method for evaluating the dissolution properties of a resist polymer according to the present invention includes the following steps (i) to (iii): the step (i) of dissolving the resist polymer in a solvent to prepare a test solution; the step (ii) of adding a solvent dropwise to the test solution while stirring the test solution, and measuring in real time the weight of the solvent added dropwise and the change in the turbidity of the test solution, as the dropwise addition proceeds; and the step (iii) of calculating the amount of the solvent added dropwise until the turbidity of the test solution reaches a predetermined value.

## Claims

### Claim 1

A method for evaluating the dissolution properties of a resist polymer, the method comprising the following steps (i) to (iii):
the step (i) of dissolving the resist polymer in a solvent to prepare a test solution;
the step (ii) of adding a solvent dropwise to the test solution while stirring the test solution, and measuring in real time the weight of the solvent added dropwise and the change in the turbidity of the test solution, as the dropwise addition proceeds; and
the step (iii) of calculating the amount of the solvent added dropwise until the turbidity of the test solution reaches a predetermined value.

### Claim 2 (depends on 1)

The method for evaluating the dissolution properties of a resist polymer according to claim 1, wherein a container into which the test solution is introduced when measuring the turbidity in the step (ii) is an Erlenmeyer flask, and wherein the test solution is stirred by orbital shaking.

### Claim 3 (depends on 1)

A method for producing a resist polymer, the method comprising:
the step of obtaining the resist polymer; and
the step of evaluating the dissolution properties of the resulting resist polymer, using the method for evaluating the dissolution properties of a resist polymer according to claim 1.